The pregnant solution after atmospheric leaching of cupriferous shale (middlings from Lubin Concentrator) with sulphuric acid and/or with sulphuric acid containing Fe(III) in the presence of oxygen were applied for solvent extraction experiments with several extractants. The solutions containing soluble sulphates of Cu(II), Zn(II), Ni(II), Co(II), Fe(II), Fe(IIII) and As as a contaminant. Aromatic hydroxyoximes, LIX 84, LIX 612 and LIX 984, were investigated as copper(II) extractants to evaluate their extraction and reextraction abilities. From the copper free raffinate Zn(II) was next extracted with di-(2-ethylhexyl)phosphoric acid (D2EHPA). Additionally, cobalt(II) and nickel(II) were separated from the zinc-free raffinate with di-(2,2,4–trimethylpentyl)phosphinic acid (Cyanex 272). Industrial aromatic hydroxyoxymes used for copper(II) extraction were not sufficient selective and other metal ion species present in leach solutions were also transferred to the organic phase. The extractive recovery of Cu(II), Co(II) and Ni(II) was better for the solutions obtained from acidic leaching of shale in the absence of Fe(III) salts. The recovery of valuable metals was not satisfactory and further experiments are necessary to establish the optimal conditions of extraction and reextraction processes.
PL
Roztwory kwasu siarkowego po ługowaniu atmosferycznym półproduktu łupkowego (odpad I czyszczenia I ciągu ZWR Lubin) w obecności tlenu i żelaza(III) zastosowano do ekstrakcji metali przy użyciu różnych ekstrahentów. Roztwory zawierały rozpuszczalne siarczany Cu(II), Zn(II), Ni(II), Co(II), Fe(II), Fe(IIII) i As jako składnika niepożądanego. Aromatyczne hydroksyoksymy: LIX 84, LIX 612 i LIX 984 były stosowane jako ekstrahenty Cu(II). Z roztworu rafinatu pozbawionego Cu(II) ekstrahowano Zn(II) za pomocą kwasu di-(2-etylohexylo)fosforowego (D2EHPA). Ponadto, kobalt(II) i nikiel(II) były wydzielane z wolnego od cynku rafinatu za pomocą kwasu di-(2,2,4–trimetylopentylo)fosfonowego (Cyanex 272). Przemysłowe hydroksyoksymy aromatyczne użyte do ekstrakcji miedzi okazały się mało selektywne i obserwowano przenoszenie jonów innych metali do fazy organicznej. Odzysk ekstrakcyjny Cu(II), Ni(II) i Co(II) okazał się znacznie lepszy dla roztworów po ługowaniu pozbawionych obecności Fe(III). Odzysk metali użytecznych okazał się niezadowalający i potrzebne są dalsze systematyczne badania nad optymalizacją procesów ekstrakcji i reekstrakcji.
2
Content available remote Atmospheric leaching of shale by-product from Lubin concentrator
EN
The results of non-oxidative leaching with sulphuric acid followed by atmospheric leaching with oxygenated H2SO4 have been presented for shale containing middlings (tailings from 1st cleaning flotation) from Lubin Concentrator. It was found that all leaching or bioleaching processes performed in acidic media has to be preceded by non-oxidative decomposition of acid-consuming carbonate components to liberate finely disseminated metal-bearing minerals. Atmospheric leaching appeared to be very efficient process for recovering Cu, Ni and Co from Lubin middlings due to favorable mineralogical composition and fine diameters of leached particles. Maximum recovery of Cu, Ni and Co after 5 hours leaching was observed for experiments at 90 C in the solutions containing 15 – 30 g/dm3 of Fe(III). Solid residue after atmospheric will be further processed by flotation or chloride leaching to recover Ag, Pb and precious metals.
PL
Przedstawiono wyniki badań nad ługowaniem nieutleniającym za pomocą kwasu siarkowego i ługowaniem atmosferycznym w natlenionym roztworze H2SO4 i w obecności jonów Fe(III) półproduktu flotacji (odpad I czyszczenia ZWR Lubin). Badany półprodukt stanowił materiał o wysokiej koncentracji frakcji łupkowej i został uznany za koncentrat tej frakcji. Wykazano, że procesy ługowania utleniającego lub bioługowania prowadzone w warunkach kwaśnych musza być bezwzględnie poprzedzone procesem niuetleniającego rozkładu składników węglanowych w celu uwolnienia bardzo drobno rozproszonych minerałów metalonośnych. Ługowanie atmosferyczne okazało się procesem bardzo efektywnym w odniesieniu do badanego półproduktu łupkowego. Proces zapewnia skuteczne odzyskanie do roztworu Cu, Ni, Co dzięki korzystnemu składowi mineralogicznemu frakcji łupkowej. Maksymalny stopień wyługowania metali, po 5 godzinnym procesie, obserwowano w doświadczeniach prowadzonych w temperaturze 90 C i obecności jonów Fe(III) o stężeniu w zakresie 15-30 g/dm3. Pozostałość stała po ługowaniu atmosferycznym będzie poddawana procesowi flotacji lub ługowaniu chlorkowemu dla odzyskania srebra, ołowiu i innych metali szlachetnych