Internal friction and the shear modulus defect of disordered by quenching equi-atomic FePd alloy has been investigated during annealing up to 900 K using an inverted torsional pendulum. The internal friction decreases until the Curie point T(c)= 740 K, whereas the shear modulus defect increases, reaching at lower heating rate a subsidiary maximum at T(c) and a main maximum at the critical order-disoder transition point of 814 K. Heating rate dependent effects (eg. shift of the Curie point, changes in the internal friction level and magnetic susceptibility) were observed and are discussed in terms of thermally activated, migrational and structural relaxations leading to atomic order.
PL
Zbadano tarcie wewnętrzne oraz wskaźnik modułu sprężystości postaciowej stechiometrycznego stopu FePd w stanie nieuporządkowanym - uzyskanego w wyniku oziębiania, podczas wyżarzania do 900 K za pomocą odwróconej skręcarki wahadłowej. Tarcie wewnętrzne maleje aż do osiągnięcia punktu Curie (T(c) = 740 K), podczas gdy wskaźnik modułu sprężystości postaciowej wzrasta, osiągając przy najmniejszej prędkości wzrostu temperatury pierwsze maksimum przy temperaturze T(c) i główne maksimum w punkcie przemiany ze stanu nieuporządkowanego w uporządkowany w 814 K. Został zaobserwowany efekt prędkości nagrzewania na punkt Curie, zmiany w poziomie tarcia wewnętrznego oraz podatności magnetycznej. Omówiono termiczną aktywację, migrację oraz relaksację strukturalną prowadzącą do uporządkowania struktury.
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.