The paper describes relationships between the kinetics of precipitation and growth of the intermetallic phase y' [Ni3(Al,Ti)] and the strengthening magnitude obtained in a creep resisting Fe-Ni alloy of the A-286 type. In order to accomplish the goal the study, the author used the LSW coagulation theory and Brown and Ham's conventional analysis of strengthening by ordered particles. The samples were subjected to a solution heat treatment at 980°C/2h/water and then aged at 715, 750 and 780°C, with holding times 0.5-500h. The heat-treated samples were subjected to structural analyses (TEM, X-ray diffraction) and analyses of mechanical properties (hardness test, static tensile test, and impact test). The author carried out analyses of strengthening and flow stress (Ax) increases as a function of the particle size of the y' phase and determined the value of the anti-phase boundary energy (YAPB) f°r the analyzed Fe-Ni alloy.
PL
Praca dotyczy określenia zależności pomiędzy kinetyk wydzielania i koagulacji fazy międzymetalicznej typu y' [Ni3(Al,Ti a wielkością uzyskiwanego umocnienia w żarowytrzymałym stopi Fe-Ni typu A-286. Do realizacji pracy wykorzystano teor koagulacji LSW oraz konwencjonalną analizę umocnienia prz( cząstki uporządkowane Brown'a i Ham'a. Próbki ze stopu Fe-f poddano przesycaniu w warunkach 980°C/2h/woda, a następnie starzeniu przy temperaturach 715, 750 i 780°C oraz czasach wytrzymania od 0.5 do 500h. Obrobione cieplnie próbki poddano badaniom strukturalnym (TEM, badania rentgenowskie) on badaniom własności mechanicznych (pomiary twardości, statyczna próba rozciągania, próba udarności). Przeprowadzono analizę; przyrostu umocnienia i naprężenia płynięcia (AT) W funkcji wielkoś cząstek fazy y' i wyznaczono wartość energii granicy antyfazowowej (YAPB) dla badanego stopu Fe-Ni.
EN
The papers presents a method which allows to eliminate the y' (Cu, Ni)3Al phase of discontinuous transition occurring during ageing of CuNi10Al3 alluy. Introduction of additions such as Si or ti in the amount of some tenths of percent into CuNi10Al3 alloy causes that y' phase of the discontinuous transition is not precipitated. CuNi10Al3 alloy, free from the lamellar y' precipitates, formed in the discontinuous transition, attains very high strenght properties and good deformability.
PL
W niniejszej pracy przedstawiono sposób pozwalający na wyeliminowanie fazy y' (Cu,Ni)3Al przemiany nieciągłej powstającej podczas starzenia stopu CuNi10Al3. Wprowadzenie do stopu cuNi10Al3 dodatków w postaci Si lub Ti w ilościach dziesiątych części procentu powoduje, ze nie wydziela się faza y' przemiany nieciągłej. Stop CuNi10Al3 pozbawiony płytkowych wydzieleń y' tworzacych się w przemianie nieciagłej uzyskuje bardzo wysokie własności wytrzymałościowe oraz dobrą odkształcalność.