The paper presents results of research associated with expanding clay slate from Carpathian flysh, near water reservoir in Świnna Poręba. Examination were associated with influence of inclination laminae this soils. The laminae constitute peculiar texture which is affecting on size of expanding and water also much easier penetrates deep layers between the laminae. This property coming into new landslides.
PL
W pracy przeprowadzono ocenę zależności wybranych parametrów ekspansywności gruntów ilastych. Wykazano wyraźną zależność wartości pęcznienia swobodnego od parametrów, takich jak powierzchnia właściwa, pojemność sorpcyjna (MBC) oraz wilgotność gruntu w stanie powietrzno-suchym. Na tej podstawie stwierdzono, że głównym czynnikiem powodującym pęcznienie badanych gruntów jest zawartość pęczniejących minerałów ilastych w frakcji iłowej. Wyniki laboratoryjne badanych prób iłów nie wykazały zależności pomiędzy wartościami ciśnienia pęcznienia, a wartościami pęcznienia swobodnego oraz powierzchnią właściwą i pozostałymi parametrami. Stwierdzono, że główną przyczyną braku korelacji tych czynników może być silne skonsolidowanie i zagęszczenie prób iłów.
EN
The paper presents estimation of the relation between selected swell parameters of clayey soils. The clear correlation of free swelling and parameters such as specific surface area, methylene blue value, water content of air-dry soil was demonstrated. On this basis, it was found that the main factor behind the swelling of tested soils is contents of swelling clay minerals in the clay fraction. Results of laboratory tests of the clay samples showed no relationship between swelling pressure values, free swelling and specific surface area, as well as other parameters. It was found that, the main reason for the absence of correlation of these factors may be high consolidation and compaction of clay samples.
EN
The purpose of this work was to determine the optimal duration of free swelling for refined unbleached kraft pine pulp. Free swelling is the effect of water sorption by cellulose fibres without their simultaneous mechanical treatment (e.g. refining). The second purpose was to determine the possibility of improving the mechanical properties of paper by testing various combinations of refining and free swelling processes. The pulp SR value and water retention value (WRV) of the fibres were tested. As regards paper properties, the tensile index and tear index were tested. Based on the results obtained, it was found that for the pulp tested, refined to 35 °SR, the optimal time of free swelling was 70 min. It was also proved that the free swelling had a significant impact on both the WRV of fibres and the mechanical parameters of paper tested. For the scheme in which refining was followed by free swelling, a 7% increase in the tear index was obtained. However, an 11% increase in the tear index was attained for the scheme with three refining stages, followed by free swelling after each refining.
PL
Celem tej pracy było określenie optymalnego czasu swobodnego pęcznienia mielonej papierniczej masy celulozowej siarczanowej niebielonej sosnowej. Drugim celem było określenie możliwości zwiększenia właściwości wytrzymałościowych papieru poprzez zbadanie różnych kombinacji procesów mielenia i swobodnego pęcznienia. Badanymi właściwościami masy włóknistej były: smarność Schoppera-Rieglera i WRV włókien. Badanymi właściwościami papieru były: wskaźnik zerwania i wskaźnik oporu przedarcia. Na podstawie uzyskanych wyników stwierdzono, że swobodne pęcznienie jest procesem długotrwałym. Dla badanej masy celulozowej mielonej do wartości 35oSR optymalny czas swobodnego pęcznienia wynosił 70 minut. Rezultaty badań wskazują, że stosowanie swobodnego pęcznienia ma zdecydowanie pozytywny wpływ zarówno na wskaźnik WRV włókien, jak i badane wskaźniki wytrzymałościowe papieru. Najlepsze rezultaty uzyskiwano, kiedy swobodne pęcznienie było stosowane także na samym końcu, po ostatnim mieleniu. Dla wariantu, w którym po pojedynczym mieleniu występowało jedno, końcowe pęcznienie swobodne uzyskano 7% przyrost wskaźnika zerwania. Największy, 11% przyrost wskaźnika przedarcia stwierdzono dla wariantu, w którym zastosowano trójetapowe mielenie, a po każdym z nich następowało pęcznienie swobodne.