Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników
Powiadomienia systemowe
  • Sesja wygasła!
  • Sesja wygasła!

Znaleziono wyników: 6

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  Thiobacillus ferrooxidans
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
The application of biotechnological methods in the metallurgical industry has the potential to provide an environmentally friendly and cost-effective direction of development. Thiobacillus ferrooxidans, a thionic bacterium, and the microalga Chlamydomonas reinhardtii TN-72 CH were used as complex reagents for extracting gold from sulfide mineral raw materials. The sorption properties of modal and productive multicomponent gold-bearing solutions were studied. The sorption characteristics of the biosorbents were compared with those of sorbents currently used in gold production – the synthetic resin AM2B and GoldCarb activated carbon. The conducted research studying the sorption properties and survival ability of the microalga C. reinhardtii TN-72 CH will make it possible to develop an industrial technology for extracting metal in the hydrometallurgical cycle of gold production. The use of microorganisms in gold hydrometallurgy as an alternative to cyanide methods will reduce the load on the environment while reducing the cost of the technology. In the process of leaching gold-bearing raw materials by microorganisms, even submicroparticles of gold are released, which makes the processing of poor and refractory ores promising. Preliminary biooxidation increases the effectiveness of thiosulfates in terms of both time and gold recovery.
2
Content available Bacterial desulphurization of coal
EN
The aim of this paper is to evaluate the suitability of a coal samples from different mines from Poland and Czech Republic for bacterial leaching. Laboratory research used a pure bacterial culture of Thiobacillus ferrooxidans. Were tested the samples from this localities: Mine Marcel, Mine Jankowice, Mine Staszic (Poland) and Mine Darkov and Mine Dukla (Czech Republic). The results showed that bacterial leaching was effective, with one month leaching time, when total desulphurization is from 38% to 72% and desulphurization of pyritic sulphur is from 60% to 82%. The paper describes changes of coal macerates after bacterial leaching.
PL
Celem tego artykułu jest ocena próbek węgla z różnych kopalń Polski i Czech pod kątem ługowania bakteryjnego. W badaniach laboratoryjnych zastosowano czystą kulturę bakterii Thiobacillus ferrooxidans. Testowano próbki z następujących kopalń: "Marcel", "Jankowice", "Staszic" (Polska) oraz "Darkov" i "Dukla" (Czechy). Wyniki badań wykazały, że ługowanie bakteryjne było efektywne w czasie jednego miesiąca, kiedy to ogólne odsiarczanie wzrosło z 38% do 72%, a odsiarczanie siarki pirytowej z 60% do 82%. Artykuł opisuje zmiany węgla po ługowaniu bakteryjnym.
3
Content available remote Removal of heavy metals from excessive activated sludge
EN
This paper presents the laboratory scale anaerobic treatment results from an acidic autolysis of a waste activated sludge and from a desulfiirication process of this sludge, too. The sludge with high contents of the heavy metals used in the study was derived from the treatment plant at Cze_stochowa. The anaerobic first-stage treatment system includes an acid reactor or a fermentation reactor with the population of the sulfate reducing bacteria e.g. Desulfovibrio desulfuricans respectively. The second stage was carried out on the aerated reactor, which was used to heavy metals extraction during bioleaching of the sludge from the first stage with Thiobacillus ferrooxidans bacteria. The removal yield of the heavy metals are given after each stages of the sludge treatment. The organic sludge after second stage operation can be application within agriculture as its heavy metals content is very low. The liquid product on separation phosphates and the metal hydroxides as the carbon source can be used to enhance the nitrogen and phosphorus removal at the waste water treatment plants. These investigations are part of the recycling project called 1TP (integrated treatment plant) process depending on the integration of the desulfurication to waste water treatment with an activated sludge technology at a treatment plant.
PL
Procesu bioutleniania odpadów arsenowych przeprowadzono w biorotorze i w kolbach Erlenmayera z wykorzystaniem bakterii Thiobacillus ferrooxidans. Kinetykę procesu opisano za pomocą równania logistycznego.
EN
The kinetics of bacterial oxidation of arsenic bearing waste using Thiobacillus ferrooxidans cells was studied. The effects on the rate of biooxidation were determined for two solid fractions. The logistic equation was used to descried experimental data.
5
Content available remote Biooxidation of mining tailings from Zloty Stok.
