EN
The aim of these research is to investigate the air content on aging of poly-(ethylene terephthalate) (PET) preforms. Three air pressures were selected and in each pressure 5 samples were aged during 21 days in 80°C. Three samples were selected to be cut for determination of density with the use of hydrostatic method. Sample mass, Young modulus and surface roughness were measured for each sample before and after aging and differences between those parameters were presented as results. The changes of parameters may lead to a conclusion that mechanism of polymeric chain oxidation is dominant during thermal aging of PET. However aging process is not the fastest in atmospheric pressure but in lower air contents. This effect may be caused by greater evaporation of small molecule degradation products and shifting of reaction equilibrium in the direction of further decomposition.
2
Content available remote „Zielony” beton mostowy
PL
W artykule zaprezentowano wyniki prac nad „zielonymi” betonami mostowymi w aspekcie możliwości redukcji ich śladu węglowego pochodzącego od/z cementu. Cementy z dodatkami mineralnymi są doskonałym przykładem świadomego „zielonego” rozwoju technologii betonu w kierunku zmniejszenia emisyjności procesu wykonywania konstrukcji betonowych. Niestety tego typu cementy w budownictwie mostowym i drogowym wciąż pozostają zakładnikami archaicznych przyzwyczajeń i opinii, stając się spoiwami drugiego wyboru w porównaniu z cementami portlandzkimi „czystymi”. W artykule przedstawiono różne podejścia do rozwiązań materiałowych z betonu w przypadku typowej konstrukcji mostowej, biorąc pod uwagę właściwości betonu jako warunek konieczny do akceptacji rozwiązania oraz obliczając potencjał zmniejszenia śladu węglowego typowych rozwiązań materiałowych.
EN
In this article presented research results about „green” bridge concretes in aspect of possibilities of CO2 reduction. Composite cements with mineral additives are perfect example of „green” development of concrete technology towards decreasing emissions of construction process. Unfortunately composite cements in bridge and road construction in Poland still remain prisoner archaic habits and bad opinions and still remain as a cements second choice. I this article presented different approaches to materials solution for concrete used in typical bridge construction. Necessary condition for this type of solution were good properties of new „green” bridge concrete and scientifically potential decrease of carbon footprint.
PL
Artykuł przedstawia wyniki badań laboratoryjnych, podjętych w celu określenia wpływu rodzaju i ilości superplastyfikatorów (SP), domieszek przeciwpieniących (AFA) oraz stabilizujących (VMA) na zawartość powietrza i konsystencję oraz wytrzymałość na ściskanie i zginanie samozagęszczalnej zaprawy cementowej. Wyniki badań dowiodły, że zarówno rodzaj, jak i ilość AFA i VMA wpływa na właściwości świeżych i stwardniałych samozagęszalnych zapraw.
EN
The article presents the results of laboratory tests undertaken to determine the effect of the type and amount of superplasticizers (SP), anti-foaming (AFA) and stabilizing (VMA) admixtures on the air content and consistency as well as compressive and bending strength of the self-compacting cement mortar. The research results proved that both the type and amount of AFA and VMA affect the properties of fresh and hardened self-compacting mortars.
PL
W artykule przedstawiono wyniki badań wpływu obniżonej i podwyższonej temperatury na napowietrzenie i konsystencję nienapowietrzonych i napowietrzonych oraz upłynnionych zapraw wg PN-EN 480-1, które były wykonane z udziałem cementu CEM I. Do zwiększenia konsystencji zaprawy z CEM I zastosowano różne rodzaje plastyfikatorów i superplastyfikatorów oraz domieszki napowietrzające różniące się bazą chemiczną. Analiza rezultatów badań wskazuje, że charakter wpływu temperatury na konsystencję zaprawy zależy od efektu współdziałania danego rodzaju domieszki napowietrzającej i upłynniającej.
EN
The paper presents the results of research on the impact of low and high temperature on air content and consistency of nonair-entrained and air-entrained and plasticized mortars according to PN-EN 480-1, which were made with CEM I cement. In the case of mortar with CEM I, various types of plasticizers and superplasticizers as well as aeration admixtures differing in chemical base were used. Analysis of the results of the research indicates that the effect of temperature influence on the consistency of the mortar depends on the result of the interaction between the air-entraining and superplasticizing admixture.
