In this work, oxidation properties of austenitic 316L stainless steel powder and sintered porous support were investigated at the temperature range of ~600-750 °C for 100 hours in ambient air. Oxidation kinetics was determined by continuous thermogravimetry and analyzed employing parabolic rate law. It was observed that oxidation leads to the formation of an oxide scale, with substantial oxidation occurring at ≥ 650 °C in the powder. The porous steel support was fabricated by tape casting method with two distinct pore former concentrations. The microstructural features of both the powder and support were investigated by X-ray diffractometry and scanning electron microscopy coupled with energy-dispersive X-ray analysis. The mechanical properties of the metal support were examined before and after oxidation via a microhardness test. The effect of porosity on the resulting properties of the metal support was also highlighted. In summary, 316L stainless steel support suits SOCs applications below 600 °C.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.