EN
The material recycling due to the environmental protection and sustainable development is playing an increasingly important role in the road pavement construction. This is especially true for the use of reclaimed asphalt pavement (RAP) materials for the pavement construction layers. One of the problems encountered in the use of larger quantities of the RAP in asphalt mixtures is the deterioration of their workability and homogeneity especially in the case of cold dosing of RAP. The paper reports the results of a study on the use of additives to improve the workability of asphalt concrete for the subbase layer with an increase of up to 40% in crushed RAP content, dosed in the cold technology. In the study, additives of the F-T waxes, plant-derived liquefiers and zeolites were used to improve homogeneity and compactability of the mixtures using reduced paving temperatures. An evaluation of the compactability of mixtures with different contents of the RAP, using 3 types of additives to improve workability, was carried out. Compactability was evaluated by the compaction analysis in a gyratory compactor, determining, among other things, the required number of cycles to achieve the required compaction, as well as the shear stress and compaction index as a function of the number of compaction cycles. Subsequently, the asphalt mixtures were tested to verify their resistance to permanent deformation and resistance to water. Based on the results of the research and analysis, it was shown that it is possible to use increased RAP materials content in asphalt concrete base layers at both standard and reduced paving temperatures, through the use of additives that improve the workability and compactability of the mixtures.
PL
Recykling materiałowy ze względu na ochronę środowiska, zrównoważony rozwój odgrywa coraz większe znaczenie w budowie nawierzchni drogowych. Szczególnie dotyczy to zastosowania destruktu asfaltowego do warstw konstrukcyjnych nawierzchni. Jednym z problemów występujących przy stosowaniu większych ilości destruktu asfaltowego w mieszankach mineralno-asfaltowych jest pogorszenie ich urabialności i jednorodności szczególnie w przypadku dozowania granulatu asfaltowego na zimno. Artykuł zawiera wyniki badań nad zastosowaniem dodatków poprawiających urabialność betonu asfaltowego do warstwy podbudowy ze zwiększonym do 40% dodatkiem granulatu asfaltowego dozowanym w technologii na zimno. W badaniach zastosowano dodatki parafin F-T, upłynniaczy pochodzenia roślinnego oraz zeolitów, które miały na celu poprawę homogeniczności i zagęszczalności mieszanek przy zastosowaniu obniżonych temperatur wbudowania. Przeprowadzono ocenę zagęszczalności mieszanek z różną zawartością granulatu asfaltowego przy zastosowaniu 3 rodzajów dodatków poprawiających urabialność. Zagęszczalność oceniano na podstawie analizy przebiegu zagęszczania w prasie żyratorowej, określając m.in. wymaganą ilość cykli do uzyskania wymaganego zagęszczenia, a także naprężenia ścinające oraz wskaźnik zagęszczenia w funkcji ilości cykli zagęszczania. W dalszej kolejności mieszanki mineralno-asfaltowe poddano badaniom w celu weryfikacji ich odporności na deformacje trwałe oraz działanie wody. Na podstawie wyników badań i analiz wykazano, że istnieje możliwość stosowania zwiększonej zawartości granulatu asfaltowego w warstwach podbudowy z betonu asfaltowego zarówno w standardowych, jak i obniżonych temperaturach wbudowania dzięki zastosowaniu dodatków poprawiających urabialność i zagęszczalność mieszanek.
EN
A statistical approach was conducted to investigate effect of independent factors of the mixing time compactability and bentonite percentage on dependent variables of permeability, compression and tensile strength of sand mould properties. Using statistical method save time in estimating the dependent variables that affect the moulding properties of green sand and the optimal levels of each factor that produce the desired results. The results yielded indicate that there are variations in the effects of these factors and their interactions on different properties of green sand. The outcomes obtained a range of permeability values, with the highest and lowest numbers being 125 and 84. The sand exhibited high values of tensile and compressive strength measuring at 0.33N/cm2 and 17.67N/cm2 . Conversely it demonstrated low levels of tensile and compressive strength reaching 0.14N/cm2 and 9.32N/cm2 . These results suggest that the moulding factors and their interactions have an important role in determining properties of the green sand. ANOVA was used to assess effect of various factors on different properties of the green sand. The results obtained suggest that compactability factor play a significant effect on permeability, the mixing time or bentonite factor has a significant effect on the compressive strength and mixing time or compactability factor has a significant impact on the tensile strength with a significance level lower than 5%. It is found that neither the mixing time nor the amount of bentonite used in the green sand mix has a significant impact on its permeability. Compactability of the green sand does not has a significant effect on the compressive strength. Bentonite used in green sand mix does not have a significant impact on its tensile strength.
