EN
The paper presents the results of comparative studies of thermal properties of various types of natural esters used as electroinsulating liquids in transformers. Adequate thermal properties of electro-insulating liquids ensure reliable work of transformers. Two natural esters were selected for the study – one commonly used in distribution transformers, the other characterized by low viscosity. Fourier Transform Infrared Spectroscopy and UV-Visible spectroscopy were used to examine the chemical structure of the examined esters. Properties such as thermal conductivity coefficient λ, kinematic viscosity υ, specific heat cp, density ρ, and thermal expansion coefficient β were analyzed. Heat transfer factor α of the liquid was calculated on the basis of obtained properties. This factor defines the ability of an insulating liquid to heat transport in the transformer, thus determining its reliability. The authors put forward a thesis that a low viscosity natural ester will have a higher heat transfer factor α due to its low viscosity, which affects the factor α. The analysis of thermal properties was carried out for the following temperatures: 25, 40, 60, and 80°C. On the basis of the calculated factor α, the temperature drops in the transformer filled with the analyzed types of natural esters were determined. It has been shown that if a low viscosity natural ester is used in the cooling system of the transformer, the temperature of the hot-spot will be lower. This fact may contribute to more reliable work of transformers and extend its service life.
PL
W pracy przedstawiono wyniki badań porównawczych właściwości cieplnych różnego rodzaju estrów naturalnych stosowanych jako ciecze elektroizolacyjne w transformatorach. Odpowiednie właściwości cieplne cieczy elektroizolacyjnych zapewniają niezawodną pracę transformatorów. Do badań wybrano dwa estry naturalne – jeden powszechnie stosowany w transformatorach rozdzielczych, drugi charakteryzujący się obniżoną lepkością. Do analizy struktury chemicznej badanych estrów wykorzystano spektroskopię w podczerwieni z transformatą Fouriera (FT-IR) oraz spektroskopię w ultrafiolecie i świetle widzialnym (UV-VIS). Analizowanymi właściwościami cieczy były przewodność cieplna λ, lepkość kinematyczna υ, ciepło właściwe cp, gęstość ρ oraz rozszerzalność cieplna β. Na podstawie przedstawionych właściwości cieplnych obliczono współczynnik przejmowania ciepła α. Współczynnik ten określa zdolność cieczy elektroizolacyjnej do transportu ciepła w transformatorze, a tym samym określa jego niezawodność. Autorzy postawili tezę, że ester naturalny o obniżonej lepkości będzie miał wyższy współczynnik przejmowania ciepła α ze względu na jego obniżoną lepkość. Analizę właściwości cieplnych przeprowadzono dla czterech wartości temperatury: 25, 40, 60 i 80°C. Na podstawie obliczonego współczynnika α określono spadki temperatury w transformatorze wypełnionym analizowanymi estrami naturalnymi. Wykazano, że jeżeli w układzie chłodzenia transformatora stosowany jest ester naturalny o obniżonej lepkości, wówczas temperatura najgorętszego miejsca (ang. hot spot) będzie niższa. Fakt ten może przyczynić się do zwiększenia niezawodności pracy transformatorów i przedłużyć okres ich eksploatacji.
2
Content available remote Preparation and dielectric properties of BaBi1.8Ln0.2Nb2O9 (Ln = Ce, Gd) ceramics
EN
The main subject of the presented research is to investigate the dielectric properties of BaBi1.8Ln0.2Nb2O9 (Ln = Ce, Gd) ceramics prepared by conventional solid state reaction route. The materials were examined using XRD and FT-IR methods. Moreover, the AC conductivity, dielectric constant and dielectric loss of the ceramics were determined. X-ray diffraction confirmed that all these compounds crystallize in an orthorhombic structure. Fourier transform infrared spectroscopy study confirmed the presence of two characteristic vibration bands located at around 617 cm-1 and 818 cm-1 for BaBi2Nb2O9. The experimental results show that the substitution of Bi by Ce or Gd causes a decrease in Curie temperature, dielectric constant and dielectric loss.
