The Nd-Fe-B type sinters were exposed to long-term (10 years) atmospheric corrosion which brought about their partial pulverization. The destruction process is markedly inhibited by partial (2 at.%) substitution of Si for Fe but it is strongly accelerated by Ti, Zr or Cu substitutions. A galvanic nature of the sinter damage is postulated. Due to contact with humidity the sinters absorb reversibly hydrogen and there is evident correlation between hydrogen uptake ability and pulverization susceptibility of the Nd-Fe-B based sinters.
PL
Długotrwała (10-letnia) ekspozycja atmosferyczna spiekanych materiałów na bazie Nd-Fe-B prowadzi do częściowej pulweryzacji spieków. Podstawienie żelaza niewielką (2% at.) ilością Si wyraźnie hamuje zaś podstawienie za pomocą Ti, Zr lub Cu – znacznie przyśpiesza degradację. Powstałe zniszczenia korozyjne sugerują ich galwaniczny charakter. W wyniku oddziaływania z wilgocią spieki na bazie Nd-Fe-B odwracalnie pochłaniają wodór, przy czym widoczna jest korelacja pomiędzy zdolnością do absorpcji wodoru a podatnością spieków na pulweryzację.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.