Flax fibres from Celitex have been obtained using a conventional line in Spain. Measurements have been made after tearing and carding. The same fibre has been processed in the Technical University of Lodz and measurements have been made also after tearing, carding and cottonized fibre. Values of fineness and length measured using Image analysis, water absorption and thermal behaviour by DSC are reported on this paper. Some relationships are studied.