3
Content available Ludwik Badian fizyk materiałów dielektrycznych
PL
W artykule opisano biografię i prace naukowe Ludwika Badiana. Z perspektywy lat zdumiewa zaskakująco szybka kariera Ludwika Badiana. Młody, wówczas bezpartyjny absolwent Politechniki został dyrektorem Państwowego Instytutu Telekomunikacyjnego już w drugim roku pracy, zaledwie ze stopniem mgr inż. Imponuje również wypromowanie 29 doktorów w okresie 18 lat (1967-1984).
EN
This paper describes biography and scientific works of Ludwik Badian. From the years perspective surprisingly quick carrier of Ludwik Badian is amazing. The young, not belonging to the PZPR party alumni of Wroclaw University o Technology with the title engineer was appointed to the director of State Telecomunication Institute after one year work in this Institution. He conferred 29 doctor degrees in the period of 18 years (1967-1984).
4
Content available remote Phase evolution and microwave dielectric properties of A5M5O17-type ceramics
EN
A number of A5M5O17 (A = Na, Ca, Sr, La, Nd, Sm, Gd, Dy, Yb; B = Ti, Nb, Ta) type compounds were prepared by a solid-state sintering route and characterized in terms of structure, microstructure and microwave dielectric properties. The compatibility of rare earths with mixed niobate/tantalate and titanate phases was investigated. The larger ionic radii mismatch resulted in the formation of pyrochlore and/or mixed phases while in other cases, pure A5M5O17 phase was formed. The samples exhibited relative permittivity in the range of 35 to 82, quality factor (Q × fo) = 897 GHz to 11946 GHz and temperature coefficient of resonance frequency (τf) = -120 ppm/°C to 318 ppm/°C.
PL
Przedstawione rezultaty badań dotyczą szacowania błędów aproksymacji metodą elementów skończonych (MES) w problemach elektrycznych ośrodków dielektrycznych. Dotychczasowe badania autora nad szacowaniem błędów dotyczyły struktur sprężystych analizowanych z wykorzystaniem modelowania hierarchicznego i adaptacyjnej MES. Zaprezentowane wyniki stanowią etap pośredni zmierzający do opracowania metod szacowania błędów w ośrodkach piezoelektrycznych, innymi słowy w sprzężonych problemach elektro-mechanicznych. Uzyskane rezultaty przedstawione są w kontekście analogii do problemów sprężystych.
EN
The presented results of the research concern approximation error estimation of the solutions obtained with the finite element method (FEM) in electric problems of dielectrics. The hitherto research of the author were focused on purely elastic structures. These structures were analysed with the hierarchical modelling and adaptive FEM. The presented outcome constitutes an intermediate stage of the research directed towards elaboration of error estimation methods for piezoelectric media, in other words, for coupled electro-mechanical problems. The obtained results are presented in the context of analogy to purely elastic problems.
EN
(La, Nd)2/3TiO3 ceramics were prepared through a conventional solid state mixed oxide route. For phase and microstructure analysis, XRD and SEM were used, respectively. Microwave dielectric properties were measured using a network analyzer. XRD patterns revealed the formation of the parent (La, Nd)2/3TiO3 phase along with (La, Nd)4Ti9O24 as a secondary phase. The microstructure consisted of rectangular and needle shaped grains, which decreased in size from 4 μ m to 2 μm with an increase in sintering temperature from 1300 °C to 1350 °C. Decrease in grain size caused an increase in density of the samples from 4.81 g/cm3 to 5.17 g/cm3. Microwave dielectric properties of the samples calcined and sintered in air atmosphere were εr = 40.35, Q × f = 3499 GHz and τ f = 0 ppm/°C, whereas for a sample calcined in nitrogen and sintered in air they were εr = 40.18, Q × f = 4077 GHz and τ f = +4.9 ppm/°C, respectively.
