Growth kinetics of boride layers in AISI H13 steel was investigated using the pack boriding method at temperatures of 1073, 1173 and 1273 K (800°C, 900°C and 1000°C) for periods of 2, 4 and 6 h with nano-sized boron (NB) and micron-sized Ekabor II powders as boriding agents. The total thickness of the boride layer (including both FeB and Fe2B) after boriding at 1273 K (1000°C) for 6 h was 103.8 μm and 96.5 μm for the NB and Ekabor II specimens, respectively. X-ray diffraction analysis of the boride layers on the surfaces borided with NB and Ekabor II revealed the presence of FeB and Fe2B phases with sawtooth morphology. The FeB/Fe2B volume ratio was higher in the specimens borided with NB. The thickness of the boride layer (FeB + Fe2B) increased with the increasing boriding temperature and time. The FeB layer in the NB specimen displayed a (002) preferred orientation.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.