This research specifically focused on the development of a novel methodology to reduce excess nitrate in drinking water utilizing zerovalent iron nanoparticles (nZVI)-stabilized radiation-grafted copolymer matrix. nZVI was synthesized by borohydrate reduction of FeCl3 and stabilized on acrylic acid (AAc)-grafted non-woven polyethylene/polypropylene (NWPE/PP-g-AAc) copolymer matrix, which was grafted using gamma radiation. The use of nZVI for environmental applications is challenging because of the formation of an oxide layer rapidly in the presence of oxygen. Therefore, radiation-grafted NWPE/PP synthetic fabric was used as the functional carrier to anchor nZVI and enhance its spreading and stability. The chemical reduction of nitrate by nZVI-adsorbed NWPE/PP-g-AAc (nZVI-Ads-NWP) fabric was examined in batch experiments at different pH values. At low pH values, the protective layers on nZVI particles can be readily dissolved, exposing the pure iron particles for efficient chemical reduction of nitrate. After about 24 h, at pH 3, almost 96% of nitrate was degraded, suggesting that this reduction process is an acid-driven, surface-mediated process. The nZVI-water interface has been characterized by the 1-pK Basic Stern Model (BSM). An Eley-Rideal like mechanism well described the nitrate reduction kinetics. In accordance with green technology, the newly synthesized nZVI-Ads-NWP has great potential for improving nitrate reduction processes required for the drinking water industry.
EN
In 1965 Parks compiled PZC of metal oxides and hydroxides and his paper is still the most frequently cited source of PZC of these materials. The recent compilation (Kosmulski 2001) covers not only oxides and hydroxides, but also mixed oxides, sparingly soluble salts and other materials whose surface charging is pH dependent. One set of data from this compilation (155 PZC of AL2O3 published in 150 papers between 1969 and 2001) was selected to show the effect of crystalline structure on the one hand and of the choice of the experimental method on the other on the PZC. There is no significant difference between the ? form (32 entries, average 8.2, median 8.55) and the ? form (58 entries, average 8.2, median 8.4) and the other forms, mixtures of different forms and materials of unknown structure (65 entries, average 8.3, median 8.7). On the other hand, the choice of the method substantially affects the PZC. The isoelectric point IEP from electroacoustic measurements (11 entries, average 9.3, median 9.5) is significantly above the IEP from classical electrokinetic measurements (78 entries, average 8.2, median 8.7) and potentiometic titration at one ionic strength (29 entries, average and median 8). The results obtained by means of two latter methods are much more scattered than in other methods. The lowest standard deviation was observed in the set of PZC obtained by means of combination of titration (the common intersection point of titration curves for three or more ionic strengths is identified with the PZC) and electrokinetic measurements (7 entries, average and median 8.6), and this value is the "recommended" PZC for alumina.
PL
Parks opublikował w 1965 roku przegląd PZC tlenków I wodorotlenków metali, który do chwili obecnej jest najczęściej cytowanym źródłem informacji. Najnowszy przegląd PZC (Kosmulski 2001) obejmuje nie tylko tlenki i wodorotlenki metali, lecz również tlenki mieszane, trudno rozpuszczalne sole i inne materiały, których ładunek powierzchniowy zależy od pH. Na podstawie przykładowego zestawu danych z tego przeglądu (155 wartości PZC dla Al2O3 opublikowano w 150 pracach w latach 1969-2001) badano wpływ struktury krystalograficznej próbki i doboru metod doświadczalnych na otrzymaną wartość PZC. Stwierdzono brak istotnej różnicy pomiędzy odmianami. Alfa (32 wartości, średnia 8.2, mediana 8.55) i (58 wartości, średnia 8.2, mediana 8.4) oraz innymi odmianami, mieszaninami różnych odmian i materiałami o nieznanej strukturze (65 wartości, średnia 8.3, mediana 8.7). natomiast wartości PZC wyraźnie zależą od zastosowanej metody. Metoda elektroakustyczna (1l wartości, średnia 9.3, mediana 9.5) daje zdecydowanie wyższy punkt izoelektryczny IEP niż klasyczne metody elektrokinetyczne (78 wartości, średnia 8.2, mediana 8.7) i miareczkowanie potencjometryczne przy jednej sile jonowej (29 wartości, średnia i mediana 8). W dwóch ostatnich metodach odchylenie standardowe jest większe niż w pozostałych metodach. Najmniejsze odchylenie standardowe występuje w zbiorze danych otrzymanych przy jednoczesnym zastosowaniu miareczkowania potencjometrycznego (jako PZC przyjmuje się punkt przecięcia krzywych miareczkowania przy co najmniej trzech rożnych siłach jonowych) i pomiarów elektrokinetycznych (7 wartości, średnia i mediana 8.6) i tę wartość można uznać za najbardziej wiarygodną.