Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 5

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  destructive method
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
This paper presents the analysis of the results of research on concrete compressive strength on cubic samples, in the early stage of its curing (after 7, 14, and 28 days). The analysis considers the variable water-cement ratio. Statistical and strength parameters were assessed, estimating the quality of the obtained concrete at the same time. Verification of the expected C25/30 concrete grade was carried out from the recipe provided by the prefabrication plant. Then, the grammage of individual components was adjusted to obtain the grade of concrete assumed by the authors. The article estimates the concrete grade based on strength parameters in three stages of concrete curing. The concrete was then compared with the concrete class calculated based on standard procedures (EC2 procedures), which could be reached after 28 days. The paper also provides an overview of the most used methods of testing concrete compressive strength.
PL
W artykule przedstawiono analizę wyników uzyskanych z badania wytrzymałości betonu na ściskanie na próbkach sześciennych we wczesnej fazie jego dojrzewania (po 7, 14 i 28 dniach), z uwzględnieniem zmieniającej się wartości stosunku wodno-cementowego. Dokonano oceny parametrów zarówno statystycznych jak i wytrzymałościowych, szacując przy tym jakość produkcji otrzymanego betonu. Przeprowadzono weryfikację oczekiwanej klasy betonu C25/30, z udostępnionej przez zakład prefabrykacji receptury, a następnie zmieniono gramaturę poszczególnych jej składników w celu uzyskania założonej przez autorów klasy betonu równej C20/25. W artykule oszacowano klasę betonu na podstawie parametrów wytrzymałościowych w trzech stadiach czasowych i porównano ją z wyznaczoną według przepisów normowych wartością, która mogłaby zostać osiągnięta po 28 dniach. Otrzymane wyniki badań porównano z wyznaczonymi zgodnie z normą Eurokod 2 wartościami wytrzymałości, które mogłaby zostać osiągnięte po 28 dniach i oszacowaną na tej podstawie klasą betonu. W pracy dodatkowo przedstawiono przegląd najczęściej stosowanych metod badań wytrzymałości betonu na ściskanie.
PL
W artykule przedstawiono wyniki badań diagnostycznych elementu betonowego poddanego działaniu pożaru. Przeprowadzono ocenę przydatności wybranych metod, głównie nieniszczących, lecz także niszczących, stosowanych do oceny stanu betonu poddanego działaniu wysokiej temperatury. Celem badań było również ustalenie zależności między wybranymi parametrami diagnostycznymi (prędkość rozchodzenia się dźwięku w materiale, liczba odbicia) i resztkowymi właściwościami mechanicznymi uszkodzonego betonu. Stwierdzono dużą zgodność prędkości rozchodzenia się ultradźwięków przy skrośnym ich przepływie, z wytrzymałością próbek na ściskanie, ponadto metoda ultradźwiękowa pozwoliła na ocenę zwartości warstwy betonu uszkodzonego.
EN
The article presents the results of diagnostic tests of the concrete elements, subjected to fire. The assessment of selected methods suitability, mainly non-destructive, but also some destructive, used to determine the properties of the concrete subjected to high temperature, was verified. The aim of the study was to determine the relationship between selected diagnostic parameters (ultrasonic pulse veIocity, rebound number) and the residual mechanical properties of the damaged concrete. It was found that ultrasonic pulse velocity in direct transmission is compliant with specimen compressive strength, moreover, this method allowed to determine the thickness of the damaged concrete layer.
3
Content available remote Ocena stopnia uszkodzenia stali 40HNMA metodami nieniszczącymi i niszczącymi
PL
W artykule przedstawiono próbę oceny stanu degradacji mechanicznej i strukturalnej stali 40HNMA, stosowanej m.in. w przemyśle motoryzacyjnym, metodami nieniszczącymi i niszczącymi. Szczególny nacisk położono na nowoczesne badania ultradźwiękowe i magnetyczne.
EN
This work presents an attempt to evaluate a stage of mechanical and structural degradation of 40HNMA steel, used for example in automotive industry, by means of non-destructive and destructive methods. The modern ultrasonic and magnetic investigation were mainly applied.
4
Content available remote Numerical estimation of internal stress relieving in destructive test
EN
The paper deals with the analysis of residual stress fields in the riveted joint and the estimation of the internal stress magnitude releasing by partial and complete removing of the rivet material. Stress relieving causes deformations around the rivet hole, which can be measured and compared to the deformation state before removal. Numerical FE simulations of the upsetting process are carried out to determine the residual stress and strain fields. The contact with friction is defined between the mating parts of the joint. Non-destructive testing methods are used in combination with numerical calculations.
PL
W pracy przedstawiono metodykę i wyniki badania obwodowych naprężeń własnych w wytłoczkach tłoczonych z blachy stalowej 08XA. Badano rodzaj i wielkość obwodowych naprężeń własnych w zależności od odległości od powierzchni ścianki. Do badań zastosowano metodę niszczącą polegającą na trawieniu kolejnych warstw wytłoczki.
EN
The article presents the method and the results of examination of residual stresses in diestampings stamped from 08XA steel sheet. The magnitude or circumferential residual stresses was examined as dependent on the distance from the wall surface. A destructive method was employed in the tests, which involves etching the successive layers of the diestamping.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.