EN
High Sb and As contents in zink and lead concentrations, have always been obtained by conducting experiments with flotation concentration of complex poly-mineral Pb-Zn-Sb-As-(Ag, Au) ore ground to varied grinding finenesses. Chemical analyses were not sufficient to explain this phenomenon. With the help of detailed mineralogical analyses of the run-of-mine ore, and, the obtained concentrates that followed, the problem has been solved. All ore minerals were identified, the degree of liberation of galena and marmatite measured, and the frequency of occurrences of certain types of binary, ternary and higher locked grains determined. The measurements of the liberation degree of galena and marmatite (at the fineness of grinding of 83% -0.074 mm), in the obtained concentrates have shown that the increase in a grinding fineness can only partially result in the increase in recovery and provide better concentration results. In addition, the use of new selective low-cost flotation reagents is required to separate hard-to-beneficiate pairs of sulphide minerals with very similar flotation properties.
PL
Wysokie zawartości Sb i As w koncentratach cynku i ołowiu zawsze były uzyskiwane przy prowadzeniu flotacji złożonych polimetalicznych mieszanin Pb-Zn-Sb-As-(Ag, Au) o drobnym uziarnieniu. Analizy chemiczne okazały się niewystarczające do wyjaśnienia tego zjawiska. Za pomocą szczegółowych analiz mineralogicznych przeprowadzanych na rudzie oraz otrzymanych koncentratach problem ten został rozwiązany. Zidentyfikowano wszystkie minerały rudne, stopień uwolnienia galeny oraz marmatytu oraz częstość występowania określonych związków dwu i trójskładnikowych lub bardziej złożonych. Pomiary stopnia uwolnienia galeny oraz marmatytu (o zawartości ziaren -0,074 mm równej około 83%) w otrzymanych koncentratach wykazały, że wzrost ilości drobnych ziaren może być jedynie częściowym powodem wzrostu uzysku i lepszych wyników jakości koncentratu. Dodatkowo, zastosowanie nowych, tanich odczynników flotacyjnych jest warunkiem rozdziału trudnych do wzbogacenia minerałów siarczkowych o podobnych właściwościach flotacyjnych.
2
Content available Concentration of Gold From Small Deposits in Serbia
EN
Tests presented in this work are conducted on samples of the Pb-Zn-Fe-Au poor mineralization from the Grabova Reka deposit, Ist Serbia. The methods are described of selective separation of auriferous minerals and accessory sulphides from complex quartz veins, small gold deposits, in Blagojev Kamen area (Grabova Reka deposit) characterized by nonunion and relatively poor gold mineralization (Au, Au+Ag, electrum, Au+Fe, Au+Pb, Au+scheelite). Gold prevailing occurs in small grains (5÷10 rarely 100 μm) contained in quartz, pyrite or in galena of pinkish shade from alloying with Bi and Cu. Electrum, a natural alloy of Au and Ag varies in grain size, but generally, electrum is found in large grains (0.5 mm on average) in the form of conglomerate where electrum is cementing cataclastic grains of pyrite (or as inclusions in pyrite and in galena) and other Pb-Zn sulphides. There are many deposits, in the mentioned region, with numerous outcrops of quartz veins with the gold rates from 10 g/t to 60 g/t or even to 120 g/t on average, somewhat lower silver, and some lead and zinc (about 1%). The analysed sample was collected by chipping in places of visible sulphide mineralization from quartz vein No. 2 in plagiogranite. The purpose of this work was to accurately establish the modes of gold or auriferous mineral occurrence, for testing its selective separation. A flow-chart is given of the mineral recovery process and the mineral balance. A characterization is given of the mineralized grains in raw material which are essential for planning the technology of processing. One of the methods used, is the heavy liquid separation analysis at the density of 13.6 g/cm2 .