7
Content available remote Growth and characterization of hexamethylenetetramine crystals grown from solution
EN
Organic nonlinear optical single crystals of hexamethylenetetramine (HMT; 10 × 10 × 5 mm3) were prepared by crystallization from methanol solution. The grown crystals were subjected to various characterization techniques such as single crystal XRD, powder XRD, UV-Vis and electrical studies. Single crystal XRD analysis confirmed the crystalline structure of the grown crystals. Their crystalline nature was also confirmed by powder XRD technique. The optical transmittance property was identified from UV-Vis spectrum. Dielectric measurements were performed as a function of frequency at different temperatures. DC conductivity and photoconductivity studies were also carried out for the crystal. The powder second harmonic generation efficiency (SHG) of the crystal was measured using Nd:YAG laser and the efficiency was found to be two times greater than that of potassium dihydrogen phosphate (KDP).
EN
Low frequency dielectric relaxation has been reported for a nematic liquid crystal in the frequency range of 1 kHz to 10 MHz and in the temperature range from 25 °C to 100 °C. The optical behaviour has also been studied by measuring the refractive indices, birefringence and optical transmittance in the temperature range mentioned above. The birefringence data have been used to calculate the order parameter by Vuks' approach, and its variation with temperature has been discussed. Transition temperatures obtained using different techniques are found to be in good agreement with each other.
EN
The effect of LiF and CBS glass additives on the microstructure and dielectric property of BaTiO3 (BT) ceramics was studied. The phase of BaLiF3 was observed from the interaction between BT and LiF when the samples were sintered at 900 °C for 1 h. Crystal grains with Ba and F in atomic ratios of 1:3 were observed from the SEM and TEM analysis of the microstructures. Abnormal grain growth (AGG) was observed to occur in the BT ceramics sintered at 950 °C. Further improvement to the composition was achieved by employing a two-stage process. This included CBS glass shell coating of the BT particles in the first stage, and the addition of LiF in the second stage. The composition thus formed had very good permittivity (1725) and an extremely low dielectric loss value (0.008).
EN
This paper investigated the fracture behaviour of a piezo-electro-magneto-elastic material subjected to electro-magneto-mechanical loads. The PEMO-elastic medium contains a straight-line crack which is parallel to its poling direction and loaded surface of the half-space. Fourier transform technique is used to reduce the problem to the solution of one Fredholm integral equation. This equation is solved exactly. The semi-permeable crack-face magneto-electric boundary conditions are utilized. Field intensity factors of stress, electric displacement, magnetic induction, crack displacement, electric and magnetic potentials, and the energy release rate are determined. The electric displacement and magnetic induction of crack interior are discussed. Strong coupling between stress and electric and magnetic field near the crack tips has been found.
PL
Przedstawiono praktyczne zastosowania elektretów z ładunkiem implantowanym z zewnętrznego źródła, w medycynie i ochronie zdrowia. Omówiono podstawowe parametry uformowanych elektretów, a szczególnie średnie położenie ładunku elektrycznego i rozkład ładunku przestrzennego. Podano izotermiczne i nieizotermiczne metody szacowania czasu życia ładunku elektretu. Przeanalizowano wpływ parametrów procesu technologicznego, warunków elektryzacji i czynników środowiskowych na stabilność ładunku włóknin filtracyjnych i jakość filtracji. Badania te zilustrowano mikrofotografiami powierzchni włóknin filtracyjnych. Zaprezentowano konstrukcję elektretowego przetwornika drgań, charakteryzującego się dużą powierzchnią i wysoką czułością. Wprowadzono w złożoną problematykę roli ładunku elektrycznego w procesach zachodzących na granicy materiał protetyczny-tkanka płynna (krew). Do scharakteryzowania właściwości elektrycznych powierzchni materiału i interpretacji zjawisk zachodzących w roztworze wykorzystano potencjał elektrokinetyczny. Dokonano doboru praktycznych metod laboratoryjnych, pozwalających na ocenę in vitro materiałów. Ustalono, że poza znakiem i jednorodnością powierzchniowej gęstości ładunku elektrycznego, wyraźny wpływ na adhezję elementów morfotycznych krwi ma rozkład ładunku w objętości materiału. Uzyskane wyniki badań, uzupełnione o badania mikroskopowe, wskazały na nowe, istotne czynniki warunkujące proces zakrzepowy krwi.