PL
Stwierdzono konieczność stosowania zaleceń normowych dotyczących poboru i badania mieszanki betonowej. Intencją autorów jest zwrócenie szczególnej uwagi na zapisy norm regulujących podstawowe reguły prowadzenia kontroli i wykonywania badań, których nieprzestrzeganie lub zbyt dowolne traktowanie może wpływać w istotny sposób na ocenę jakości dostawy mieszanki betonowej na budowie.
EN
This article is intended to emphasize the legitimacy of using the standard recommendations for the collecting and testing of concrete mix. The intention of the authors was to pay particular attention to the provisions of standards regulating the basic principles of quality control and performing tests, the non-observance of which, or too arbitrary treatment, has significantly influence of the quality of concrete mix delivery at the construction site.
PL
Trwałość kompozytu cementowego jest najważniejszym kryterium oceny tego materiału. Natomiast ze względu na trwałość kompozytu cementowego istotną właściwością jest jego mrozoodporność. W celu zapewnienia mrozoodporności betonu norma europejska PN-EN 206-1:2013 [1] wymaga jego napowietrzenia na poziomie 4-7%. Również Komitet 201 Amerykańskiego Instytutu Betonu (ACI) wymaga stosowania domieszki napowietrzającej w betonach narażonych na destrukcję mrozową. Na ilość stosowanej domieszki napowietrzającej znaczący wpływ ma skład stosowanego cementu. Aby zminimalizować problemy z uzyskaniem betonu mrozoodpornego, podjęto próbę stworzenia cementów napowietrzających beton.
EN
The durability of a cement composite is the most important criterion of assessing this material, while frost resistance is significant as far as its stability is concerned. In order to ensure the frost resistance of concrete, the European standard BS EN 206-1: 2013 [1] requires its 4-7% air content. The Committee 201 of the American Concrete Institute (ACI) also requires the application of air-entraining admixtures in concrete exposed to frost destruction. The composition of the applied cement has a significant impact on the amount of the required air-entraining admixture. In order to minimize problems with obtaining frost-resistant concrete, we have attempted to manufacture air-entraining cement.
EN
In order to explain the effect of air entraining admixture (AEA) and the type of cement on the properties of fresh mortar, the following tests were carried: bulk density, flaw and air content of 20 air entrained mortars and 20 nan air entrained mortars made of ordinary Portland cement (OPC) and blended Portland cements: blast furnace slag (BSF) - limestone powder (LP), fly ash - limestone, fly ash (FA) and (BFS) cement. It has been found that the modern anionic AEAs from the group of alkyl sulfates are much more efficient and active than traditional ones i.e. sodium abietate. It is difficult to entrain air into mortars with cement of various types to the same content of air. This requires to carry out a number of tests to determine the appropriate amounts of AEA. The air entrainment of LP cement mortar does not significantly change its flow. The air entrainment of BSF and FA cement mortars increases their workability. The lowest content of air was stated in non-air-entrained mortars with FA cement, the highest air content was observed in BFS cement mortars. According to the results the bulk density of mortars is inversely proportional to the amount of air entrained.
8
Content available remote Admixtures effectiveness in mortars in the presence of calcareous fly ash
EN
This paper presents a study on the influence of various admixtures (SP, PL, AE , R, ACC ) on rheological properties, air content, setting time and heat of hydration of mortars with the addition of calcareous fly ash. Rheological parameters of mortars were determined using a rheometer Viskomat NT. The content of air in the mortar was determined using pressure method according to PN-EN 413-2 and initial setting time was specified according to PN-EN 196-3. The study on the heat of hydration was based on an isothermal microcalorimeter TamAir. The calcareous fly ash presence usually exerts negative influence on additives effectiveness. Activating the ash by grinding improves the additives efficiency (e.g. plasticizers, superplasticizers). The influence of calcareous fly ash on effectiveness of the additives is dependent not only on its type, but also on the type of admixture. The choice of compatible admixture should be made experimentally, taking into account the presence of calcareous fly ash.