PL
Zaprezentowane testy w pracy zostały przeprowadzone na próbkach Pb-Zn-Fe-Au ze złoża Grabova Reka w Serbii. Metody separacji selektywnej złotonośnych minerałów oraz siarczków ze złożonych żył kwarcu zostały opisane. Małe złoża złota w rejonie Blagojev Kamen (złoże Grabova Reka) charakteryzują się relatywnie słabą i rozproszoną mineralizacją (Au, Au+Ag, elektrum, Au+Fe, Au+Pb, Au+szelit). Złoto występuje w małych ziarnach (5-10, rzadko 100 μm) zawartych w kwarcu, pirycie lub galenie o różowawym zabarwieniu ze stopów z Bi oraz Cu. Elektrum, naturalny stop Au i Ag jest zróżnicowane pod względem uziarnienia, ale zazwyczaj spotyka się je w dużych ziarnach (średnio 0.5 mm) w formie konglomeratu, gdzie elektrum zespala kataklastyczne ziarna pirytu (lub występuje jako wtrącenie w pirycie oraz w galenie) lub innych siarczków Pb-Zn. W omawianym regionie znajduje się wiele złóż, z wieloma żyłami kwarcu o średniej zawartości złota od 10 g/t do 60 g/t lub nawet 120 g/t. Ponadto zawierają one nieco mniej srebra oraz nieco cynku i ołowiu (ok. 1%). Analizowana próbka została pobrana za pomocą strugania w miejscach o widocznej mineralizacji siarczkowej w żyłach kwarcu w plagiogranicie. Celem tej pracy jest prawidłowe ustalenie występowania złota lub minerałów złotonośnych aby przetestować ich selektywną separację. Przedstawiono schemat technologiczny procesu przeróbki oraz bilans minerałów. Charakterystyka ziaren mineralnych w surowcu mineralnym została podana co jest bardzo istotne przy planowaniu technologii przeróbki. Jedną z zastosowanych metod jest rozdział w cieczach ciężkich przy gęstości 13.6 g/cm2.
EN
The methods are described of selective separation of thallium mineral lorandite from the Allchar hydrothermal-volcanogenic Sb-As-Tl deposit (FYR Macedonia) characterized by relatively complex mineralization. In addition to antimony and arsenic, the Allchar Mine at the village of Majden works one of the richest thallium mineral lorandite deposits. The aim of the research was to separate lorandite as much and as free grain as possible mainly through physical concentration. Thallium is very important because of a possibility to apply its mineral lorandite (TlAsS2) in obtaining knowledge in fundamental investigations. The reaction between Tl and solar neutrinos, producing Pb, is on the purpose of studying the neutrino flux from the Sun. For this purpose, a thallium-rich mineral is required as the target. Geochemically natural, pure thallium mineral lorandite is used to test solar neutrino under the current, two decades long LOREX Project. The Allchar ore from Crveni Dol contains a comparatively complex association of Sb-As-Tl minerals: pyrite, marcasite, antimonite, arsenopyrite, realgar, auripigmentum, barite, cinnabar, and accessory thallium lorandite, vrbaite, raguinite, picopaulite, parapierrotite, rebulite, greigite, tetrahedrite, and various sulphosalts that are found only in Allchar. The research used conventional laboratory methods for mineral fractionation and for liberation of lorandite grains, which included size reduction, sieve analysis, Wilfley table, sink and float analysis (bromoform, methylene iodide), electrostatic separation, electromagnetic separation and centrifugal separator. Gradual separation from successive communition and classification of fractions allowed separation of the free sink (heavy) product from which nonconductive minerals, including lorandite, were selected.
PL
Opisano wybrane metody separacji talu z minerału lorandytu ze złoża hydrotermalnego – wulkanogenicznego Sb-As-Tl w Allchar (Macedonia) charakteryzującego sie relatywnie złożoną mineralizacją. Oprócz antymonu i arsenu, kopalnia Allchar w wiosce Majden jest jednym z najbogatszych złóż talu w lorandycie. Celem badań było separacja lorandytu i uzyskanie jak największego uwolnienia minerałów za pomocą separacji mechanicznej. Tal występuje w minerale lorandyt (TlAsS2). Celem badań jest uzyskanie koncentratu bogatego w tal. Czysty tal w minerale lorandyt jest używany do badań neutrin w promieniowaniu kosmicznym w projekcie LOREX Project, realizowanym od 20 lat. Ruda Allchar z CrveniDol zawiera stosunkowo złożoną kombinację związków Sb-As-Tl: pirytu, markazytu, antymonianu, arsenopirytu, reaglaru, auripigmentu, barytu, cynobru, oraz dodatkowo związków talu lorandytu, vrbaitu, raguinitu, pikopaulitu, parapierrotytu, rebulitu, greigitu, tetrahedrytu i różnych sól siarkowych, które można znaleźć jedynie w Allchar. W badaniu zastosowano konwencjonalne metody laboratoryjne separacji mechanicznej i wydzielania ziaren lorandytu, uwzględniając rozdrabnianie, analizę sitową, wzbogacanie na stole Wilfley’a, analizę granulometryczna (w bromoformie, jodku metylenu), separację elektrostatyczną, separację elektromagnetyczną oraz separator odśrodkowy.
