The article presents various forms of deterioration in sandstone panels of the Collegium Iuridicum building in Poznań. The facade of this building is exposed to various urban and rural pollutants, which have a very significant influence on the weathering of the stone. The climatic conditions in which the test building is located and structure of the stone are also an important factors of the weathering. They can significantly accelerate the stone destruction processes. Based on the ICOMOS guidelines, deterioration forms were described and classified in macro and micro scales. For this purpose, optical, cathodoluminescence and scanning microscopy with EDS analyser were used. As a result of the research, secondary mineralization and the presence of numerous elements in the black crusts were identified. They are directly related to polluted air and the combustion of solid fuels. The identified elements include: Na, Mg, Al, Ca, P, K, S, Hg, Pb, Fe, Ti, Sc, Ni, Br, Mo, Zn, Mn, gypsum, calcite, fly ash particle.
Celestite containing very low amounts of barium occurs in weathering reaction zones developed on the Pińczów limestone exposed to the polluted atmosphere of Cracow. The mineral occurs both in limestone pore spaces filled with gypsum and in black gypsum crust. The Pińczów limestone contains ca 500 ppm strontium which was released during the reaction with atmospheric pollutants. The nucleation and growth of celestite, requiring significant concentration of components in evaporating solutions, is associated with gypsum crystallization.
PL
Celestyn z niewielką zawartością baru występuje w strefach reakcji rozwiniętych na wapieniu pińczowskim wystawionym na działanie zanieczyszczonej atmosfery w Krakowie. Minerał ten występuje zarówno w porach wypełnionych gipsem, jak i w czarnych naskorupieniach gipsowych. Wapień pińczowski zawiera około 500 ppm strontu, który jest uwalniany podczas reakcji z zanieczyszczeniami atmosfery. Zarodkowanie i wzrost celestynu wymagające znacznej koncentracji składników podczas parowania roztworów są związane z krystalizacją gipsu.
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.