EN
The monograph presents practical applications of electrets with the charge implanted from an external source, in medicine and health protection. Basic characteristics of the formed electrets, especially an average location of electric charge and space charge distribution are discussed. The isothermal and non-isothermal methods of assessment of the charge lifetime of the electrets are presented. The effect of the manufacturing process parameters, electrization state and environmental conditions on the charge stability of filtration fibers and filtration quality is analyzed. The investigation is illustrated with the microphoto-graphs of the surfaces of the filtration fibers. The structure of on electret condenser transducer characterized by a large area and high sensitivity is presented. A brief explanation is given of a complex role of the electric charge in the processes occurring at the interface of prosthetic material--liquid tissue (blood). The electrokinetic potential was used for characterization of the electrical properties of material surface and interpretation of physical phenomena taking place in the solution. The practical laboratory methods enabling in vitro assessment of the materials investigated have been selected. Besides the sign and homogeneity of the surface electric charge also the charge distribution in the bulk was found to play an important part in adhesion of morphotic blood elements. Results obtained, together with the results of additional microscopic examination, showed the new important factors determining the process of blood clotting.
EN
The transition regions of GdSiO/SiOx and HfO2/ SiOx interfaces have been studied with the high-k layers deposited on silicon substrates. The existence of transition regions was verified by medium energy ion scattering (MEIS) data and transmission electron microscopy (TEM). From measurements of thermally stimulated current (TSC), electron states were found in the transition region of the HfO2/SiOx structures, exhibiting instability attributed to the flexible structural molecular network expected to surround the trap volumes. The investigations were focused especially on whether the trap states belong to an agglomeration consisting of a single charge polarity or of a dipole constellation. We found that flat-band voltage shifts of MOS structures, that reach constant values for increasing oxide thickness, cannot be taken as unique evidence for the existence of dipole layers.
PL
W artykule opisano nową koncepcyjną konstrukcję mechatronicznego pozycjonera biegunowego opracowaną dla potrzeb technologii znakowania i grawerowania podpowierzchniowego szkła i innych przezroczystych dielektryków. Omówiono warunek sztywności konstrukcji pozycjonera (dla przypadku klasycznego kartezjańskiego i rozwiązania propo- nowanego – biegunowego), wpływający bezpośrednio na dokładność obróbki laserowej. W pracy wskazano również możliwe pola zastosowań opracowanej koncepcji pozycjonera biegunowego. Zaproponowana konstrukcja aparatu ruchowego pozwoli na uzyskanie nowej jakości pozycjonowania (uzyskanie efektu synergii) poprzez połączenie komputerowego sterowania z prostym mechanizmem biegunowym (parami obrotowymi), wzorowanym na konstrukcji dysku twardego komputera osobistego.
EN
New construction of mechatronics polar positioning system of laser device for engraving glass and other transparent dielectrics there is presented in the work. The results of analysis of stiffness Cartesian positioning system and alternative new polar positioning system are presented too. The description of the constructions of working arm and rotation table of polar positioning system is given in the paper. Possible applications of describe polar positioning system are defined. Presented in the work construction of movement device brings the new quality of positioning (a synergy effect) through connection the computer control technology with the simple polar mechanism similar to construction of computer hard drive.
EN
The dielectric properties of Sb2O3 doped (Ba0.992-xSrxDy0.008)TiO3.004ceramics fabricated by a solid state route with various Sb2O3 contents and Sr/Ba ratios were investigated. The XRD patterns confirm the samples to be multiphase compounds composed of perovskite major phase and Ba4Ti13O30, Ba6Ti17O40, Ti7O13 secondary phases. The average lattice constant indicates that Sb3+ ions initially occupy the A-sites and then enter the B-sites serving as acceptor dopants. The Curie temperature decreases as the Sb2O3 content increases and as the Sr/Ba ratio increases also. The thermal stability of the electric permittivity increases as the Sb2O3 concentration increases but decreases as the Sr/Ba ratio increases. The resistivity and ac standing voltage decrease as the Sr/Ba ratio decreases. The Sb2O3 doped (Ba0.992-xSrxDy0.008)TiO3.004 ceramics with high permittivity, low dielectric loss, high ac standing voltage and low temperature coefficient of capacitor are obtained for applications in environment friendly capacitors.
