Polymer composite structures and structural elements made of them are often subjected to various machining processes, particularly drilling for assembling purposes. Considering their compliance to high temperature resulting from drilling, various phenomena may occur during this process, e.g. thermal phase transitions, which directly influence on both mechanical properties as well as occurrence of manufacturing damage of a treated structure. The following study presents experimental results of monitoring of drilling process using infrared thermography. An influence of a type of an applied drill bit on resulting temperature evolution was analyzed in this paper. The obtained results indicate a necessity to limit a heat occurred during the drilling process to critical temperatures of a drilled composite in order to avoid manufacturing damage occurrence by selection of appropriate drill bits or by applying techniques of cooling down a drill bit.
PL
Polimerowe struktury kompozytowe oraz wykonywane z nich elementy strukturalne są często poddawane różnym procesom obróbczym, m. in. wierceniu do celów montażu. Biorąc pod uwagę ich podatność na wysokie temperatury wynikające podczas procesu wiercenia, można zauważyć podczas tego procesu różne zjawiska, np. cieplne przemiany fazowe, co bezpośrednio wpływa zarówno na właściwości mechaniczne, jak i powstawanie uszkodzeń technologicznych w obrabianej strukturze. Niniejsze badania przedstawiają wyniki eksperymentalne monitorowania procesu wiercenia z wykorzystaniem termografii w podczerwieni. W artykule zbadano wpływ typu zastosowanego wiertła na wynikową charakterystykę temperaturową. Otrzymane wyniki wskazują na potrzebę ograniczenia ciepła powstającego podczas procesu wiercenia do temperatur krytycznych wierconego kompozytu w celu uniknięcia wystąpienia uszkodzeń technologicznych poprzez wybór odpowiednich wierteł lub zastosowania technik chłodzenia wiertła.
EN
Wide application of polymer composites in various industrial branches and their treatment requires the development and adaptation of suitable methods of quality control after treatment. One of the most often technological operation on composite structures is drilling. The paper focuses on evaluation of drilled holes quality in two composite structures using the most common methods of non-destructive testing (NDT) applied for composite materials. The applied NDT methods cover microscopic imaging, ultrasonic testing, infrared testing and X-ray computed tomography. Moreover, the new delamination factor as well as an automatic detection method of delaminations was proposed. The obtained results of quality control of drilled holes in composites were compared and discussed. Based on them the recommendations of quality control of drilled holes in composite materials were formulated.
PL
Szerokie zastosowanie kompozytów polimerowych w różnych gałęziach przemysłu i ich obróbka wymagają rozwoju i adaptacji odpowiednich metod kontroli jakości po obróbce. Jedną z najczęściej wykonywanych operacji technologicznych na strukturach kompozytowych jest wiercenie. W artykule skupiono się na ocenie wierconych otworów w dwóch strukturach kompozytowych, stosując metody badań nieniszczących najczęściej wykorzystywane do materiałów kompozytowych. Zastosowane metody badań nieniszczących obejmują obrazowanie mikroskopowe, badania ultradźwiękowe i termograficzne oraz rentgenowską tomografię komputerową. Ponadto zaproponowano nowy wskaźnik delaminacji oraz metodę automatycznego wykrywania delaminacji. Uzyskane wyniki kontroli jakości wierconych otworów w kompozytach zostały porównane i omówione. Na ich podstawie sformułowano zalecenia kontroli jakości wierconych otworów w materiałach kompozytowych.