EN
The mineral deposit Bor-Cerovo is a relatively simple Cu-(Fe)ore that is becoming poorer and more complex in texture with the depth of mining. The Bor Copper Mine has expanded mine workings to the Cerovo field margins, where the same type of porphyry copper ore was found for which the Bor Mine is known as one of largest in Europe. Under the oxidized zone in the vertical deposit section lie paragenetic mineral associations typical of the cementated zone, or a transitional layer from the primary mineralized rock. Average concentrations of sulphide copper and oxide copper in the primary rock range from 0.263% to 0.164% and from 0.102% to 0.008%, respectively. Concentration of the ore of simple mineral composition has given a product of unsatisfactory both concentrate quality and metal recovery. More study is felt necessary of the structural/textural properties, of the identified mineral relations, and of the rate of mineral product liberation for the given grind fineness. Mineralogical analyses were conducted in the course of laboratory (and technological) tests. It has been learned that chemical analyses of the floatation concentrated material alone were inadequate, especially where complex texture of intergrowths and poor ore were involved. Structural properties and complex integrowths, and concequently low liberation degree, were found to be the reason of poor concentration. This paper discusses importance of the mineral liberation measurement for the technological results of copper ore concentration at the Bor-Cerovo flotation plant, and explains the functional relation between the mineral liberation and the grind fineness. Data on the microscopy of ore texture and the mineral liberation degree presented in this paper are aimed at improving the recovery and grade of chalcopyrite concentrate in the Veliki Krivelj Flotation Plant. Ore microscopy in the laboratory and technological tests indicate that chemical analysis as a tool for monitoring ore flotation is insufficient, especially where the processed ore is complex-textured and poor.
PL
Złoże mineralne Bor-Cerovo jest stosunkowo prostą rudą Cu-(Fe), która staje się uboższa i bardziej złożona w teksturze wraz z głębokością wydobywania. Kopalnia miedzi Bor rozszerzyła prace wydobywcze do granic obszaru Cerovo gdzie znaleziono ten sam typ porfirowej rudy miedzi, z którego kopalnia Bor jest znana jako największa w Europie. Poniżej strefy utlenionej w pionowej strefie złoża znajduje się zespół paragenetycznego minerału typowego dla strefy cementacji, lub warstwa przejściowa ze skały pierwotnie zmineralizowanej. Średnie stężenie siarczanu miedzi i tlenku miedzi w skale pierwotnej znajduje się w przedziale kolejno od 0,263% do 0,164% oraz od 0,102% do 0,008%. Stężenie w rudzie niezłożonego minerału daje produkt niezadowalający pod względem zarówno jakości koncentratu jak i odzysku metalu. Koniecznych jest więcej badań na temat właściwości strukturalnych/tekstury, identyfikacji zależności minerału, oraz na temat stopnia wyzwalania produktu mineralnego dla danego stopnia rozdrobnienia. Przeprowadzono analizę mineralogiczną podczas badań laboratoryjnych (i technologicznych). Dowiedziano się, że analiza chemiczna i flotacja koncentratu mineralnego była nieadekwatna, szczególnie gdy zaangażowana była skomplikowana struktura narostów między ziarnami i uboga ruda. Odkryto, że właściwości strukturalne i skomplikowane narosty, a co za tym idzie niski stopień uwalniania, były powodem ubogiej koncentracji. Artykuł ten omawia znaczenie pomiarów uwalniania minerału dla wyników technologicznych koncentracji miedzi w rudzie w zakładzie flotacyjnym Bor-Cerovo, i wyjaśnia funkcjonalną zależność miedzi uwalnianiem minerału a stopniem rozdrobnienia. Dane mikroskopowe tekstury rudy i stopnia uwalniania minerału prezentowane w tym artykule mają na celu polepszenie odzyskiwania i stopnia koncentratu chalkopirytu w zakładzie flotacyjnym VelikiKrivelj. Laboratoryjne i technologiczne badania mikroskopowe rudy wykazują, że analiza chemiczna jako narzędzie monitorowania flotacji rudy jest niewystarczająca, szczególnie jeśli przetwarzana ruda ma skomplikowaną teksturę i jest uboga.
EN
In this study, the fly ash taken from the lignite thermal power plant Kostolac-B, Kostolac, Serbia, is characterized and separated from its byproducts. Fly ash is composed of unburned carbon, iron compounds typically of magnetite, pozzolanic material and cenospheres. A systematic study is conducted to establish the optimum conditions for the separation of these materials from fly ash. In this context, concentration techniques such as magnetic, gravity separations (heavy liquids separation) and flotation are put forward. Finally the lightweight fraction, from which the magnetic minerals and the unburned coal substance were removed, as well as microspheres, is an excellent material for the production of building materials – blocks and bricks, for concrete mixtures, cement additives, for fly ash pelletization process using Portland cement binder and other purposes. The main elements (fractions of valuable components) of the fly ash that determine its usability are: the quantity of unburned carbon, content of iron compounds (typically of magnetite and haematite), the pozzolanic material, microsphere (cenospheres) content, size distribution, mechanical properties of the pellets etc. The preliminary investigations and accomplished tests exhibited satisfactory results.
