EN
This paper presents laboratory analyses of the influence of an acidic environment, salinity and temperature change are able to exert on the geomechanical properties of the opoka-rocks. This rock material, deriving from four sites in East-Central Poland, was found to be variously resistant to factors like the destructive action of water-soluble salts and the effects of an acidic environment, on account of the actually-diverse nature of the rocks in question. Ultimately, the work offered a basis for a distinction to be drawn between the light opoka-rocks present at the Annopol and Kazimierz Wielki sites, and the heavy opoka-rocks from Bochotnica and Krasnobród, in terms of both textural and physical-mechanical features. The heavy opoka-rocks from Krasnobród proved least resistant to an acidic environment, which left strength reduced significantly. This kind of rock also experiences both an increase in porosity and absorbability and a decrease in weight. Furthermore, the influence of an acidic environment on aesthetic features of the examined rocks was in all cases negative, salts formed a patina on surfaces that obscured original structural and textural features. None of the tested types of rock presented resistance to the crystallization pressure such salt is able to exert.
PL
W ramach przeprowadzonych badań nad opokami pochodzącymi z miejscowości: Kazimierz Dolny, Annopol, Bochotnica i Krasnystaw stwierdzono, że należą one do grupy skał przejściowych pomiędzy węglanowami a krzemionkowymi. W efekcie badań stwierdzono opoki lekkie oraz ciężkie, różniące się gęstością objętościową. W miejscowościach Annopol i Kazimierz Dolny rozpoznano opoki lekkie, natomiast w Bochotnicy i Krasnobrodzie, opoki ciężkie. Przedmiotowe skały charakteryzują się dużym współczynnikiem zmienności w badaniach wytrzymałościowych, dlatego zaleca się wykonywanie badań opok na większej liczbie próbek. Wysoka porowatość opok wpływa na ich dobre właściwości termoizolacyjne, jednak cecha ta oddziałuje na wzrost nasiąkliwości badanych skał. W wyniku oddziaływania wody radykalnie spada ich wytrzymałość na ściskanie. W opokach lekkich zanotowano trzykrotny spadek tego parametru od wartości pierwotnej. Wszystkie typy skał, wykazały brak odporności na krystalizację soli. Wykazano, ze obecność kryształów soli w porach i pustkach skalnych powodowała wzrost wytrzymałości na ściskanie. W przypadku opoki lekkiej z Kazimierza Dolnego zaobserwowano wzrost wytrzymałości o 8.9%, a opoki ciężkiej z Krasnobrodu o 28,9%. Sól krystalizująca w warstwach przypowierzchniowych ma właściwości higroskopijne, co wpłynęło na zwiększenie nasiąkliwości powierzchniowej. Zaobserwowano, że w pewnych przypadkach, kiedy pory kamienia mają duże rozmiary lub gdy roztwór soli nie wypełnił ich w dostatecznym stopniu, krystalizacja soli nie powoduje wzrostu ciśnienia, w wyniku czego nie dochodzi do obniżenia wytrzymałości. Badania oddziaływania kwaśnych roztworów na opoki, wykazały wpływ na redukcję wytrzymałości. Największy spadek wytrzymałości na ściskanie wykazała ciężka opoka z Karsnobrodu. Wynikało to z największej zawartości węglanu wapnia wchodzącego w reakcję z kwasami. Ponadto, rozpuszczanie się składników skały w kwaśnym roztworze zwiększa jej porowatość, co skutkuje zwiększeniem nasiąkliwości. W wyniku reakcji węglanu wapnia z kwasem na powierzchni kamienia, tworzą się sole o właściwościach higroskopijnych, które mogą znacznie zwiększyć powierzchniową absorpcję wody. Na skutek zanurzania w kwasie i rozpuszczania się składników skały, zaobserwowano utratę ich masy. Największy spadek wynoszący 4,1% wykazała ciężka opoka z Krasnobrodu. Oddziaływanie kwaśnego środowiska powoduje pogorszenie ich walorów estetycznych. Sole krystalizujące na ich powierzchniach tworzą warstwę patyny, która zaciera pierwotne cechy strukturalno-teksturalne opok.
EN
The main issue of the article is the corrosion of the reinforced concrete elements by the co-influence of the aggressive and power factors. The problem of corrosion is extremely actual one. Therefore the tests were carried out upon the specimens considering the corrosion in the acid environment, namely 10 % H2SO4. The acid environment H2SO4 was taken as a model of the aggressive environment. Conclusions concerning the corrosion model of the cross section and investigation of stress-strain state have been made. That material concerns the problem of the reinforced concrete corrosion as a whole construction. Reinforced concrete beams were tested with and without the co-action of the aggressive environment and power factor.
