In this investigation three steels HCT 780T, AISI 347 and HSDr 600 with different content of metastable austenite and different austenite stability were monotonically loaded at ambient temperature. Using x-ray diffraction and scanning electron microscopy changes in the microstructure were characterized in detail. Hence, the most important mechanisms, which occur by deformation were determined.