This study evaluated some properties of sesenduk (Endospermum malaccense) wood treated with propionic anhydride and exposed to outdoor conditions for up to one year. Defect-free samples of sesenduk were extracted with a 3:1:1 (v/v) mixture of toluene, ethanol and acetone for 3 hours at a temperature of 100°C. The samples were then modified at the same temperature for another 3 hours using propionic anhydride and 10% sodium formate as catalyst. Modulus of elasticity (MOE), modulus of rupture (MOR) and parallel-to-grain compression strength of the samples exposed to weathering were tested. Chemical treatment reduced the MOE but slightly increased the MOR and parallel-to-grain compression strength compared with untreated samples. However, treated samples retained higher strength properties than untreated ones. The modulus of elasticity, modulus of rupture and parallel-to-grain compression strength of treated samples at radial orientation were respectively 20%, 31% and 62% higher than those of untreated samples after one year’s outdoor exposure. Weathering adversely influenced the surface quality of the specimens for all exposure times.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.