A study was made of water-related properties of Pinus pinaster wood impregnated with paraffin or modified by heat treatment or furfurylation. Treated woods were submerged in water for periods ranging from 2 to 1680 hours. Water absorption, swelling, and dimensional stability in the radial and tangential directions – expressed as Anti-Shrinking Efficiency (ASE) – were determined. Water absorption increased with time, reaching approximately 140% after 1680 h for untreated and heat-treated wood, and 60% for paraffinated and furfurylated wood. The rate of swelling differed between the first hours of soaking and after prolonged immersion. The final swelling was approximately 9% and 6% for untreated pine, 8% and 4% for paraffinated pine, 5.5% and 3% for heat-treated pine and 2.5% and 1% for furfurylated pine (in the tangential and radial directions respectively). At the end of the soaking test, furfurylated pine had the best ASE of approximately 80% and 70% in the tangential and radial directions respectively, followed by heat-treated pine with 44% and 34%, and paraffinated wood with 35% and 13%.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.