PL
W artykule przedstawiono badania dotyczące wpływu różnych domieszek (SP, PL, AE, R, ACC) na właściwości reologiczne, zawartość powietrza, czas wiązania oraz ciepło hydratacji zapraw z dodatkiem popiołu lotnego wapiennego. Parametry reologiczne zapraw wyznaczono za pomocą reometru Viskomat NT. Ilość powietrza w zaprawie określano metodą ciśnieniową według PN-EN 413-2, a czas początku wiązania określono według PN-EN 196-3. Do badania ciepła hydratacji wykorzystano mikrokalorymetr izotermiczny TamAir. Obecność popiołu lotnego wapiennego zwykle wpływa negatywnie na efektywność działania domieszek. Uzdatnienie popiołu przez przemiał poprawia w niektórych przypadkach efektywność działania domieszek (np. plastyfikatorów, superplastyfikatorów). Wpływ popiołu lotnego wapiennego na efektywność działania domieszek zależy nie tylko od jego rodzaju, ale przede wszystkim od rodzaju domieszki. Dobór kompatybilnej domieszki należy dokonywać doświadczalnie, uwzględniając obecność popiołu lotnego wapiennego.
9
Content available remote Współczesne domieszki napowietrzające do betonu
PL
Destrukcja mrozowa to jeden z najpoważniejszych czynników, ograniczających trwałość betonu w klimacie, w którym jest on poddawany powtarzającym się cyklom zamrażania i rozmrażania. Skutecznym sposobem nadania betonowi mrozoodporności jest stosowanie domieszek napowietrzających. Powodują one zmianę struktury materiału, polegającą na stabilizowaniu w stwardniałym betonie mikropęcherzyków o takim rozkładzie przestrzennym i rozmiarach, że zabezpieczają one beton przed naprężeniami powstającymi na skutek zwiększania objętości przez zamarzającą wodę. Domieszki napowietrzające są nieodzowne wszędzie tam, gdzie beton jest narażony na czynniki atmosferyczne, zwłaszcza w budownictwie komunikacyjnym, ale także w innych obszarach technologii betonu.
EN
Frost action is one of the most significant factors, limiting the durability of concrete in the climate, in which it undergoes to repeating cycles of freezing and thawing. The effective measure for making concrete frost-resistant is use of air-entraining admixtures. They cause the change in the material structure, consisting in the stabilization of the air micro-bubbles in the hardened concrete. Themicro-bubbles have such spatial distribution and sizes that protect concrete against the excessive stresses created by the water, which expands when freezing. The air entraining admixtures are necessary, when the concrete is exposed to the atmospheric factors, particularly in the communication construction but also in the other fields of concrete technology.
PL
Przedstawiono zasady kontroli zgodności (obowiązkowej dla producenta) wymagane według normy PN-EN 206-1. Zamieszczono przykłady tej kontroli dotyczące zawartości powietrza w napowietrzonej mieszance betonowej oraz kontroli zgodności konsystencji.
EN
The rules of concrete control required by PN-EN 206-1 for conformity control (which is obligatory for concrete producers) are presented. The paper includes examples of this control for air content of air-entrained fresh concrete and control for consistency.
PL
Zbadano wpływ czterech domieszek stabilizujących lepkość (DSL) na zawartość powietrza i konsystencję oraz wytrzymałość na ściskanie i zginanie samozagęszczalnej zaprawy i betonu. Stwierdzono, że zarówno rodzaj, jak i ilość dodatku DSL wpływa na właściwości samozagęszalnych zapraw. Dodatek DSL w formie kopolimeru zwiększa wytrzymałość zapraw natomiast metyloceluloza w mniejszym stopniu. W przypadku betonu dodatek DSL w formie kopolimeru zmniejsza wytrzymałość, przy czym zmiana ta jest minimalna. Równocześnie następuje znaczny wzrost wytrzymałości napowietrzonego BSZ w wyniku dodatku DSL.
