Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 8

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  cyclic deformation
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
Two single crystals with compositions Fe-Ni-Co-Al-Ta and Fe-Ni-Co-Al-Ta-B were selected and fabricated by Bridgman method. Subsequently, ingots were homogenized, oriented and subjected to a two-step heat treatment process in order to obtain fine and coherent γ' precipitates. Subsequently, superelastic cycling experiments were performed at 77 K. The next step included detailed microstructural characterization using transmission electron microscopy and high-energy synchrotron X-ray diffraction measurements together with Rietveld refinement. The results show that the number of fully reversible superelastic strains is very sensitive to the size of γ' precipitates. The smaller (3 nm) γ' precipitates ensured more superelastic response compared to material with larger γ' particles size (5 nm), in which the material did not receive its original shape after 10 cycles even after being heated.
EN
After washing cycles, textiles having minimum deformation, maximum dimensional stability and the same performance of an unused product are major expectations of customers. This study examined the effects of washing cycles on the cyclic deformation of elastane knitted fabrics in detail. 12 knitted fabrics with two different linear densities of viscose yarn and three different polyamide/elastane gimped yarn of two different tightness levels (normal and tight) were used in the experiments. M&S P15A test method were used to evaluate the cyclic deformation of unwashed and washed fabrics (0, 5, 15 and 25 cycles) for four different recovery time periods (0 min, 2 min, 30 min and 24 h). Dimensional change, tightness factor and mass per unit area values were also examined in order to investigate the residual deformation of the fabrics after each washing stages. Consequently, it is determined that the fabrics having 21 tex viscose ground yarn and 78dtex20f elastane gimped yarn with higher setting show less residual extension (%). 5 and 15 washing cycles and a 30 min. recovery time are found significant for all repeated washings.
PL
Główne oczekiwanie klientów to minimalne odkształcenie i maksymalna stabilność wymiarowa po wielokrotnych cyklach prania. W pracy szczegółowo zbadano wpływ cykli prania na deformację dzianin elastycznych. W doświadczeniach zastosowano 12 dzianin o dwóch różnych gęstościach liniowych przędzy wiskozowej i trzech różnych przędz rdzeniowych z poliamidu /elastanu o dwóch różnych poziomach naprężenia. Metodę M&S P15A zastosowano do oceny cyklicznej deformacji nie pranych i pranych próbek (0, 5, 15 i 25 cykli) w czterech różnych okresach czasu (0 min, 2 min, 30 min i 24 h). W celu zbadania resztkowego odkształcenia próbek po każdym praniu zbadano m.in. zmiany wymiarów. Stwierdzono, że 5 i 15 cykli prania i 30 min. czas regeneracji jest znaczący dla wszystkich powtarzanych prań.
EN
Specimens of the austenitic steels AISI 304, 321 and 348 were investigated in total-strain control fatigue tests in the temperature range from -60°C to 25°C. The fatigue behavior and phase transformation from paramagnetic austenite to ferromagnetic martensitewere investigated by means of stress-strain hysteresis, electrical resistance and magnetic measurements. The influence of the testing temperature on the cyclic deformation behavior and phase transformation is shown in Fig. 1. Due to a decrease in temperature an increase of the stress amplitude occurs. The pronounced cyclic hard- ening can be correlated with two phenomena, an increase of the amount of martensiteand the cyclic hardening of not transformed austenite.
4
EN
In order to develop a two-way rotary shape memory alloy thin strip actuator, the torsional deformation and fatigue properties of a TiNi SMA thin strip were investigated. The results obtained are summarized as follows. (1) In the SMA thin strip subjected to torsion, the MT appears along the edge of the strip due to elongation of the edge of the strip and grows to the central part. (2) The number of cycles to failure decreases with an increase in the maximum angle of twist in torsion fatigue. The fatigue life in pulsating torsion is longer than that in alternating torsion by five times. The fatigue limit exists in a certain value of dissipated work of the strip in each cycle. (3) Based on the two-way motion of a lifting actuator model driven by two kinds of SMA thin strip, it is confirmed that the two-way rotary actuator with a small and simple mechanism can be developed by using the SMA thin strips.
PL
Wpracy zbadano termomechaniczne właściwości skręcania i zmęczenia stopu TiNi z pamięcią kształtu (SMA) w celu zbudowania skrętnego siłownika taśmowego zaprojektowanego na bazie dwukierunkowego efektu pamięci kształtu. Otrzymane wyniki podsumowano w sposób następujący. (1) W cienkich taśmach SMA poddawanych skręcaniu, przemiana martenzytyczna (MT) inicjuje się na krawędzi taśmy w związku ze składową rozciągania, a następnie rozwija w kierunku jej środka. (2) W badaniach zmęczeniowych ilość cykli do zniszczenia maleje wraz ze wzrostem maksymalnego kąta skręcania. Wytrzymałość na męczenie w przypadku skręcania pulsującego jest pięciokrotnie dłuższa niż w przypadku obciążania symetrycznego. (3) Przeprowadzone badania dwukierunkowego ruchu na zaprojektowanym modelu siłownika poruszanego przy pomocy dwóch rodzajów cienkiej taśmy SMA potwierdziły możliwość zbudowania skrętnego siłownika z małym i prostym mechanizmem na bazie dwukierunkowego efektu pamięci kształtu.