PL
Celem pracy badawczej opisanej w niniejszej publikacji było zbadanie wpływu środowiska kwaśnego i zasadowego na degradację powierzchniową ceramiki cyrkonowej stabilizowanej itrem (Y-TZP). Miarą degradacji (starzenia) były zmiany ilości fazy jednoskośnej (m-ZrO2) w materiale i wartości wytrzymałości na zginanie. Próbki wykonane z trzech proszków Y-TZP oznaczonych jako: OLD, CH3 i HT poddano procesowi starzenia w roztworach: 5M H3PO4 (K1), 5M H2SO4 (K2), 5M NaOH (Z) i wodzie destylowanej (W) w temperaturze 90°C przez 72 godziny. Próbą odniesienia były próbki niestarzone (NS), a próbą kontrolną – próbki starzone w wodzie destylowanej (W). Aby ocenić wpływ poszczególnych czynników wykonano analizę fazową XRD, obserwacje powierzchni w mikroskopie skaningowym SEM oraz badania wytrzymałości na zginanie. We wszystkich próbkach starzonych zaobserwowano przyrost ilości fazy jednoskośnej w porównaniu do próbek niestarzonych. Wyniki badań wskazują, że największy przyrost zawartości m-ZrO2 występuje po starzeniu w 5M NaOH oraz że wytrzymałość na zginanie nie jest jednoznacznie skorelowana ani z rodzajem starzenia, ani z przyrostem fazy m-ZrO2 w próbkach.
EN
The aim of the research described in this publication was to investigate the influence of acidic and alkaline environments on the surface degradation of Yttrium-Stabilized Zirconia Ceramics (Y-TZP). The measure of degradation (aging) were changes in the amount of monoclinic zirconia phase (m-ZrO2) in the material and bending strength values. Tests samples were prepared from three Y-TZP powders marked as: OLD, CH3 and HT and were subjected to an aging process in the following solutions: 5M H3PO4 (K1), 5M H2SO4 (K2), 5M NaOH (Z) and distilled water (W) at 90°C during 72 hours. The reference samples were these not aged (NS) and as a control – samples aged in distilled water (W). To assess the impact of individual factors, the XRD phase analysis, surface observations in the SEM scanning microscope and bending strength tests were performed. In all aged samples an increase in the amount of monoclinic phase was observed as compared to not aged samples. The results indicate that the highest increase in m-ZrO2 phase occurs after aging in 5M NaOH and the bending strength is not unequivocally correlated neither with the type of aging nor with the increase in the monoclinic phase in the samples.
4
Content available remote Uszkodzenia zbiornikowej powłoki kwasoodpornej
PL
Przedstawiono przypadek uszkodzenia zbiornikowej powłoki chemoodpornej w środowisku mieszaniny kwasów w podwyższonej temperaturze. Stwierdzono, że główną przyczyną uszkodzeń były wady konstrukcyjne zbiornika, a nie wadliwe wymalowanie lub zły dobór powłok.
EN
Destruction of acid-proof coating on industrial tank in the acidic environment and increased temperature was presented. It was found that the main reason of destruction were neither failure painting nor the incorrect choice of coatings but design failures of the tank construction.
5
Content available remote Badania trwałości betonu cementowego w środowisku kwasowym
PL
Mimo że beton jest uważany za materiał mało kwasoodporny, istnieje potrzeba testowania i oceny trwałości betonu z różnymi spoiwami w agresywnym środowisku kwasów. W artykule przedstawiono ocenę odporności betonów z dwoma rodzajami cementu na działanie kwasu solnego. Ze względu na brak odpowiednich procedur normowych wszystkie testy zostały przeprowadzone zgodnie z własną procedurą ZIMBPW. Próbki wyeksponowano na działanie kwasu o różnym stężeniu i w różnym czasie ekspozycji. Jako kryteria oceny kwasoodporności przyjęto: zmianę masy, zmianę wytrzymałości na ściskanie i zginanie.
EN
Although concrete is hardly considered as the acid resistant material, it should be possible to test and evaluate the ability of concrete of various cements to resist the chemically aggressive environments. The paper presents assessment of the resistance of concretes with two types of cement to hydrochloric acid. Due to the lack of proper standard procedures all tests were performed according to the DBME own procedure: specimens were exposed to acids of various concentrations and for various exposure times. Concrete acid resistance evaluation criteria were: change ofmass, change of compressive and flexural strength.
