In this study, the newly designed Al-9Si/SiC particles (SiCp) + Ti-fiber (2step-reinforced Al-9Si alloy matrix) metal matrix composites (MMCs) were fabricated by hot-pressing sintering at 560°C. 2step-reinforced Al-based MMCs were characterized by thermal shrinkage, phase transition, microstructure and tensile strength. The addition of Ti-fiber reduced thermal shrinkage was caused by temperature difference in sintering process as well as enhanced assistance for tensile strength and plastic deformation at room temperature. Experimental results reveal that the 2step-reinforcment sintering by ceramic and metal has a significant effect to increase interface bonding in boundary of each component material and the improved mechanical properties were due to the influence of interfacial product by diffusion. Tensile strength and elongation at room temperature by 2step-reinforcement were improved in 19.5% and 26.2% more than those of Al-9Si/SiCp, respectively. Especially, it reveals that diffusion direction may be varied by sintering methods at low temperature in this study.
EN
The newly designed Ti-based bulk metallic glass (BMG) in which case of fracture behavior was observed 1990MPa to compressive strength with a wide plastic deformation around 7% after process of elastic deformation. This phenomenon can be compared with those of Ti-based alloys and other Ti-based BMGs and indicates high potential to be applied in use. It was evaluated the Ti-based BMG for thermal stability that the reduced glass parameters, ΔTx, Trg and γ, are 79K, 0.50 and 0.38, respectively. In addition, it reveals high activation energies for crystallization in which are estimated to Ex1 = 291.77 ±9.71 kJ/mol, Ex2 = 588.77 ±28.88 kJ/mol and Ex3 = 330.26 ±3.61 kJ/mol on kissinger plotting in this study.