EN
The modern dielectrics for electrical industry applications and the new ways of their production are reviewed shortly. The development needs and future technologies to engineer nano-structured materials for dielectric applications are presented. The perspectives on the development with novel properties of nanodielectris and possible area of their applications are shown. The limitations resulting from failure to understand properties and mechanisms related to new nanocomposites and research problems are indicated.
EN
Zawiera tylko streszczenia angielskie referatów z konferencji: 4th Conference International Dielectric Society and 9th International Conference Dielectric and Related Phenomena. IDS & DRP 2006 (03-07.09.2006 ; Poznań ; Poland). Konferencja obejmowała następujące zagadnienia: Glass transition; Johari-Goldstein β-relaxation; Dynamics under spatial confinement; Dynamics under applied pressure; Charge transport in disordered systems; Relaxation theories; Simulations of molecular dynamics; Nano-confined systems, ultrathin layers; Micro- and nanocomposites; Molecular dynamics of functional polymers; Special dielectrics for opto-electronics; Nanostructured dielectrics and electrets; Liquid crystalline and ferroelectric materials; Biological systems: biopolymers, biodielectrics; Molecular dynamics in aqueous systems; BDS in comparison with another spectroscopic techniques; Time-domain spectroscopy; Real-time dielectric spectroscopy - monitoring of structure evolution; Novel methodological developments. Wybrane pełne teksty referatów: Journal of Non-Crystalline Solids, Vol. 353, Iss. 47-51 (December 1, 2007).
17
Content available remote Wpływ rodzaju dielektryku na właściwości dielektromagnetyków
PL
Magnetyczne kompozyty proszkowe nabierają ostatnio szczególnego znaczenia jako materiały magnetyczne do wykonania magnetowodów urządzeń elektrycznych. Szczególnym zainteresowaniem, ze względu na ich właściwości, cieszą się dielektromagnetyki. W pracy przedstawiono zmiany wybranych właściwości mechanicznych, elektrycznych i magnetycznych dielektromagnetyków wykonanych przy zastosowaniu różnych rodzajów dielektryku, w postaci żywic epoksydowych, dodanych w ilości 0,5% wagowo. Wykorzystano dielektryki dotychczas niestosowane: Amicon SE 617, Araldit K-600 oraz używa­ne: Epidian 101 oraz Epidian 101 rozpuszczony w acetonie w proporcji 10 ml/g żywicy. W celach porównawczych wykonano wypraski bez dodatku dielektryku z proszku żelaza, tego samego, który stanowił bazę dla prezentowanych dielektromagnetyków. Dielektromagnetyki do badań wykonano jako próbki pierścieniowe (toroidalne) o wymiarach średnica 50 x średnica 60x5 mm, prasowane pod ciśnieniem 800 MPa i utwardzane w temperaturze 200°C w ciągu 2 godzin. Największe wartości gęstości (rys. 2) uzyskano dla kompozytów wykonanych bez dodatku dielektryku, duże dla Amiconu i Epidianu rozpuszczonego w acetonie. Zdecydowanie największą wartość rezystywności (rys. 3) uzyskano dla dielektryku Epidian/aceton, co dowodzi równomiernego rozprowadzenia warstwy tego dielektryku na powierzchniach proszku żelaza. Jest to wiec efektywny sposób izolowania cząstek magnetycznych. Zastosowanie pozostałych dielektryków, które są w formie bardzo drobnego proszku, nie powoduje tak dobrej izolacji cząstek magnetycznych. Rezystywność kompozytu bez dielektryku jest oczywiście bardzo mała. Brak dielektryku powoduje, że wytrzymałość na zginanie (rys. 4) jest niewielka (rzędu 70 MPa). Największą wartość wytrzymałości (rzędu 120 MPa) uzyskano przy zastosowaniu dielektryku Epidian/Aceton, a klejący wpływ Aralditu jest niewielki (wytrzymałość około 80 MPa), co może być wynikiem większej wielkości ziaren proszku Aralditu niż pozostałych (Amicon i Epidian). Na rysunkach 5-8 przedstawiono rozdział strat dielektromagnetyków przy indukcji 0,5 oraz 1 T dla częstotliwości 50 i 200 Hz. Wartości stratności korespondują z rezystywnościami wykonanych kompozytów. Najniższą stratność uzyskano dla dielektryków z Amiconem, zaś nieco wyższą dla dielektryku Epidian/aceton. Generalnie wartości stratności dla