Content available remote Influence of cooling rate on y' morphology in cast Ni - base superalloy
EN
The Ni - base superalloys, which are combined an unique physical and mechanical properties, are used in aircraft industry for production of aero engine most stressed parts, as are turbine blades. From this reason a dendrite arm spacing, carbides size and distribution, morphology, number and value of [...] - phase are very important structural characteristics for blade life time prediction as well as aero engine its self. In this article are used methods of quantitative metallography (software LUCIA for carbides evaluation, measuring of secondary dendrite arm spacing and coherent testing grid for [...] - phase evaluation) for evaluation of structural characteristics mentioned above on experimental material - Ni base superalloy ŽS6K. The high temperature effect represented here by heat treatment at 800oC followed with holding time about 10 hours, and cooling rate, here represented by three various cooling mediums as water, air, and oil, on structural characteristics and application of quantitative methods evaluation are presented in this paper.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.