Brass as an alloy composed mainly of copper is great industrial uses such as heat exchangers and similar other facility due to its good thermal properties. Due to the presence of the considerable ratio of zinc the alloy suffers from zinc dissolution or dezincification. Dezincification rate increases with the increase in the ratio of zinc in the alloy. In this study benzothiazole (BTH) and its substituent’s 2-methylbenzothiazole (MeBTH), 2-aminobenzothiazole (ABTH), 2-mercaptobenzothiazole (MBTH) and 2-phenylbenzothiazole (PhBTH) have been used as corrosion inhibitors for α-brass in stirred 0.1 M HClO4. The methods of investigation include weight loss, Tafel and linear polarizations and electrochemical impedance spectroscopy. The order of inhibition efficiency (% E) was calculated and the values obtained has indicated the sequence of inhibition efficiency was found to be BTH < MeBTH < ABTH < PhBTH < MBTH. The calculated values of thermodynamic parameters support this order. The inhibitors were found to suppress the corrosion rate by the formation of films which were identified by IR, SEM and EDAX techniques.
Słowa kluczowe
Rocznik
Tom
Strony
87--102
Opis fizyczny
Bibliogr. 43 poz., rys., tab.
Twórcy
autor
- Department of Chemistry & Industrial Chemistry, College of Appl. Sci., University of Bahri, Sudan
autor
- Department of Chemistry & Industrial Chemistry, College of Appl. Sci., University of Bahri, Sudan
autor
- Department of Chemistry & Industrial Chemistry, College of Appl. Sci., University of Bahri, Sudan
autor
- Department of Chemistry & Industrial Chemistry, College of Appl. Sci., University of Bahri, Sudan
Bibliografia
- [1] S. L. Li, H. Y. Ma, S. B. Lei, R. Yu, S. H. Chen, D. X. Liu, Corrosion 54 (1998) 947-954.
- [2] Vinicius C. Machado, Annelise M. Schmidt, Denise S. Azambuja, J. Braz. Chem. Soc. 11(4) (2000) 387-392.
- [3] Gomma G. K., Wahdan M., Bull. Chem. Soc. Jpn. 67 (1994) 2621-2626.
- [4] Hur E., Varol G. A., Gorgun K., Sakarya H., J. of Sci. 24 (4) (2011) 699 707.
- [5] Quraishi M. A., Khan M. A., Wajid Ajmal, M., Muralidharan S., Iyer S. Venkatakrishna, British Corrosion Journal 32(1) (1997) 72-76.
- [6] Quraishi M. A., Wajid Khan M. A., Ajmal A., Muralidharan S., J. Appl. Electrochem. 26 (1996) 1253-1258 .
- [7] Al-Mayouf A. M., Al-Suhybani A. A., Al-Ameery A. K., Desalination 116(1) (1998) 25-33.
- [8] Quraishi M. A., Ahamed M. A. S., Venkatchari G., Bull. Electrochem. 13 (1997) 257 -259.
- [9] Rafique M. Z. A., Khan S., Saxena N., Quraishi M. A., Electrochim. Acta 25 (4) (2007) 419-434.
- [10] Antonijevic M. M., Petrovic M. B., A review. Int. J. Electrochem. Sci. 3 (2008) 1-28.
- [11] Nandeesh L. S., Sheshadri B. S., Br. Corr. J. 23 (4) 91988) 239-244.[12] Rehan H. H.,Material Science and Engineering Technology 24 (8) (1993) 304-308.
- [13] Vastag Gy., Szocs E., Shaban A., Bertoti I., Popov-Pergal K., Kalman E., Solid State Ionics 141-142 (2001) 87-91.
- [14] Ramji K., Cairns D. R., Rajeswari S., Appl. Surf Sci. 254 (2008) 4483-4493.
- [15] Rawat J., Quraishi M. A., Corrosion 59(3) (2003) 238-241.
