The influence of aging process parameters on selected mechanical properties of profiles from EN AW-6106 aluminium alloy

Identyfikatory
Warianty tytułu
PL
Wpływ parametrów procesu starzenia na wybrane właściwości mechaniczne profili ze stopu aluminiowych EN AW-6106
Języki publikacji
EN
Abstrakty
EN
The aim of this article was to analyze the influence of temperature and time period of artificially aging process on selected mechanical properties: Brinell hardness, yield strength, tensile strength, and elongation of hot extruded profiles from EN AW-6106 aluminum alloy. The result of the conducted research has pointed out that the temperature and the time of aging process had a significant effect on the selected mechanical properties. In the study it was found that the highest mechanical properties such as the yield strength and tensile strength for analyzed aluminum alloy were achieved for samples aged in temperature of 165°C for time period of 6 hours. The value of mechanical properties required be the standards for T6 temper were achieved after 2 hours of artificial aging in temperature of 165°C.
PL
Celem pracy była analiza wpływu temperatury i czasu procesu sztucznego starzenia na wybrane właściwości mechaniczne: twardość Brinella, umowną granice plastyczności, wytrzymałość na rozciąganie i wydłużenie wyciskanych na gorąco profili ze stopu aluminium EN AW-6106. Wyniki przeprowadzanych badań wykazały, że temperatura i czas procesu sztucznego starzenia ma istotny wpływ na wybrane do badań właściwości mechaniczne. W badaniach stwierdzono, że najwyższą wartość własności mechanicznych takich jak: umownej granicy plastyczności oraz wytrzymałości na rozciąganie uzyskano po przeprowadzonym procesie sztucznego starzenia w temperaturze 165°C przez czas 6h. Niezbędny poziom własności mechanicznych wymaganych przez normy dla stanu T6 osiągnięto już po dwóch godzinach procesu starzenia w temperaturze 165°C.
Rocznik
Strony
62--65
Opis fizyczny
Bibliogr. 16 poz., fig., tab.
Twórcy
autor
  • University of Technology, The Faculty of Production Engineering and Materials Technology, Institute of Metal Forming and Safety Engineering
  • University of Technology, The Faculty of Production Engineering and Materials Technology, Institute of Metal Forming and Safety Engineering
  • University of Technology, The Faculty of Production Engineering and Materials Technology, Institute of Metal Forming and Safety Engineering
autor
  • University of Technology, The Faculty of Production Engineering and Materials Technology, Institute of Metal Forming and Safety Engineering
Bibliografia
  • [1] Dobrzański Leszek. A. 2006. Podstawy nauki o materiałach i metaloznawstwo. Warszawa: Wydawnictwo Naukowo Techniczne.
  • [2] Goryckiewicz Ryszard. 2003. „Wpływ twardości i mikrostruktury stopów aluminium na udarność”. Archiwum Odlewnictwa 8: 279-286. Katowice: Polish Academy of Sciences.
  • [3] Kawecki Artur. 2013. Wysoko wytrzymałe stopy Cu-Ag o wysokiej przewodności elektrycznej. Kraków: Wydawnictwo: Wzorek.
  • [4] Mróz Sebastian, Szota Piotr, Stefanik Andrzej,Wąsek Seweryn, Stradomski Grzegorz. 2015. Analysis of Al-Cu bimetalic bars properties after explosive welding and rolling in modified passes. Archives of Metallurgy and Materials Volume 60, Issue 1: 427-432.
  • [5] Podręcznik konstruktora. 1997. Jak radzić sobie z profilami aluminiowymi. Trzcianka: Dział Marketingu SAPA.
  • [6] PN-EN 573-3:2014-02. 2014. Aluminium and aluminium alloys - Chemical composition and form of wrought products - Part 3: Chemical composition and form of products. Warszawa: Polski Komitet Normatyzacyjny.
  • [7] PN-EN ISO 6892-1:2016, Metale Metallic materials - Tensile testing - Part 1: Method of test at room temperature, Polski Komitet Normatyzacyjny, Warszawa.
  • [8] [PN-EN ISO 6506-1:2014-12. 2014. Metallic materials - Brinell hardness test - Part 1: Test method. Warszawa: Polski Komitet Normatyzacyjny.
  • [9] PN-EN 755-2:2016, Aluminium Aluminium and aluminium alloys. Extruded rod/bar, tube and profiles – Part 2: Mechanical properties, Polski Komitet Normatyzacyjny, Warszawa 2010.
  • [10] Richert Jan. 2010. Innowacyjne metody przeróbki plastycznej metali. Kraków: Wydawnictwo AGH.
  • [11] Richert Jan, Mroczkowski Marcin, Gellner Jerzy. 2006. „Nowy sposób starzenia stopów AlMgSi wyciskanych w stanie T5”. Rudy i Metale Nieżelazne Nr 12: 747-753. Warszawa: Sigma-NOT.
  • [12] Richert Jan, Woźnicka Agata. 2013. „Przeróbka plastyczna trudno odkształcalnych stopów aluminium zintegrowana z przesycaniem”. Rudy i Metale Nieżelazne Nr 2: 90-95. Warszawa: Sigma-NOT.
  • [13] Romański Piotr, Adamczyk Justyna, Pilarczyk Jan Walenty. 2014. „The influence of temperature and time period of ageing process of extruded aluminium profiles from 6063 alloy on the selected mechanical properties”. XV International Scientific Conference - New Technologies and Achievements in Metallurgy and Material Engineering and Production Engineering, Monografia Nr 40: 150-155. Częstochowa: Wydawnictwo Wydziału Inżynierii Produkcji i Technologii Materiałów Politechniki Częstochowskiej.
  • [14] Romański Piotr, Stradomski Grzegorz, Ciepiela Wojciech, Pilarczyk Jan Walenty. 2015. „The influence of heat treatment on toughness of extruded profiles from EN AW-6060 aluminium alloy”, Hutnik Wiadomości Hutnicze Nr 1: 101-104. Warszawa: Sigma-NOT.
  • [15] Romański Piotr, Stradomski Grzegorz, Pilarczyk Jan Walenty. 2016. „The influence of heat treatment on toughness of extruded profiles from EN AW - 6063 aluminium alloy”, Hutnik-Wiadomości Hutnicze 5: 223−227.
  • [16] Wendland Justyna, Borowski Jacek, Jurczak Henryk. 2014. „Matryce do wyciskania profili aluminiowych i sposoby ich umacniania”. Projektowanie I Konstrukcje Inżynierskie 4. Warszawa: Wydawnictwo: ITER.
Uwagi
Opracowanie ze środków MNiSW w ramach umowy 812/P-DUN/2016 na działalność upowszechniającą naukę (zadania 2017).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-c517197e-dc80-4c7a-8e04-4b449e980239
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.