Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 1

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  coagulation bath
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
An analysis was carried out concerning the influence of coagulation bath temperature on the porous structure and the sorption & strength properties of polyacrylonitrile (PAN) fibres which include montmorillonite (MMT). We stated that fibres formed at a temperature of 25 °C were characterised by maximum tenacity at the level of 19 cN/tex. Obtaining fibres with increased total pore volume up to 0.34 cm3/g, which is beneficial for the medical purposes of the carbon fibres obtained from the PAN fibres discussed, requires the solidification process to be conducted in a coagulation bath at a temperature of 35 °C.
PL
Przeprowadzono analizę wpływu temperatury kąpieli zestalającej na strukturę porowatą, właściwości sorpcyjne i wytrzymałościowe włókien PAN z montmorylonitem. Stwierdzono, że najwyższą wytrzymałość właściwą na poziomie 19 cN/tex charakteryzują się włókna formowane w temperaturze 25 °C. Uzyskanie całkowitej objętości por podwyższonej do 0,34 cm3/g korzystnej ze względu na medyczne przeznaczenie włókien węglowych otrzymywanych w dalszych procesach z badanych włókien PAN wymaga prowadzenia procesu zestalania w kąpieli o temperaturze 35 °C.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.