Water scarcity has been well pronounced in the Middle East Region; however, Lebanon is still characterized by wet climate and sufcient water resources. It is a paradox that Lebanon is now under water stress, and many contradictory studies on the climate of Lebanon attributed water stress to the changing climate. Most of these studies were applied with incomplete climatic data records. Therefore, all management approaches were implemented after considering climate as a major infuencer on water resources. In this study, the Emberger Aridity Index (EAi) was employed to investigate the climate regime of Lebanon over more than 30 years focusing on ten representative meteorological stations where comprehensive climatic records were analysed and supported by remotely sensed data. The EAi indicates that Lebanon is still characterized by humid climate, which conficts with the concept of drought existence. Thus, 47% of the Lebanese territory is characterized by humid to sub-humid climate and 29% by semi-arid climate according to Emberger classifcation. This obviously shows that even the climate impact has a role on water scarcity, but it is not the principal infuencer. The results of this study help applying new approaches for water management where the negative human interference should be accounted. It guides stakeholder and decision-maker to follow appropriate water and agricultural policies and strategies for better sustainable development.
PL
Obciążenia cieplne, którym poddawane są formy i rdzenie, powodują termiczne zmęczenie materiału, które może generować tworzenie się wad takich jak: pęknięcia, wżarcia, żyłki, wykruszanie materiału formy podczas zalewania. Może dochodzić także do przypalenia i penetracji metalu do masy formierskiej lub rdzeniowej. Jednym z rozwiązań ograniczającym występowanie niekorzystnych zjawisk jest zastosowanie powłok ochronnych. Nanoszone są one w celu poprawy jakości powierzchni odlewów oraz ułatwienia wyjęcia odlewu z formy. W niniejszym artykule zaprezentowano wstępne wyniki badań wpływu zwiększonej ilości rozcieńczalnika w powłokach, na głębokość penetracji powłoki w głąb rdzeni oraz pomiar parametru hot distortion.
EN
Thermal loads applied to moulds and cores cause thermal fatigue and the appearance of flaws such as: cracks, penetration, veins, spalling of mould material during casting. Scorching and penetration of metal into the moulding sand or core sand are also possible. One of the solutions that limit the occurrence of unfavourable phenomena is using protective coatings. They are applied in order to improve the quality of castings and make it easier to extract a casting from the mould. This article presents a general classification of coatings applied to casting moulds and cores. It focusses mainly on protective coatings and describes the methods of applying and drying them. Preliminary results of coating tests are presented, including microscopic observation of the depth of coating penetration into mass and a measurement of the hot distortion parameter relative to the amount of solvent added.
PL
W artykule zaprezentowano wyniki badań doświadczalnych wpływu podwyższonej temperatury na wytrzymałość przy rozciąganiu drewna sosnowego oraz drewna egzotycznego merbau (Intsia Bijuga), stosowanego w budownictwie i konstrukcjach inżynierskich, impregnowanego nowoczesnymi środkami ogniochronnymi zawierającymi nanocząstki SiO2 o rozmiarach 10 – 20 nm. Impregnację przeprowadzono metodą próżniową przez 15 min, stosując podciśnienie ok. 0,7 at. Badania wytrzymałościowe zostały wykonane w Zakładzie Mechaniki Stosowanej SGSP.
EN
The article presents results of the experimental studies of the effects of increased temperature on tensile strength of pine wood and exotic woodmerbau (Intsia Bijuga) used in building and engineering constructions impregnated with modern fire-retardant agents containing SiO2 nanoparticles of size 10 – 20 nm. The impregnation was carried out by vacuum method for 15 minutes using a vacuum row (0,7 atm). The strength tests were carried out at the Department of Applied Mechanics of The Main School of Fire Service.
PL
W pracy przedstawiono wyniki badań skłonności do pęknięć gorących austenitycznej stali Super 304H przeznaczonej do pracy w wysokiej temperaturze. Stal została poddana próbie Transvarestraint, a wyniki tej próby zostały porównane z wynikami próby Transvarestraint dla stali 304. Ustalono, że stal Super 304H wykazuje bardzo dużą skłonność do pęknięć zarówno krystalizacyjnych, jak i segregacyjnych. Ponadto w wysokotemperaturowej strefie wpływu ciepła stwierdzono uszkodzenia granic ziaren o charakterze pęknięć gorących.
EN
The paper presents results of hot crack sensitivity of Super 304H austenitic steel designed for work at increased temperature. Steel has been put to the Transvarestraint test. The results of this test were compared with the results of tests for steel 304. It was found that the steel Super 304H is highly sensitive to crystalline and segregation crack. In addition, high temperature heat-affected zone were damaged grain boundaries of a hot cracks.