- [16] Shanbhag A. V., Venkatesha T. V., Prabha A., Praveen B. M., Bull. Mater. Sci. 34(3) (2011) 571-576.
- [17] Samar Y. Al-Nami, J. Mater. Environ. Sci. 4(1) (2013) 39-48.
- [18] Osarolube E., Owate I. O., Oforka N. C., Scientific Research and Essay 3(6) (2008) 224-228.
- [19] Fontana M. G., Stactile W., Corrosion Science and Technology, Plenum Press, London, 1 (1970) 149.
- [20] Yurt A., Mihrican Y., Anti-Corros. Methods Mater. 55(4) (2008) 195-203.
- [21] Quraishi M. A., Mideen A. S., Khan M. A. W., Ajmal M., Indian Journal of Chemical Technology 1 (1994) 329.
- [22] Rosliza R., Wan Nik W. B., Curr. Appl. Phy. 10 (1) (2010) 221-229.
- [23] Gao B., Zhang X., Sheng Y., Mater. Chem. Phys. 108(2-3) (2008) 375-381.
- [24] Stern M., Geary A. J., Electrochem. Soc. 104 (1957) 56-63.
- [25] Tebbji K., Oudda H., Hammouti B., Benkaddour M., Elkodadi M., Ramadani A., Colloids and surfaces physiochemical and engineering aspects 259 (1-3) (2005) 143-149.
- [26] S. Muralidharan, K. L. N. Phani, S. Pitchumani, S. Ravichandran, S. V. K. Iyer, J. Electrochem. Soc. 142(5) (1995) 1478-1483.
- [27] Juttner K., Electrochim. Acta 35 (10) (1997) 1501-1508.
- [28] Mansfeld F., Electrochim. Acta 35 (10) (1990) 1533-1544.
- [29] Franklin T. S., Rajesh A., Sheik Mideen A., Karthikeyan J., Anitha S., Indian Journal of Science and Technology 6 (2012) 1810-1815.
- [30] Lece H. D., Kaan A., Emregtil C., Orhan A. Cotrrosion Sci. 5 (2008) 1460-1468.
- [31] Loto R. T., Loto A. A., Popoola A A. P. I., J. Mater. Environ. Sci. 3(5) (2012) 885-894.
- [32] Shahrabi T., H. Tavakholi, M. G. Hosseini, Anti-Corros. Methods Mater. 54 (2007) 308-313.
- [33] Patel N. K., Makwana S. C., Patel M. M., Corr. Sci. 14 (1974) 91-94.
- [34] Mantell A. E., Smith R. M., Critical Stability Constant, Plenum N.Y., 1997, vol. 3,p. 313.
- [35] Kumar S., Sankara Narayanan T. S. N., Suresh Kumar M., Manimaran M.,International Journal of Electrochemical Science 1 (2006) 456-459.
- [36] Oshawa M., Suetaka W., Corr. Sci. 19 (7) (1979) 709-722.
- [37] Trabanelli G., Carassiti V., in Advances in Corrosion Science and Technology, 1, p. 147, Plenum Press, N.Y., 1970.
- [38] Zhang D. Q., Gao L. X., Zhou G. D., Corrosion Science 46(12) (2004) 3031-3040.
- [39] Rao C. N. R., Chemical Application of Infrared Spectroscopy, P-330, Academic Press, N.Y. (1963).
- [40] Bellamy L. J., Advances in IR Group Frequencies, Chapman and Hall, London 1980.
- [41] Motevalli M., O’Brien P., Walsh J. R., Watson I. M., Polyhedron 15 (1996) 801-808.
- [42] Barsoukov E., Maodona J. R., Impedance Spectroscopy: Theory, Experiment and Application, J.Wiley & Sons, 2005.
- [43] Musa E. Mohamed, Kamal K. Taha, Nature and Science 9(8) (2011) 34-39.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-b36b5a5c-5e56-46be-afe9-40c1285d8d74