Ceramic coatings are especially suitable for thermal loaded parts protection. These coatings are obtained by plasma spraying. Among most extended from them there are oxide-base coatings with or without addition of dopel material. Significant problem there is degradation of listed coatings as result of coating adhesion decreasing. This is caused mainly by different index of dilatability between coating and base material. This contribution deals with solving of these problems.