Bis-l,3-oxothiolane-2-thione resins (Scheme 1) were prepared in the reactions of commercial low-M epoxy resins, Epidian 5 and Epidian 6, with carbon disulfide. Compositions including Epidian 5 or 6 and various amounts (5, 10, 20, 30 or 40 wt. %) of oxothiolane resins as additives were prepared and cured with piperidine. Mechanical properties such as bending, compressive, tensile and impact strengths were determined. Water absorbency, combustibility and thermal stability were also determined. Addition of 5 to 10 wt. % of sulfur-containing resin was found to improve mechanical strength by 15% (Fig. 1) and thermal stability by 35"C (Table 3, Fig. 3).
PL
Malocząsteczkowe handlowe żywice epoksydowe "Epidian 5" i "Epidian 6" poddano reakcji z CS2, otrzymując żywice bis-l,3-oksotiolano-2-tionowe (Schemat 1). Produkty te zastosowano jak dodatki (5; 10; 20; 30; lub 40% mas.) do kompozycji na podstawie wyjściowych żywic epoksydowych; uzyskane kompozycje usieciowano piperydyną. Określono właściwości mechaniczne (wytrzymałość na zginanie i ściskanie, naprężenie zrywające, udarność), wodochłonność, palność oraz odporność termiczną otrzymanych materiałów. Dodatek 5-10% mas. żywic oksotiolanowych polepszał właściwości mechaniczne o 15% (rys. 1) i odporność termiczną o 35°C (tab. 3, rys. 3).
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.