EN
The influence of four viscosity modifying agents VMA on air entrainment and consistency as well as the compressive and flexural strength of self-compacting mortars and concretes were examined. It was established that kind and content of VMA effects the properties of self-compacting mortars. The addition of VMA as copolymer increases the strength of mortars, but methyl cellulose type agent in much lower degree. In the case of copolymer VMA decreases strength, however, this change is very small. Simultaneously a significant increase of aerated SCC strength occurs with VMA addition.
PL
W referacie przedstawiono analizę istotności wpływu podstawowych czynników składu na zawartość powietrza w mieszance betonowej dla BSZWW oraz opracowano matematyczny model, ujmujący wpływ właściwości reologicznych na zawartość powietrza w mieszance betonowej dla BSZWW. Pomiar parametrów reologicznych wykonano za pomocą testu rozpływu. Zawartość uwięzionego powietrza w mieszance mierzono metodą ciśnieniową.
EN
The significance analysis of the fundamental composition factors on the air entrained in fresh concrete for HPSCC as well as a mathematical model influences the rheological properties of fresh concrete on the air entrained in fresh concrete for HPSCC are presented and discussed in the paper. Rheological parameters are measured using technical test (slump-flow test). Air entrained in fresh concrete is measured by concrete air entrainment tests.
PL
Istotą samozagęszczalnej mieszanki betonowej (SCC) jest samoczynne wyprowadzenie pęcherzyków powietrza z jej objętości. W przypadku, gdy superplastyfikator (SP) wykazuje działanie napowietrzające, mieszanka betonowa, pomimo że spełnia kryterium rozpływu jest nadmiernie napowietrzona. Powstaje pytanie względem przyjętych kryteriów powszechnie stosowanych w takiej sytuacji testów. W artykule analizowana jest metodyka postępowania w przypadku, gdy występuje problem nadmiernego napowietrzania SCC przez SP.
EN
The essence of a self-compacting concrete (SCC) mixture is the spontaneous elimination of air bubbles from its volume. In a case where a superplasticizer (SP) has an aerating effect, the concrete mixture is excessively aerated even though it satisfies the dispersion criterion. A question arises concerning the criteria adopted for the generally applied tests in such a situation. This paper analyses methods of proceeding in cases involving the problem of excessive aeration of SCCs by SPs.
PL
Jednym z ubocznych efektów działania niektórych superplastyfikatorów karboksylanowych jest znaczne zwiększenie zawartości powietrza w samozagęszczalnej mieszance betonowej. Stwierdzono, że przyczyną zwiększenia napowietrzenia jest obniżenie napięcia powierzchniowego ciekłej fazy w zaczynie w wyniku działania superplastyfikatora. Omówiono zagadnienie wpływu napowietrzenia związanego z działaniem superplastyfikatora, na właściwości mieszanki i stwardniałego betonu, o różnym składzie. Wyniki przeprowadzonych badań wykazują, że napowietrzenie SCC może zmniejszyć zdolność do płynięcia samozagęszczalnej mieszanki betonowej. Skład betonu wpływa w dużym stopniu na charakterystykę jego porowatości. Badania mikrostruktury wykazały, że pory powietrzne, zależnie od stopnia płynności mieszanki, mogą być regularne, swoim kształtem i wymiarami przypominając pory powstałe w wyniku działania domieszki napowietrzającej.
EN
One of the side-effects of functioning of some superplasticizers is forming much larger than 2% air content in self-compacting concrete mix. It was found out that the cause of air-entrainment effect with the usage of superplasticizers is the decrease of surface tension value of liquid phase in paste. The problem of the air-entrainment was discussed, formed as a result of superplasticizer's functioning on the characteristics both of the concrete and mixture, depending on the content. The research results show that SCC air-entrainment, depending on its content, may reduce the aptitude of concrete's self-compacting mixture flowing. The concrete's content influence fundamentally the porosity characteristic. The structure's tests show that air pores, depending on the level of mix flowing, can be regular and similar in shape and size to pores formed as the result of air-entrainment admixture functioning.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.