Features of Formation Stress State of Amorphized Detonation Coatings of the Zr-Al-B Systems

Treść / Zawartość
Identyfikatory
Warianty tytułu
Języki publikacji
EN
Abstrakty
EN
The results of experimental studies on the dependence of the thickness of amorphous-crystalline Zr-Al-B coatings on the value and level of distribution of type 1residual stresses were presented. It was demonstrated that residual compressive stresses arise in the surface layers of coatings, which in absolute value are not significant for its integrity and quality. It was established that the amorphous-crystalline composition, under the conditions of minimizing residual stresses and the optimal combination of the volume fraction of components, the structure and morphology of their components, has the best surface strength and wear resistance under friction compared to tungsten carbide and iron coatings
Twórcy
  • Department of Fundamentals of Technology, Lublin University of Technology, Nadbystrzycka 38, 20-618 Lublin, Poland
  • Airport Technology Department, National Aviation University, ave. Kosmonavta Komarova, 1, Kiev, 03067, Ukraine
  • Institut of Engineering Thermophysics of National Academy of Scinces of Ukraine, Kiev, Ukraine
  • Department of Fundamentals of Technology, Lublin University of Technology, Nadbystrzycka 38, 20-618 Lublin, Poland
  • Khmelnitskee National university, Mailing str. Institutskaya, 11, Khmelnitskee-16, 29016, Ukraine
Bibliografia
  • 1. Babak V.P., Shchepetov V.V., Nedayborshch S.D. Wear resistance under vacuum of nanocomposite coatings with dry lubricant. Scientific Bulletin of NMU, 2016, 1, 47-52.
  • 2. Babak V.P.. Shchepetov V.V. Wear resistance of amorphous crystalline coatings under lubrication. Friction and Wear, 2018, 39(1), 50-56.
  • 3. Dinzhos R.V., Fialko N.M., Lysenkov E.A. Analysis of the Thermal Conductivity of Polymer nanocomposites Filled with Carbon Nanotubes and Carbon Black. Journal of Nano- and Electronic Physics, 2014, 6(1), 1015-1021.
  • 4. Nedayborsch S.D., Shchepetov V.V. Wear resistance of Cr-Si-B detonation coatings under friction loading at high temperatures. Powder Metallurgy, 2014, 1/2, 81-89.
  • 5. Nedayborsch S.D. Rules and wear mechanism of Cr-Si-B detonation coatings under friction loading in the absence of lubricant. Problems of friction and wear, 2010, 54, 163-170.
  • 6. Pashechko M., Lenik K. Segregation of atoms of the eutectic alloys Fe-Mn-C-B-Si-Ni-Cr at friction wear. Wear, 2009, 267, 1301-1304.
  • 7. Pashechko M. Wear resistance of eutectic coatings of the Fe–Mn–C–B system alloyed with Si, Ni and Cr. Materials Science, 2011, 46(5), 695–701.
  • 8. Patent No. 82902 of Ukraine. Wear-resistant amorphous zirconium based material; С22С 9/01. О.V. Kharchenko, V.V. Shchepetov, M.S. Yakovleva and others. Declared. dated 19.12.2012; Bull. No. 16
Uwagi
Opracowanie rekordu w ramach umowy 509/P-DUN/2018 ze środków MNiSW przeznaczonych na działalność upowszechniającą naukę (2019).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-c6ac7306-bab3-431e-9ed1-a62e395789d5
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.