EN
The biooxidation of gold-bearing arsenic concentrate from mining tailing was investigated. The strain of Thiobacillus ferrooxidans isolated from the Zloty Stok tailing heaps was used. The chemical and biooxidation processes were monitored by checking the ferrous, ferric and arsenic concentration in the leaching solution. Leaching experiments, were conducted using both coarse (-0.5 +0.125 mm) and fine (-0.045 mm) fractions. The samples were examined. by means of the specific surface area measurements and the X-ray diffraction analysis. The small differences were observed during the oxidation of coarse and fine fractions. The slow chemical dissolution of loellingite (AsFe2) a main arsenic-bearing mineral, was supported by X-ray diffraction anal. In the case of a fine fraction oxidation, the precipitation of ferric arsenate was responsible for the lower Fe and As readings. The production of new phase was also supported by the FTIR spectra. Obtained results suggest that the direct biooxidation mechanism was responsible for the arsenic-bearing concentrate biooxidation.
PL
Przeprowadzone wcześniej badania wykazują, że odpady górnicze zgromadzone na Hałdzie Jan koło Złotego Stoku stanowią potencjalny surowiec do otrzymania złota. Przedstawiona Praca zawiera wyniki badań nad procesem bioutleniania próbek mineralnych pobranych z hałdy Jan. W badaniach użyto homogenizowanych bakterii Thiobacillus ferrooxidations wcześniej wyselekcjonowanych z tego złoża. Próbom bioługowania poddano grubo i drobnoziarnistą frakcję surowca. Przebieg procesu bioutleniania analizowane przez kontrole zmian stężenia jonów Fe(II), Fe(III), As przez pH roztworu. Określono zmiany w powierzchni właściwej próbek mineralnych wywołane procesem bioutleniania. Zachowanie gruboziarnistej próbki mineralnej mało różni się od chemicznego i biologicznego utleniania materiału drobnoziarnistego. Badania rentgenowskie wskazują na łatwiejsze bioutleniania loellingitu w porównaniu z procesem chemicznym. Zmniejszenie stężenia jonów arsenu w roztworze w końcowym okresie chemicznego ługowania należy tłumaczyć wytrąceniem się arseninu żelaza. W przypadku zastosowania pożywki 9K do bioługowania stężenia arsenu w roztworze spadło do zera. Badania spektroskopowe potwierdzają powstanie arseninu żelaza w procesie bioutleniania drobnoziarnistej frakcji odpadów górniczych z hałdy Jan.
6
Content available remote Bacterial leaching of nickel and cobalt from pentlandite.
EN
The influence of Thiobacillus ferrooxidans bacteria on efficiency of nickel and cobalt leaching from natural pentlandite (Ni,Fe)9S8 have been examined. The effect of pulp density, particle size and initial ferrous ion concentration in leaching solution. on the leaching yield was also evaluated. It has been demonstrated that the presence of T.ferrooxidans bacteria in leaching system induced considerable increase in nickel and cobalt leaching from pentlandite. The decrease in efficiencies of nickel and cobalt bacterial leaching processes have been denoted in systems containing. high amounts of ferrous ions. Initial Fe2+ concnentarion of 4.5 g/dm3 seems to be the most favorable for pentlandite bioleaching. The 20% pulp density may be admitted to be optimum regarding both satisfactory yields of bioleaching process and high nickel and cobalt concentrations in leaching solutions. The obtained results showed that particle size of 90-125 m was optimum for nickel and cobalt bioleaching from pentlandite.
PL
Badano wpływ bakterii Thiobacillus ferrooxidans na efektywność ługowania niklu i kobaltu z naturalnego pentlandutu (Ni, Fe)9S8, zawierającego 5,21% Ni 51.10% FE i 0.25% Co. Oceniano także wpływ gęstości pulpy (1%, 5%, 20%), rozmiaru ziaren (36-63 mm, 90-125 mm, 200-250mm, 63-200um) i początkowego stężenia jonu żelazawego Fe(II) w roztworze ługujacym (4,5 g/dm3, 9,0g/dm3, 13.5 g/dm3) na wydajność ługowania. Wykazano, że obecność bakterii T. Ferrooxidans w układzie ługujacym powodowała istotne zwiększenie wyługowania niklu i kobaltu z pentlandytu. W układach zawierających wysokie stężenie jonów żelazawych (?9 g/dm3)odnotowano zmniejszenie efektywności procesów bakteryjnego ługowania niklu i kobaltu. Wydaje się, że najbardziej korzystne dlabioługowania pentlandytu jest początkowe stężenie Fe(II) wynoszące 4.5 g/dm3. Biorąc pod uwagę zarówno satysfakcjonujące wydajności procesów bioługowania, jak i wysokie stężenia niklu i kobaltu w roztworach ługujacych, można przyjąć 20%-ową gęstość pulpy jako otymalną. Wielkość ziaren pentlandytu, optymalna dla bioługowania nuklu i kobaltu z tego minerału, powinna mieścić się w zakresie 90-125mm.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.