Effect of titanium source and sol-gel TiO2 thin film formation parameters on its morphology and photocatalytic activity

Identyfikatory
Warianty tytułu
Języki publikacji
EN
Abstrakty
EN
TiO2 thin films with different surface structure have been prepared from alkoxide solutions by the sol-gel method using different cationic precursors and heat treatment techniques. The effect of using titanium isopropoxide as well as titanium butoxide as a titanium source on the surface structure and photocatalytic activity of the resultant thin films was studied. Significant differences in the rate of hydrolysis and condensation reactions during the sol-gel synthesis were observed for these titanium precursors. This had a direct influence on the morphology of the as-prepared TiO2 films. Higher quality oxide coatings were obtained from titanium isopropoxide. They were characterized by a smaller grain size, improved surface roughness and uniform coverage of the glass substrate. A beneficial effect of calcination process after each sol application cycle in contrast to single step calcination after all dip-coating cycles was observed. Photocatalytic degradation tests showed that methyl orange was decolorized in the presence of all prepared TiO2 films by exposing their aqueous solutions to UV light (λ = 254 nm). The highest photocatalytic activity had the TiO2 layer produced using titanium isopropoxide.
Słowa kluczowe
Wydawca
Rocznik
Strony
424--433
Opis fizyczny
Bibliogr. 32 poz., rys., tab.
Twórcy
autor
  • Faculty of Chemical Engineering and Technology, Cracow University of Technology, 24 Warszawska St., 310155 Cracow, Poland
autor
  • Faculty of Chemical Engineering and Technology, Cracow University of Technology, 24 Warszawska St., 310155 Cracow, Poland
  • Faculty of Chemical Engineering and Technology, Cracow University of Technology, 24 Warszawska St., 310155 Cracow, Poland
Bibliografia
  • [1] MOHAMED K.K., The Impact of Air Pollution on Health, Economy, Environment and Agricultural Sources, InTech, Rijeka, 2011.
  • [2] MARCELO L.L., SONIA S., Emerging Pollutants in the Environment - Current and Further Implications, In-Tech, Rijeka, 2015.
  • [3] SCHULTZ D.M., YOON T.P., Science, 343 (6174) (2014), 1239176.
  • [4] MONDAL K., SHARMA A., RSC Adv., 6 (87) (2016), 83589.
  • [5] BARATI N., SANI M.A.F., SADEGHIAN Z. GHASEMI H., Prot. Met. Phys. Chem., 50 (2014), 371.
  • [6] BARATI N., SANI M.A.F., GHASEMI H., Prot. Met. Phys. Chem., 49 (2013), 109.
  • [7] LI F., LI Q., KIM H., Appl. Surf. Sci., 276 (2013), 390.
  • [8] ZHAO Y.L., SONG D.M., QIANG Y.H., GU X.Q., ZHU L., SONG C.B., Appl. Surf. Sci., 309 (2014), 85.
  • [9] SHANAGHI A., ROUHAGHDAM A.S., SHAHRABI T., ALIOFKHAZRAEI M., Mat. Sci., 44 (2) (2008), 233.
  • [10] BURTAN B., REBEN M., CISOWSKI J., WASYLAK J., NOSIDLAK N., JAGLARZ J., JARZABEK B., Acta Phys. Pol. A, 120 (4) (2011), 579.
  • [11] MARSZAŁEK K., WINKOWSKI P., JAGLARZ J., Mater. Sci.-Poland, 31 (2014), 80.
  • [12] REBEN M., DOROSZ D., WASYLAK J., BURTAN B., JAGLARZ J., ZONTEK J., Opt. Appl., 42 (2) (2012), 353.
  • [13] MARKKU L., MIKKO R., Thin Solid Films, 409 (2002), 138.
  • [14] HANS B., DIETER K., Thin films on glass, Springer-Verlag, Berlin Heidelberg, 2003.
  • [15] MOSER E.M., CHAPPUIS S., OLLEROS J., Surf. Coat. Tech., 227 (2013), 2.
  • [16] SCHEFFEL B., MODES T., METZNER C., Surf. Coat. Tech., 287 (2016), 138.
  • [17] VERA M.L., ALTERACH M.Á., ROSENBERGER M.R., LAMAS D.G., SCHVEZOV C.E., ARES A.E., Nanomater. Nanotech., 4 (1) (2014), 1.
  • [18] LEE D-S., LIU T-K., J. Sol-Gel Sci. Techn., 25 (2) (2002), 121.
  • [19] SEDIK A., FERRARIA A-M., CARAPETO A-P., BELLAL B., TRARI M., OUTEMZABET R., J. Electr. Eng., 68 (2017), 31.
  • [20] ASHKARRAN A-A., MOHAMMADIZADEH M-R., Mater. Res. Bull., 43 (2008), 522.
  • [21] SU C., TSENG C-M., CHEN L-F., YOU B-H., HSU BC., CHEN S-S., Thin Solid Films, 498 (2006), 259.
  • [22] SU C., HONG B-Y., TSENG C-M., Catal. Today, 96 (2004), 119.
  • [23] KOMINAMI H., KATO J.-I., MURAKAMI S.-Y., KERA Y., INOUE M., INUI T., OHTANI B., J. Mol. Catal. A Chem., 144 (1999), 165.
  • [24] ALZAMANI M., SHOKUHFAR A., EGHDAM E., MASTALI S., Prog. Na. Sci.-Mater., 23 (1) (2013), 77.
  • [25] BENSOUICI F., SOUIER T., IRATNI A., DAKHEL A.A., TALA-IGHIL R., BOUOUDINA M., Surf. Coat. Tech., 251 (2014), 170.
  • [26] SO W-W., PARK S-B., KIM K-J., MOON S-J., J. Colloid. Inerface. Sci., 191 (1997), 398.
  • [27] OHYA Y., MISHINA J., MATSUDA T., BAN T., TAKAHASHI Y., J. Am. Ceram. Soc., 82 (10) (1999), 2601.
  • [28] KEDDIE J.L., GIANNELIS E.P., J. Am. Ceram. Soc., 74 (10) (1991), 2669.
  • [29] KEDDIE J.L., BRAUN P.V., GIANNELIS E.P., J. Am. Ceram. Soc., 77 (6) (1994), 1592.
  • [30] KENANAKIS G., VERNARDOU D., DALAMAGKAS A., KATSARAKIS N., Catal. Today, 240 (2015), 146.
  • [31] BOUACHIBA Y., BOUABELLOU A., HANINI F., KERMICHE F., TAABOUCHE A., BOUKHEDDADEN K., Mater. Sci.-Poland, 32 (1) (2014), 1.
  • [32] NEGISHI N., TAKEUCHI K., IBUSUKI T., J. Sol-Gel Sci. Techn., 13 (1998), 691.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-d432f0ff-1578-4daf-96be-bafd160d1da9
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.