Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 16

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  chloride ions
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
In hydrometallurgy, precipitation would be easier and simpler than solvent extraction as a separation operation. In this work, the separation performance of Co(II), Mn(II) and Ni(II) by oxidative precipitation was investigated. For this purpose, NaClO was employed as an oxidizing agent and the separation behavior of the three ions was compared between chloride and sulfate solutions by varying some factors such as the dosage of NaClO, solution pH and reaction temperature. By controlling the molar ratio of NaClO to Mn(II), Mn(II) were easily separated as MnO2 by oxidative precipitation from both chloride and sulfate solutions. At the same experimental conditions, precipitation percentage of Co(II) from chloride solution was higher than that from sulfate solution, which can be ascribed to the stronger tendency of Co(II) to form complexes with chloride ion than with sulfate ions. Addition of NaCl to sulfate solution and oxidative precipitation at high temperature enhanced the precipitation percentage of Co2O3 and thus separation degree between Co(II) and Ni(II) was improved. Under the optimum conditions, MnO2 and Co2O3 powders with 99.9% purity were completely recovered by oxidative precipitation from chloride solution. By contrast, the purities of the MnO2 and Co2O3 thus recovered from sulfate solution were only 76 and 91%, respectively. Our results indicated that chloride solution would be more effective than sulfate solution in separating Mn(II) and Co(II) by oxidative precipitation with NaClO. Therefore, the use of chloride-based leaching solutions such as HCl and FeCl3 might be better for the leaching medium of spent lithium-ion batteries.
PL
W pracy przedstawiono badania zawartości chloru w betonie i proces korozji, w oparciu o pomiary oporu przewodnictwa elektrycznego i potencjału półogniwa próbek betonowych. Te analizy opierały się na doświadczalnych pomiarach próbek w funkcji czasu zanurzenia w 3,5% roztworze NaCl w wodzie, w temperaturze pokojowej, przez 18 miesięcy, zgodnie z europejskimi normami. Przygotowano mieszanki betonowe o różnym składzie, do których dodawano inhibitor, jakim był azotan wapnia i dwa rodzaje superplastyfikatorów. Wyniki doświadczeń pokazały, że po sześciu miesiącach zanurzenia próbki miały dużą zawartość jonów chlorkowych. Próbki C4 z dodatkiem 3% inhibitora i superplastyfikatora w formie Oxydtronu, jak również C3 z tym samym dodatkiem inhibitora i superplastyfikatora MAPEI Dynamon SR 31, wykazały dobrą odporność na korozję, w stosowanym roztworze NaCl. Znalazło to również potwierdzenie w serii pomiarów przewodnictwa elektrycznego i potencjału półogniwa, przeprowadzonych po doświadczalnym okresie 18 miesięcy.
EN
This work presents a study of the total chloride contents in concrete and the corrosion process by testing electrical resistivity and half-cell potential of concrete samples. The analysis was based on an experimental investigation of the samples with the time of immersion in 3.5% mass NaCl aqueous solution at room temperature for 18 months, according to European Standards. For this study, different mixtures of concrete were prepared by adding two types of superplasticizers and calcium nitrate inhibitor, in different concentrations. The results of the Cl- ions test showed that all the samples, after an immersion testing period of six months, contained high concentrations of Cl- ions. Samples C4 with 3% calcium nitrate inhibitor and Oxydtron superplasticizer as well as C3 with 3% calcium nitrate inhibitor and Mapei Dynamon SR 31 superplasticizer, showed good resistance to corrosion, in the tested environment. It was also proved by the results of several sets of measurements of the electrical resistivity and half-cell potentials carried on the concrete test samples, to the end of the 18 months testing period.
EN
In this paper, results of adsorption kinetic studies of Pd(II) chloride complex ions on activated carbon Organosrob 10 CO are presented. Spectorphotometrical method was applied to investigate the process. Kinetic model was proposed, and fundamental thermodynamic parameters were determined. Proposed kinetic model describes well observed phenomenon in the studied range of concentration of Pd(II) chloride complex ions as well, as concentration of activated carbon.