PL
Streszczenie W artykule przedstawiono charakterystykę oraz wyniki badań nad wzbogacaniem popiołów lotnych ze spalania węgla w Ciepłowni Kostolac –B w miejscowości Kosolac w Serbii. Popioły lotne składają się z niedopału węgla, składników żelazo nośnych (najczęściej magnetyt, materiałów pucolanowych i cenosfer. Celem badań było określenie optymalnych warunków separacji popiołów. Badania przeprowadzono wykorzystując metody wzbogacania magnetycznego, grawitacyjnego(wzbogacanie w cieczy ciężkiej) i flotacji. W końcowym etapie wzbogacania uzyskano frakcję lekką, pozbawiona części magnetycznej i niedopału oraz ceno sfer, która może być wykorzysta na do produkcji materiałów budowlanych – bloczków, cegieł, betonu, dodatków do cementu, jako dodatek do procesu pelletyzacji z wykorzystaniem cementu portlandzkiego i podobnych zastosowań. Najważniejsze czynniki, które decydują o jakości popiołu są ilość niedopału, zawartość minerałów żelaza (magnetyt, hematyt), zawartość pucolanów i mikrosfer (ceno sfery), sklad ziarnowy, właściwości mechaniczne peletów itd. Wstępne badania i testy dały zadowalające wyniki.
EN
The effect of lead ions on the galena and sphalerite surface properties, ethylxanthate adsorption in alkaline medium were studied for the possible use of recycled flotation water. The flotation tests and the zeta-potential measurements were carried out and correlated with the results of the infrared attenuated total reflection spectrophotometry (ATR-IR) and UV data. Lead adsorbed on the galena or sphalerite surface as Pb()H)+ and less as Pb 2+ reduces the collectorless galena floatabiblity from pH 7 to 9.5, but has a strong activating effect on natural sphalerite floatability (in PH range 7.6-10.5). After collection of Pb-modifield minerals with K-ethylxanthate both forms of lead athylxanthate, monolayer Pb-EX (chemiclally adsorbed (EX~), and multilayer, physically adsorbed Pb (EX)2 were detection on the mineral surface. Sphalerite flotated nearly 100% in the examined pH range but galena floated better anly from PH 8 to 9.5 (85-95%). The main surface reaction in pH range 8-9,5 is probably the ion-exchange reaction M-Pb-OH + (EX)- = M-Pb-EX +(OH)- (M - mineral), which contributes to the chemical adsorption of (EX)- ion is the reaction of pseudo-first order (on Pb-midifield galena - rate constant is k = 0.711 min -1; on Pb-modifield sphalerite k=0.102 min -1).
PL
Badano wpływ jonów ołowiu (II) na powierzchniowe właściwości galeny i sfalerytu oraz kinetykę adsorpcji ksantogenianu etylowego w środowisku alkalicznym w celu określenia możliwości ponownego użycia wód flotacyjnych. Przeprowadzono flotację i pomiary potencjału dzeta, które skorelowane z wynikami wod flotacyjnych. Przeprowadzono flotację i pomiary potencjału dzeta, które skorelowano z wynikami badań spektroskopowych w podczerwieni (ATR-IR) i ultrafilolecie (UV). Ołów zaadsorbowany na powierzchni galeny i sfalerytu jako Pb(OH) oraz mniejszym stopniu jako Pb +2 redukuje flotowalność galeny w zakresie pH od 7 do 9,5 oraz ma silne działanie aktywacyjne na naturalną flotowalność sfalertu w zakresie pH od 7,6 do 10,5. Na powierzchniach ziarn minerałów aktywowanych jonami ołowiu i wyflotowanych za pomocą ksantogenianu etylowo-potasowego wykryto obie formy ksantogenianu ołowiu tj. monowarstwę chemiczne zaadsorbowanego ksantogenianu (-Pb-EX) i wielowarstwę fizycznie zaadsorbowanego (Pb(EX)2. Sfaleryt flotował prawie całkowicie w badanym zakresie pH, a galena flotowała lepiej tylko przy pH od 8do 9,5 przy uzysku 85-95%. Główne reakcje zachodzące na powierzchni w zakresie pH 8-9,5 to prawdopodobie reakcja wymiany M-Pb-OH + (EX)- =M-Pb-EX + (OH)- , gdzie M oznacza minerał, co daje chemicznie zaadsorbowaną monowarstwę -Pb-EX na powierzchni minerału. Reakcja pomiędzy minerałem, który był modyfikowany jonami ołowiu i jonem (EX)- jest reakcją pseudo pierwszego rzędu. Na galenie modyfikowanej jonami ołowiu stała szybkość wynosi k=0,711 min -1 podczas gdy na modyfikowanym jonami ołowiu sfalerycie ma wartość k=0,102 min -1.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.