EN
Sand Casting process depends mainly on properties of the green sand mould, sand casting requires producing green sand mould without failure and breakage during separation the mould from the model, transportation and handling. Production of the green sand mould corresponding to dimensions and form of the desired model without troubles depends on the properties of the green sand. Ratio of constituents, preparation method of the green sand, mixing and pressing processes determine properties of green sand. In the present work, study effect of the moulding parameters of bentonite content, mixing time, and compactability percentage on the properties of the green sand mould have been investigated. Design of experiments through Taguchi method was used to evaluate properties of permeability, compressive strength, and tensile strength of the green sand. It was found that 47% of compactability, 9(min) of mixing time, and 6% of bentonite content gives highest values of these properties simultaneously.
EN
The production of castings by green sand moulds is a very important method for the manufacture of final products for different sectors of industry. In this green sand moulding process the quality of castings depends strongly on the quality of the mould, which in turn is determined by parameters such as the type of foundry machine, the characteristics of the moulding sand and the specifications of the patterns. The mould’s stability for use casting is achieved by filling and compacting moulding sand. This means, that the clay-bonded moulding sand is changed from the free flowing to the compacted state. In this process flowability is a very important parameter. Therefore, a variety of methods for the determination of flowability have been in use. However, it is fair to say that these methods do no longer meet the requirements of the modern moulding process. This paper introduces a new method for the determination of flowability of clay-bonded moulding sand using a specifically designed type of density sensor that was developed by a research team led by Professor Jürgen L. Bast at the Mechanical Department of Technical University Bergakademie Freiberg. The high levels of accuracy in the determination of flowability that this method is capable of achieving have been tested and indeed proven by varying sand parameters such as water and clay content, grain composition, mixing time, and compaction pressure. A further innovative characteristics of this new method of sensor-based flowability measurement is the possibility of using the sensor not only for the lab-based testing of sands but in the actual mould during the production process in the foundry, which allows to determine whether the sand in the mould has the required qualities based on real-time flowability measurements.
PL
Produkcja odlewów w formach wilgotnych jest bardzo ważna metodą w wytwarzaniu finalnych wyrobów w wielu dziedzinach przemysłu. W procesie formowania ”na wilgotno” jakość odlewów zależy istotnie od jakości formy, która z kolei jest określona przez takie parametry jak: rodzaj maszyny formierskiej, charakterystyka masy formierskiej oraz parametry modeli. Stabilność formy odlewniczej jest osiągana podczas wypełniania przestrzeni technologicznej oraz zagęszczania masy formierskiej. Oznacza to zmiane stanu masy formierskiej od stanu luźno usypanego do stanu zagęszczonego. W tych procesach płynność masy jest bardzo ważnym parametrem. Dlatego też, stosowanych jest wiele metod określania płynności masy. Trudno jest jednak stwierdzić, że metody te spełniają wymagania nowoczesnych procesów formowania. W artykule zaprezentowano nową metodę określania płynności mas z lepiszczem, wykorzystującą specjalnie zaprojektowany czujnik zagęszczenia - opracowany w zespole badawczym kierowanym przez Profesora Jürgena Basta na Wydziale Mechanicznym Uniwersytetu Technicznego (Akademii Górniczej) we Freibergu. Wysoki poziom dokładności określania płynności, który może być osiągany w tej metodzie, został wykazany badaniami testowymi, przy zmiennych parametrach: wilgotności masy i zawartości lepiszcza, składu ziarnowego osnowy, czasu mieszania masy oraz wartościach nacisków podczas zageszczania. Kolejne cechy innowacyjne tej nowej metody określania płynności z zastosowaniem wspomnianych czujników to możliwość jej wykorzystania nie tylko w warunkach badan laboratoryjnych masy, ale również podczas procesu wytwarzania form w odlewni. Umożliwia to określenie w czasie rzeczywistym, czy masa wykorzystywana w procesie formowania ma wymagana jakość.
EN
The paper presents results of investigations carried out on compaction ability of colliery spoils from Sośnica mine. Laboratory tests were carried out in semi-size and standard Proctor apparatuses. Aim of the project was determination the influence of choosen factors on compation parameters and their usability for engineering purposes.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.