Uniform and adherent Zn1-xMnxO films have been deposited by using spray pyrolysis technique on glass substrates. The optical properties and dispersion parameters of zinc oxide have been studied as a function of doping concentration with Mn. Changes in direct optical energy band gap of cobalt oxide films were confirmed after doping, The optical energy gap Eg increased from 3.13 eV for the undoped ZnO to 3.39 eV with increasing the doping concentration of Mn to 4%. The changes in dispersion parameters and Urbach tails were investigated. An increase in the doping concentration causes a decrease in the average oscillator strength. The single-oscillator parameter has been reported.
EN
Thin films of CdO and 9 % Mg doped CdO doped have been prepared using spray pyrolysis technique. Transmission and absorption spectra were recorded in order to estimate these films. The deposited thin films were exposed to γ - rays. We have studied the transmission, absorptions and absorption coefficient as a function of photon energy before and after irradiation. The optical constants such as: reflectance, extinction coefficient, refractive index, real and imaginary parts of the dielectric constant and the electrical conductivity were calculated also.
EN
Thin films of ZnO0.7NiO0.3 have deposited on glass substrates at room temperature by using thermal evaporation technique under vacuum 10-5 mbar. The optical properties and dispersion parameters of the films have been studied. Changes in direct optical energy band gap of films were confirmed before and after annealing. The optical energy gap Eg decreased from 3.11 to 2.86 eV with increasing of annealing temperature to 200 ºC. Some of the optical absorption parameters, such as optical dispersion energies Eo and Ed, Urbach tails EU , dielectric constant ε, the average values of oscillator strength So, and wavelength of single oscillator λo have been reported. An increase in the annealing temperature causes an increase in the average oscillator strength from 62.02 to 87.71 eV.