After Vosikovsky (1975), the corrosion fatigue crack growth rate (CFCGR) characteristics have been divided into three regions. The region-III rates are very close to mechanical fatigue crack growth rates. CFCGR formulae, including the long-crack length effect (in region I only), the loading frequency effect (in region II only), and the saltwater temperature effect, have been proposed. It has been assumed that CFCGR is proportional to f –k, where f is the loading frequency and k is a constant. The averaged k-value for all steels of yield stress (YS) below 500 MPa, usually with ferrite-pearlite microstructures, is higher than that for YS > 500 MPa, usually with quenched and tempered microstructures. The temperature effect does not appear in region I below room temperature. In the remaining cases, that is, in region I for elevated temperatures and in region II for both low and elevated temperatures, the CFCGR increases with increasing temperature. Under a potential of –0.8 V, a long-crack-length effect, qualitatively similar to analogous effect for free corrosion conditions, appears.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.