This work aimed to observe the influence of calorific value and proximate properties in the fabrication of rice husk (RH) and coffee shell (CS) briquettes composite. Rice and coffee husks contain cellulose, hemicellulose, and lignin. These contents are necessary for the adhesive to bind the briquette (amylose and amylopectin). The raw materials were carbonized at 400 °C for 60 minutes. Variations of sieving size (60, 80, and 100 mesh) and the composition ratio of raw material CS:RH were reviewed to study their effect. Tests of density, moisture content, volatile matter content, ash content, fixed carbon content, shatter index, combustion rate, and calorific value were carried out to determine the optimum composition. The results were obtained with the best quality at a particle size of 60 mesh with the highest calorific value of 17.422 MJ/kg. It showed that the briquettes have good quality and are comparable with the standard briquette.
EN
Previous research has found that the fixed carbon in blast furnace dust (BFD) could be used as the reductant of co-reduction roasting of the iron oxides in seaside titanomagnetite and BFD to replace coals. This research studied the influence mechanism of the fixed carbon and ash in BFD on coreduction.Results showed that both fixed carbon and ash in BFD promoted the reduction of iron, while ash had adverse effect on separation of titanium and iron. The main mechanism was as follows: The ash in BFD accelerated melting. In addition, the iron oxide in the ash of BFD could be reduced to metallic iron cores more easily in the initial stage, providing the site of inhomogeneous core and promoting the aggregation and growth of metallic iron. Furthermore, the fixed carbon mainly reacted with iron ore by solid-solid reaction, leading to a rapid reduction rate and a high utilization rate of fixed carbon.