PL
Przedstawiono wyniki badań termicznej dekompozycji fragmentów obwodu drukowanego z podzespołami elektronicznymi prowadzonej w reaktorze z pęcherzowym złożem fluidalnym, oraz ługowania produktów spalania w środowisku kwaśnym. Uzyskaną po spaleniu pozostałość poddano dwuetapowej ekstrakcji w środowisku kwaśnym (H₂SO₄ i woda królewska). Uzyskano stopnie ekstrakcji wynoszące od 99,95% (Cu) do 97,42% (Mn), dla ołowiu (2,60%), przy użyciu H₂SO₄, oraz od 99,94% (Cu) do 71,73% (Ti) przy użyciu H₂SO₄ i wody królewskiej. Warunkiem uzyskania wysokich stopni ekstrakcji przy użyciu kwasu siarkowego było zastosowanie w początkowym okresie tego procesu kwasu stężonego.
EN
Printed circuit boards with electronic components were combusted in a fluidized bed reactor in air-liq. petroleum gas stream. The combustion products were leached with concd. H₂SO₄ and HNO₃/H₂SO₄ at 50°C for 120 min. The metal recovering degree ranged from 99.95% (Cu) to 97.42% (Mn), with the exception of lead (2.60%), when H₂SO₄ was used, and from 99.94% (Cu) to 71.73% (Ti) when in a 2-stage process H₂SO₄ and HNO₃/H₂SO₄ were used.
EN
The article discusses studies and corrosion tests of binary Mg-Li alloys for plastic forming examined in an acid medium (5% HCl solution) for the time of 0-144 hours. In short it can be stated that corrosion of the examined Mg-Li alloys in 5% HCl solution proceeded in a similar mode in all the studied alloys, regardless of the lithium content.
EN
The paper outlines the course of corrosion processes in magnesium and Mg-Li alloys. The methodology of corrosion studies of alloys for plastic forming and their chemical composition as well as micrographs of alloys intended for research are presented.
PL
Zbadano efekty technologiczne procesu dwustopniowego rozjaśniania świerkowych mas termomechanicznych nadtlenkiem wodoru w środowisku kwaśnym i alkalicznym. Dokonano oceny wpływu pH i temperatury roztworu rozjaśniającego, ilości dozowanego nadtlenku oraz czasu obróbki na wskaźniki chemiczno-technologiczne rozjaśniania w środowisku kwaśnym. Porównano efektywność obróbki jednostopniowej w środowisku alkalicznym i dwustopniowej prowadzonej w obecności katalizatora miedziowego w środowisku kwaśnym oraz stabilizatorów siarczanu magnezu i krzemianu sodu w środowisku alkalicznym. Stwierdzono, iż dwustopniowa obróbka nadtlenkiem wodoru w środowisku kwaśnym i alkalicznym, umożliwia otrzymywanie świerkowych mas termomechanicznych o podwyższonej białości, z porównywalną wydajnością i przy mniejszym zużyciu nadtlenku wodoru w porównaniu do tradycyjnego jednostopniowego rozjaśniania w środowisku alkalicznym.
EN
The technological efficiency of two stage brightening of the spruce TMP with hydrogen peroxide under acidic and alkaline conditions has been studied. The influence of pH and temperature of the brightening solution, peroxide charge and time of treatment on chemical and technological indices of process under acidic conditions was evaluated. The effects of one stage alkaline hydrogen peroxide treatment in comparison with two stage sequence, initially under acidic conditions in the presence of copper catalyst, followed by alkaline conditions with addition of stabilizers magnesium sulphate and sodium silicate were examined. The results of this study show that two stage brightening of the spruce TMP with hydrogen peroxide under acidic and alkaline conditions has beneficial effect first of all on peroxide consumption than on brightness response and does not affect the yield when compared to standard one stage alkaline peroxide treatment.
11
Content available remote Korozihja betonu konstrukcihjj v seredovihshhih kislot
EN
The paper is devoted to the investigation of the concrete corrosion procedure with the effect of the hydrochloric and sulfuric acids. There is the aggressive acid environment in the most industrial buildings of the chemical industry and galvanic shops. Thus investigation of the corrosion procedures in such environments are very important. The article presents the experimental results of the mass loss, the flexural strength and the compressive strength of the concrete specimens, which depends on the effect of the aggressive environments and time. The paper contains as well the results of studying of qualitative concrete composition and microstructure of the concrete. The testing was performed upon the plain concrete and concrete with antirust coating, namely by silicorganical varnish. The efficiency of the antirust coating with the effect of the aggressive acid environment is also defined.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.