Mechanism and Kinetics Studies on Non-Isothermal Decomposition of Ludwigite in Inert Atmosphere

Autorzy
Treść / Zawartość
Identyfikatory
Warianty tytułu
Języki publikacji
EN
Abstrakty
EN
Ludwigite is the main available boron-bearing resource in China. In order to enrich the theory system and optimize its utilization processes, this paper study the mechanism and kinetics on non-isothermal decomposition of ludwigite in inert atmosphere by means of thermal analysis. Results show that, the decomposition of serpentine and szajbelyite is the main cause of mass loss in the process. At the end of decomposition, hortonolite and ludwigite are the two main phases in the sample. The average E value of structural water decomposition is 277.97 kJ/mol based on FWO method (277.17 kJ/mol based on KAS method). The results is proved to be accurate and reliable. The mechanism model function of structural water decomposition is confirmed by Satava method and Popescu method. The form of the most probable model function is G(α) = (1 – α)–1– 1 (integral form) and f (α) = (1 – α)2 (differential form), and its mechanism is chemical reaction. This is verified by the criterion based on activation energy of model-free kinetics analysis.
Twórcy
autor
  • Northeastern University, School of Metallurgy, No. 3-11, Wenhua Road, Heping District, Shenyang, P. R. China, 110819 Shenyang, China
autor
  • Northeastern University, School of Metallurgy, No. 3-11, Wenhua Road, Heping District, Shenyang, P. R. China, 110819 Shenyang, China
autor
  • Northeastern University, School of Metallurgy, No. 3-11, Wenhua Road, Heping District, Shenyang, P. R. China, 110819 Shenyang, China
autor
  • Northeastern University, School of Metallurgy, No. 3-11, Wenhua Road, Heping District, Shenyang, P. R. China, 110819 Shenyang, China
Bibliografia
  • [1] X. J. Zheng, Boron Iron Ore Processing, Chemical Industry Press, Beijing (2009).
  • [2] Q. M. Peng, M. R. Palmer, Econ. Geol. 97, 93-108 (2002).
  • [3] X. J. Zheng, Production and Application of Boron Compounds, Chemical Industry Press, Beijing (2008).
  • [4] Y. F. Lu, Y. C. Cheng, H. Q. Li, C. J. Xue, F. W. Cheng, Acta Geol. Sin. 79, 408-414 (2005).
  • [5] Y. Z. Wang, S. J. Liu, Y. G. Jia, R. J. Li, Non-f errous Mining and Metallurgy 23 (3), 5-8 (2007).
  • [6] X. J. Fu, J. Q. Zhao, S. Y. Chen, Z. G. Liu, T. L. Guo, M. S. Chu, J. Iron Steel Res. Int. 22 (8), 672-680 (2015).
  • [7] G. Wang, J. S. Wang, Y. G. Ding, S. Ma, Q. G. Xue, ISIJ Int. 52, 45-51 (2012).
  • [8] S. L. Liu, C. M. Cui, X. P. Zhang, ISIJ Int. 38 (10), 1077-1079 (1998).
  • [9] Z. D. Yang, S. L. Liu, Z. F. Li, X. X. Xue, J. Iron Steel Res. Int. 14 (6), 32-36 (2007).
  • [10] X. P. Zhang, J. F. Lang, C. M. Cui, S. L. Liu, Iron and Steel, 30 (12), 9-12 (1995).
  • [11] Y. G. Ding, J. S. Wang, G. Wang, S. Ma, Q. G. Xue, J. Ir on Steel Res. Int. 19 (6), 9-13 (2012).
  • [12] J. Li, Z. G. Fan, Y. L. Liu, S. L. Liu, T. Jiang, Z. P. Xi, Trans. Nonferrous Met. Soc. China, 20 (6), 1161-1165 (2010).
  • [13] A. Mergen, M. H. Demirhan, M. Bilene, Adv. Powder Technol. 14 (3), 279-293 (2003).
  • [14] Z. T. Sui, P. X. Zhang, C. Yamauchi, Acta Mater. 47 (4), 1337-1344 (1999).
  • [15] P. X. Zhang, Z. T. Sui, Metall. Mater. Trans. B 26 (2), 345-351 (1995).
  • [16] N. Acarkan, G. Bulut, O. Kangal, G. Onal, Mine. Eng. 18 (7), 739-741 (2005).
  • [17] G. H. Li, B. J. Liang, M. J. Rao, Y. B. Zhang, T. Jiang, Mine. Eng. 56, 57-60 (2014).
  • [18] R.Z . Hu, Thermal Analysis Kinetics[M]. 2nd ed. Science Press, Beijing (2008).
  • [19] S. Vyazovkin, C. A. Wight, Int. Rev. Phys. Chem. 17 (3), 407-433 (1998).
  • [20] S. Vyazovkin, Int. Rev. Phys. Chem. 19 (1), 45-60 (2000).
  • [21] T. Ozawa, Bull. Chem. Soc. Jan. 38 (11), 1881-1886 (1965).
  • [22] J. H. Flynn, L. A. Wall, J. Polym. Sci. Part B, Polymer Letters. 4 (5), 323-328 (1996).
  • [23] H. E. Kissinger, Anal. Chem. 29 (11), 1702-1706 (1957).
  • [24] V. Satava, Thermochim. Acta. 2 (5), 423-428 (1971).
  • [25] C. Popescu, Thermochim. Acta. 285 (2), 309-323 (1996).
  • [26] J. J. Zhang, N. Ren, J. H. Bai, Chin. J. Chem. 24 (3), 360-364
Uwagi
EN
1. This work is supported by Ph. D. Programs Foundation of Ministry of Education of China (No. 20100042110004) and Fundamental Research Funds for the Central University (No. N090502004 and N140206003).
PL
2. Opracowanie rekordu w ramach umowy 509/P-DUN/2018 ze środków MNiSW przeznaczonych na działalność upowszechniającą naukę (2018).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-f33cfed1-896b-4c19-bd64-8128ec95e49d
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.