EN
To study the influence of temperature field and stress field on the cracking of the small thickness steel plate concrete composite shear wall (SPCW) in the early stage of construction. The temperature field and stress field of a 400 mm thickness SPCW was monitored and simulated through experimental research and numerical simulation. Moreover, a series of parameter analyses were carried out by using ANSYS to investigate the distribution of temperature field and stress field of SPCW. Based on the analysis results, some suggestions are put forward for controlling the cracking of SPCW in the early stage of construction. The results show that the temperature stress of 400 mm thickness SPCW in the early stage of construction is small, and there is no crack on the wall surface. For SPCW with thickness less than 800mm, the temperature stress caused by hydration heat in the early stage of construction is small, and the wall will not crack. The parameters such as wall thickness, steel plate thickness, boundary condition and stud space significantly influence the temperature field and stress field distribution of the small thickness SPCW in the early stage of construction, and reasonable maintenance measures can avoid cracking.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.