różnych dielektryków niewiele różnią się od siebie. Przy wyższej indukcji (rys. rys. 7 i 8) różnice dla poszczególnych dielektromagnetyków zacierają się, zwłaszcza dla częstotliwości 200 Hz (rys. 8). Charakterystyki magnesowania (rys. rys. 9 i 10) wykazują praktycznie jednakowe przebiegi dla wykonanych dielektromagnetyków zarówno przy 50, jak i 200 Hz. Gorszą charakterystykę magnesowania posiada dielektromagnetyk z dodatkiem Epidian/aceton. Przebiegi charakterystyk magnesowania przekładają się na wartości przenikalności magnetycznej (rys. rys. 11-14). Badania wykazały, że w zakresie badanych częstotliwości 50:200 Hz rodzaj zastosowanego dielektryku nie ma znaczącego wpływu na właściwości magnetyczne dielektromagnetyków. Może mieć on wpływ na niektóre właściwości, np. wytrzymałość mechaniczną czy rezystywność.
EN
Magnetic powder composites gather lately special meanings as materials for magnetic cores of electric devices. Special interest is focused on dielectromagnetics. Changes of selected mechanical, electric and magnetic properties of dielectromagnetics, executed at use of different kinds of dielectrics are presented in the paper. Various epoxy resins in quantities 0.5% by weight were used as dielectrics. It includes: Amicon SE 617, Araldit K-600 and epoxy resin which was used up till now: Epidian 101 in powder form and as diluted in acetone in proportion 10 ml/g of resin. In comparative aims one executed compacts from iron powder without addition of dielectric. This iron powder was the same as used as a base for other presented dielectromagnetics. Dielectromagnetics for tests were compacted in form of ring samples with dimensions diameter 50 x diameter 60 x5 mm. Applied compacted pressure was 800 MPa and samples were cured at temperature 200°C in the course of 2 hours. The greatest values of density (Fig. 2) were obtained for composite executed without addition of dielectric. Quite large values one can observe for Amicon and Epidian resins diluted in acetone. Decidedly the greatest values of resistivity (Fig. 3) were obtained for Epidian in acetone. It proves uniform distribution of dielectric layers on surfaces of iron powder. Thus this is the most effective manner of magnetic particles insulating. Use of remaining dielectrics, which are in form of very tiny powder, does not cause so good insulation of magnetic particles. Resistivity of the composite without a dielectric is of course very small. Lack of a dielectric causes, that bending strength of such composite (Fig. 4) is not big (around 70 MPa). The greatest value of bending strength (around 120 MPa) was obtained at use Epidian in acetone. Sticking ability of Araldit is not satisfactory (bending strength about 80 MPa), what can be a result of greater sizes of its grains if compare with remaining dielectrics (Amicon and Epidian). Distribution of dielectromagnetics energy losses at induction 0.5 and 1 T for frequencies 50 and 200 Hz are presented in Figures 5-8. Values of losses correspond with resistivity of executed composites. The lowest losses were obtained for dielectromagnetics with Amicon, while a little bit higher for Epidian in acetone. Generally values of losses for different dielectrics little differ from oneself. At higher value of magnetic induction (Figs.7 and 8), differences of losses for tested dielectromagnetics wear away, especially for frequencies 200 Hz (Fig. 8). Magnetization characteristics (Figs.9 and 10) show practically similar, if not saying identical courses for executed dielectromagnetics, both at 50 and 200 Hz. Worse characteristic exhibits dielcctromagnetic with addition of Epidian in acetone. Courses of magnetizing characteristics translate oneself on values of permeability (Figs 11-14). Research showed that, within the range of examined frequencies 50:200 Hz, kind of applied dielectric does not have significant influence on magnetic proprieties of tested dielectromagnetics. It can have more essential influence on such proprieties as mechanical strength or resistivity.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.