5
Content available remote Torsional deformation and rotary driving characteristics of SMA thin strip
EN
The torsional deformation properties of a TiNi shape-memory alloy thin strip were investigated. The results obtained are summarized as follows. (1) The martensitic transformation starts at the edge of the thin strip. (2) The torsional deformation properties change slightly under thermomechanical cycling. (3) The fatigue life in pulsating torsion is longer than that in alternating torsion. (4) A simple rotary driving element can be developed by using the SMA thin strip.
6
Content available remote Tensile or compressive plastic deformation of cylinders assisted by cyclic torsion
EN
Technological metal forming processes of extrusion, forging and rolling with imposed cyclic torsion or shear deformation have been recently studied in view of their advantages with respect to monotonic loading processes, cf. Bochniak and Korbel [2-4]. The present work is aimed to analyze such process in the case of simple tension or compression of a cylindrical tube with imposed cyclic torsional deformation. The material element response is assumed to be rigid-perfectly plastic or elastic-perfectly plastic. For these models, the analytical solutions can be provided for the steady cyclic responses and the effect of two process parameters, namely the ratio of shear and axial strain rates ... and the amplitude of shear strain ... , can be clearly demonstrated. Three different regimes of cyclic response can be visualized in the plane ... , ... . The cyclic response of a cylinder under combined axial compression and cyclic torsion is predicted by considering a simplified model of a set of concentric tubes and neglecting their radial stress interaction. The axial force and torsional moment are then specified by averaging the responses of consecutive tubes. The cyclic response diagrams for the cylinder are then generated in terms of axial force and torsional moment related to axial deformation and angle of twist.
EN
Two different principles of TMF-testing were investigated for the wrought aluminium alloy AlCuBiPb (2011). In the first testing method the specimens are clamped in a stiff load frame. A cyclic temperature load is applied, which leads to an out-of-phase (OP) TMF loading. The local strain is measured within the parallel cross section of the specimen. The second series of OP-TMF tests are conducted using closed loop strain control on a servo-hydraulic TMF testing system, which guarantees a rigid restraint condition within the parallel section of the specimen. To compare these two principles of TMF-testing, additional experiments were conducted with different mechanical strain amplitudes. The two experiments can be compared well, when the local strains are taken into account. Therefore, the method of the rigid clamped specimen can be used to get experimental data in a wide range of strain amplitudes.
PL
Badano dwie różne metody termomechanicznych testów zmęczeniowych (TMF) dla stopów aluminiowych do obróbki plastycznej AlCuBiPb (2011). W pierwszej z badanych metod próbki materiału są mocowane w sztywnej ramie obciążeniowej. Stosuje się cykliczne obciążenie temperaturowe, które wywołuje niezsynchronizowane fazowo obciążenie termomechaniczne (OP TMF). Lokalne naprężenia są mierzone w obrębie równoległego przekroju próbki. W drugiej z przeprowadzonych serii testów OP TMF zastosowano zamkniętą pętlę sterowania naprężeniem w systemie serwomechanizmu hydraulicznego do termomechanicznych badań zmęczeniowych, co gwarantowało sztywne spełnienie warunku granicznego w równoległym przekroju próbki. Aby porównać dwie wymienione zasady testów TMF przeprowadzono dodatkowe eksperymenty przy różnych amplitudach naprężeń mechanicznych. Obydwa eksperymenty dają porównywalne wyniki, gdy uwzględni się naprężenia lokalne. Metoda, w której próbki mocuje się w sztywnej ramie, może więc być użyta dla uzyskania danych eksperymentalnych w szerokim zakresie amplitud naprężenia.
8
Content available remote Badanie zmęczenia niskocyklowego stopu Al-Li-Cu-Zr
PL
Badano trwałość niskocyklową próbek klepsydrowych z przemysłowego stopu Al-Li-Cu-Zr przy sterowaniu odkształceniem poprzecznym ∆ε'ac = const. Analizowano zależności zmiany pętli histerezy w procesie niskocyklowego zmęczenia, istotne z punktu widzenia kryteriów energetycznych trwałości. Wyznaczono współczynnik wytrzymałości zmęczeniowej K' oraz wykładnik cyklicznego wzmocnienia n'. Sporządzono wykres cyklicznego odkształcenia dla badanego stopu uwzględniający orientację próbek względem kierunku walcowania arkusza materiału.
EN
Low cycle fatigue lifeunder laterial deformation ∆ε'ac = const. condition of Al-Li-Cu-Zr commercial alloy hourglass specimens was investigated. Relations of hysteresis loops changes during fatigue process were analyzed as a significant from an energetic criteria view point. The fatigue strength coefficient K' and cyclic hardening exponent n' were determined based on the experimental data. A plot of cyclic strain curve for tested material was made taking into account a different rolling sheet orientation of the specimens.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.