5
Content available remote Wpływ zasolenia piaskowca na rozwój grzybów pleśniowych
PL
W artykule opisano wpływ łącznego działania dwóch środowisk agresywnych. Określono wpływ zawartości jonów siarczanowych lub chlorkowych na wzrost mikroorganizmów i ewentualny wpływ chemicznej i biologicznej korozji na właściwości materiału kamiennego (piaskowca). Prezentowane wyniki badań pozwoliły sformułować kilka stwierdzeń: piaskowiec nie jest odporny na zanieczyszczenie jonów siarczanowymi ani chlorkowymi. Skażenie chemiczne powoduje przyspieszenie działania środowiska mikrobiologicznego.
EN
This paper describes the effects of the combined action of two aggressive environments. The effect of sulphate or chloride ion content on the growth of microorganisms and possible effect of chemical and biological corrosion on the properties of stone material (sandstone). The research results made it possible to formulate a number of statements: sandstone is not resistant to contamination by sulphate or chloride ions. Chemical contamination enhances the action of the microbial environment.
EN
Chlorides content in cement is related to the production process – the sources of chlorides are mainly fuels, especially alternative fuels. Some chlorides are drawn off with by-pass powder, which is a by-product not easy for utilization. To reduce the production of environmentally noxious waste, cement producers attempt to increase the chloride content in ground granulated blast furnace slag cement (CEM III) above the value of 0.10% by weight. In European standard (EN 197-1) the limit value of chloride content in cement is generally 0.10% by mass, however, for CEM III there is a note in this standard which permits higher content of chlorides in this type of cement. The accelerated tests on the effect of the chloride content in CEM III, in the range of 0.1 – 0.5%, on the chemical resistance of concrete in solutions simulating acid rain and wastewater were performed. The solution of nitric acid and sulfuric acid was used as a solution simulating the acid rain. Solution simulating the wastewater contained ammonium sulfate, magnesium sulfate and sulfuric acid. After five weeks of exposure of concrete to corrosive solutions, weight change and the strength of the concrete samples were determined. No significant effect of the chloride content in cement over a range of tested values on the chemical resistance of concrete in environment simulating acid rain and wastewater was found.
PL
Przedstawiono wyniki badań odporności korozyjnej staliw wysokochromowych w stanie surowym w warunkach oddziaływania środowiska o wysokiej koncentracji jonów chloru. Takie warunki pracy występują najczęściej w kopalniach, gdzie maszyny górnicze narażone są na działanie wód zawierających duże ilości substancji negatywnie wpływających na trwałość elementów maszyn ciężkich. Większość części maszyn górniczych, oprócz narażenia na korozję, jest dodatkowo obciążona mechanicznie i podlega zużyciu ściernemu. Prezentowane badania dotyczą staliw, które dzięki połączeniu dobrej odporności korozyjnej z podwyższoną odpornością na ścieranie mogą być stosowane na elementy maszyn górniczych oraz innych maszyn ciężkich.
EN
The corrosion resistance studies of high-chromium cast steels for as-cast state in high-chloride concentration environment are presented. Such conditions can be found mainly in mining industry, where the heavy machinery parts are subjected to water containing high quantity of substances negatively affecting their durability. Most of the working elements are also mechanically loaded and subjected to wear. Presented studies concerned cast steels, which thanks to combined proper corrosion resistance and high wear resistance can be applied for heavy machinery parts used in mining and other heavy machinery industry.
8
Content available remote Stężenie chlorków w betonie a zagrożenie korozją zbrojenia
PL
Przedmiotem referatu jest przegląd światowych wymagań normowych dotyczących dopuszczalnego stężenia chlorków w elementach żelbetowych i sprężonych, z uwzględnieniem innych czynników. Rozważono czynniki decydujące o wartości krytycznego stężenia chlorków wystarczającej do zainicjowania korozji stali. Przedstawiono porównanie wyników badań dotyczących krytycznego stężenia chlorków inicjującego korozję z dopuszczalnymi wartościami normowymi.
EN
The subject of this paper is an overview of the world standards requirements for concentration of chlorides in reinforced and prestressed elements, taking into account other factors. Factors affected on the level of the critical concentration of chloride sufficient to initiate corrosion of steel were considered. The results of tests for a critical chloride concentration initiating steel corrosion and standard limits were compared.
