This paper presents the results of an examination of cast-on-strap joints of lead acid batteries with different discharge capacities. The galvanic joints of lugs of selected cells in lead acid batteries were analyzed. The study showed some defects that may occur in these joints. Examples of the defects that can affect battery lifespan were presented.