Content available remote Weld defects and precipitates of deposited metal in 9Ni steel welded joint
EN
Three kinds of electrode with different niobium contents were developed and compared, and the influence of alloying elements on microstructure and mechanical properties was summarized. Strong carbide elements such as Nb, Ti, and V were added to form stable precipitates. The existence of intercrystalline precipitates leads to pinning and zigzag of grain boundaries, hinders the propagation of cracks, and enhances the low temperature strength and impact toughness of the materials. The No. 1 and No. 2 ENiCrMo-6 electrodes meet the requirements of LNG (liquified natural gas) equipment. The tensile strength of the deposited metal reaches 687 MPa, while the average impact energy at −196°C is 131 J. Owing to fluctuations in the stress concentration at the junction of grain boundaries, cracks may easily form. MC carbide can retard the crack propagation. With the increase of Nb and other alloys, the strength and hardness increase gradually, but the plasticity and toughness are retarded to a certain extent.
PL
Jedną z perspektywicznych technik wykonywania prac naprawczych pod wodą jest spawanie metodą lokalnej komory suchej. Ze względu na miejscowe odizolowanie miejsca spawania od kontaktu z wodą, warunki stygnięcia i zawartość wodoru w złączach są zbliżone do spawania w środowisku powietrznym. W artykule zaprezentowano stan wiedzy oraz wyniki badań wstępnych dotyczących wpływu warunków spawania na ilość wodoru dyfundującego w stopiwie otrzymanym metodą lokalnej komory suchej. Zastosowanie planu Placketta - Burmana pozwoliło na ocenę statystycznej istotności wpływu siedmiu wybranych czynników: ilości zwojów opaski elastycznej, długości wolnego wylotu drutu elektrodowego, natężenia prądu spawania, napięcia łuku, prędkości spawania, zasolenia wody oraz wydatku gazu osłonowego.
EN
One of the methods with great potential for applications in underwater repairs is local cavity welding. In local cavity method cooling conditions and diffusible hydrogen amount in weld metal are nearly the same as those existed during welding in the air. Article presents results of literature survey and preliminary tests of effect of local cavity welding conditions on diffusible hydrogen amount in deposited metal. A Plackett-Burman design was applied to screen seven parameters: thickness of elastic cover, stick-out of electrode wire, welding current, voltage, travel speed of welding, salinity of water and flow rate of shielding gas.
PL
Omówiono zależność pomiędzy stężeniem tlenu w stopiwie elektrod otulonych rutylowych i zasadowych a wielkością wtrąceń niemetalicznych. Wyprowadzono wzór matematyczny pozwalający obliczyć średnicę wtrącenia niemetalicznego w stopiwie w zależności od ilości tlenu.
EN
Relation between concentration of oxygen in basic and rutile weld metal deposit and size non metalic inclusions were discussed. Furthermore mathematical equation allowing to calculate diameter of non metalic inclusion in metal weld deposit in terms of oxygen concentration in MWD have been done.
PL
Mokre spawanie pod wodą znajduje stosunkowo szerokie zastosowanie w praktyce. Poza zwiększoną prędkością stygnięcia złączy najpoważniejszym ograniczeniem spawalności stali w środowisku wodnym jest wysoka zawartość wodoru dyfundującego w stopiwie. Przedstawiono wyniki badań rozpoznawczych wpływu warunków spawania mokrego elektrodą otuloną na ilość wodoru dyfundującego. Dzięki zastosowaniu planowania doświadczeń (plan Placketta-Burmana) zbadano ilościowy i jakościowy wpływ siedmiu wybranych czynników na generowaną ilość wodoru. Analiza statystyczna wykazała, że największe znaczenie ma zasolenie wody, zanieczyszczenie elektrody, biegunowość i natężenie prądu spawania.
EN
Wet welding is the most popular method of joining in water environment. During underwater joining weldability of steel is limited by higher cooling rates and hydrogen content in weld metal. In article results of preliminary tests of effect of wet welding conditions on diffusible hydrogen amount are presented. Seven parameters were optimized using a Plackett-Burman design to get the most relevant variables. These parameters were: salinity of water, contamination of electrode, electrode polarity and welding current.