9
Content available remote Ocena szybkości korozji stali zbrojeniowej w środowisku chlorku amonu
PL
Przedstawiono wyniki badań potencjokinetycznych i grawimetrycznych stali St3 eksponowanej w środowiskach chlorkowych. W wyniku przeprowadzonych badań grawimetrycznych najwyższe wartości szybkości korozji stal St3 uzyskała w środowisku chlorku amonu o pH ok. 5.
EN
Corrosion rates for St3 steel in the environments containing chloride ions were presented. The most corrosive environment was ammonic chloride solution, pH = 5. Tests were provided by using two investigation methods: gravimetric and potentiokinetic.
PL
W wyniku współspalania węgla i biomasy, uzyskuje się popioły lotne o właściwościach fizykochemicznych odmiennych w porównaniu z typowymi popiołami lotnymi, W referacie przedstawiono wyniki badań laboratoryjnych zastosowania do produkcji betonu popiołów lotnych powstających w wyniku współspalania węgla kamiennego i biomasy drzewnej. Przeanalizowano wpływ badanych popiołów lotnych na proces narastania wytrzymałości betonów cementowych oraz oddziaływanie tych popiołów na odporność betonów na wnikanie jonów chlorkowych.
EN
The properties of fly ash from co-combustion of coal and biomass have different properties in comparison with properties of typical fly ash. The results of research programme concerning concretes with fly ash from co-combustion of coal and wood biomass were presented in the paper. The effect of fly ash tested on cement concrete process of compressive strength increase, as well as the fly ash effect on resistance to chloride ion penetration were analysed.
EN
This paper presents research results on corrosion resistance of self compacting concretes made of cement containing blast furnace slag in water solutions with chlorides. On the basis of defined resistance coefficient OK. It has been proved that these concretes possess high resistance to environments containing chlorides and the corrosion resistance series has been established for solutions of MgCl2, NH4Cl and HCl.
PL
W niniejszym artykule przeanalizowano doniesienia literaturowe dotyczące błokomponentów paliw ciekłych ze szczególnym uwzględnieniem eterów tert-butylowych. Przedstawione zostały ich właściwości użytkowe i korzyści wynikające z zastosowania tego typu związków jako dodatków-tlenowych do benzyn silnikowych. Wprowadzenie eterów do praktyki znalazło swoje reperkusje w zanieczyszczeniu środowiska. Omówiono wzrastające zanieczyszczenie wód, jak i powietrza, eterami. W celu wyjaśnienia obecności eterów tert-butylowych w środowisku scharakteryzowane zostały ich źródła przenikania. Zaprezentowano wyniki badań udziału eterów (ert-butylowo-metylowego (MTBE), tert-butylowo-etylowego (ETBE) i tert-amylowo-metylowego (TAME) w reakcjach z rodnikiem hydroksylowym. W niniejszej pracy omówiono procesy biodegracacji eterów terf-butylowych. Wykazano wpływu jonu chlorkowego i czynnika utleniającego na przemiany ETBE i MTBE obecne w środowisku wodnym. Przedstawiono schemat przemian eterów tert-butylowych w układzie Cl: H2O2, w wyniku których powstają toksyczne produkty chloroorganiczne.
EN
The scientific publications concerning biocomponents added to the liquid fuels have been analyzed making a particular allowance for tert-butyl ethers. Their functional properties as well as the advantages resulting from the application of these compounds as the oxygen additives to the motor petrol have been characterized. Introduction of ethers into practice found its repercussions in the environment pollution. An increasing pollution both of waters and air with ethers have been discussed. In order to explain presence of tert-butyl ethers in environment, the sources of their penetration have been characterized. The results of studies on the effect of presence of tert-butyl-methyl ether (MTBE), tert-butyl-ethyl ether (ETBE) and tert-amyl-methyl ether (TAME) in reaction with hydroxyl radical have been presented. In this paper, processes of biodegradation of tert-butyl ethers have been talked over. The effect of chloride ion and oxidizing agent on ETBE and MTBE conversions in water medium has been demonstrated. The scheme of conversions of tert-butyl ethers in the system Cl :H2O2, resulting in formation of toxic chloroorganic products has been presented.
