Oxide dispersion-strengthened (ODS) superalloys are usually manufactured by a hot isostatic pressing after mechanical alloying (MA-HIP). However, this process cannot produce complex-shaped parts. Here, we used an additive manufacturing product (powders produced by laser powder bed fusion, L-PBF) to address this issue. Modified ODS Ni-based superalloy powders with a similar composition to the mechanical alloy 6000 (MA6000) were manufactured using a gas atomization process. The obtained powders and L-PBF synthesized samples were analyzed by scanning electron microscopy (SEM), X-ray diffraction (XRD), LPSA, and EBSD analyses.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.