PL
Jony chlorkowe, są czynnikiem agresywnym, wywołującym korozję stali zbrojeniowej i korozję betonu. W pracy przedstawiono wyniki badań nad wpływem dodatku bitumicznego na odporność betonu cementowego na penetrację jonów chlorkowych. Do oceny odporności betonów zastosowano pomiary zmian rezystywności elektrycznej materiału. Wpływ zawartości dodatku bitumicznego, stężenia NaCl w cieczy, w której nawilżano próbki, czasu oddziaływania środowiska, jak również rodzaju cementu na zmiany rezystywności materiału analizowano przy zastosowaniu metod statystycznych: analizy wariancji i regresji. Wyniki analizy statystycznej wskazują na bardzo korzystny wpływ dodatku bitumicznego na odporność betonu na wnikanie roztworów soli chlorkowych.
EN
The chloride-induced corrosion of reinforcing steel is the major reason for the premature deterioration and degradation of field concrete structures built in salt-laden environment. The results of investigation of the effect of bituminous addition on Portland cement concrete resistance to chloride ions penetration are presented in this paper. Chloride penetration was simulated by subjecting samples to cyclic loading with salt solution and drying. Concrete resistivity development was monitored during 12 months. The test results have been analysed using the analysis of variance and regression to verify the effect of addition content, the time of exposure in aggressive environment, as well as the sort of cement on chloride ion permeability of Portland cement concrete. The statistical analysis showed that bituminous addition significantly improves the concrete resistance to chloride salt solution penetration.
CS
Příspěvek se zabývá vlivem trhlin na pronikání chloridových iontů do železobetonové mostovky ve které je betonářská výztuž chráněna povlakem na bázi epoxidové pryskyřice. Stochastické chování úlohy je podchyceno s využitím kombinace konečněprvkového modelu a pravděpodobnostní metody Simulation-Based Reliability Assessment (SBRA) [2]. Data užitá pro modelování difuzního koeficientu a krytí výztuže jsou založena na práci studii vykonané na mostech na severovýchodu USA (viz. [1])
PL
Przedstawiono analityczny opis procesu wnikania jonów chlorkowych do betonu z zastosowaniem równania Nernsta-Plancka. Na podstawie badań przeprowadzonych pod wpływem działania pola elektrycznego podjęto próbę oszacowania wartości współczynnika dyfuzji jonów chlorkowych wnikających do betonu.
EN
An analytic description of the process of chloride ions penetration inside concrete is presented with the use of Nernst-Planck equation. The diffusion coefficient of chloride ions inside concrete was estimated according to experiments where electric field was employed.
PL
Roztwór siarczanu cynku stosowany do elektrolitycznego otrzymywania cynku zawiera między innymi, jako zanieczyszczenia, jony chlorkowe. Szkodliwe ich działanie ujawnia się w procesie elektrolizy i przejawia się zwiększoną korozją anod, katod i chłodnic aluminiowych. Eliminacja jonów chlorkowych z roztworu elektrolitu może być zrealizowana poprzez związanie ich w postaci trudnorozpuszczalnego chlorku miedzi(I). Wyniki badań wskazują, że przeprowadzenie skutecznego odchlorowania roztworu siarczanu cynku jest możliwe przy zachowaniu odpowiednego stosunku stężeń jonów Cu2+/Cl-, Zn0/Cu2+ w roztworze, a także utrzymaniu temperatury w przedziale 323-333 K.
EN
Zinc sulphate solution used in electro-winning of zinc contains chloride ions as one of contaminants. Their harmful effect reveals during electrolysis process through increased corrosion of anodes, cathodes and aluminium coolers. The chloride ions can be eliminated from electrolytic solution by binding them into sparingly soluble cuprous chloride(I). The tests have shown that an effective dechlorination of a zinc sulphate solution is possible when suitable ratio of the concentrations of Cu 2+/Cl- and Zn0/Cu2+ ions in a solution is maintained and the temperature is kept within a range of 323-333 K.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.