An improvement in fatigue strength is one of the main factors enabling the use of high-durability Al-Mg-Mn-Sc-Zr alloys in functional components of mobile robots. As part of this study, a computer simulation was carried out using ANSYS LS-DYNA software that involved the hybridization of high pressure torsion (HPT) and shot peening (SP) forming processes. The numerical analysis was aimed at determining residual stresses and strains that affect the durability and stress characteristics of the analyzed Al alloy. Results of the study indicate that tensile stresses of σ = 300 MPa generated as a result of HPT are transformed into a beneficial stress of σ = 25 MPa resulting from plastic strains caused by SP surface treatment.
Twórcy
  • Lodz University of Technology, Institute of Materials Science and Engineering, 1/15 Stefanowskiego Str., 90-924 Lodz, Poland
  • Lodz University of Technology, Institute of Materials Science and Engineering, 1/15 Stefanowskiego Str., 90-924 Lodz, Poland
autor
  • Lodz University of Technology, Institute of Materials Science and Engineering, 1/15 Stefanowskiego Str., 90-924 Lodz, Poland
  • Lodz University of Technology, Institute of Materials Science and Engineering, 1/15 Stefanowskiego Str., 90-924 Lodz, Poland
  • Lodz University of Technology, Institute of Materials Science and Engineering, 1/15 Stefanowskiego Str., 90-924 Lodz, Poland
autor
  • Lodz University of Technology, Institute of Materials Science and Engineering, 1/15 Stefanowskiego Str., 90-924 Lodz, Poland
Bibliografia
  • [1] A. Zaki, U. Anwar, Corr. Sci. 43, 1227-1243 (2001).
  • [2] S. Costa, H. Puga, J. Barbosa, A.M.P. Pinto, Mat. Sci. and Design. 42, 347-352 (2012).
  • [3] Z. Jia, J. Røyset, J. K. Solberg, Q. Liu, Trans. Nonferrous Met. Soc. China 22, 1866-1871 (2012).
  • [4] Y. Kun, L. Wenxian, L. Songrui, Z. Jun, Mat. Sci. and Eng. A. 368, 88-93 (2004)
  • [5] B. Fuller Christian, Submitted To The Graduate School In Partial Fulfillment Of The Requirements, Evanston, Illinois 2003.
  • [6] S. A. Meguid, G. Shagal, J.C. Stranart, J. Daly, Finite Elements in Analysis and Design. 31, 179-191 (1999).
  • [7] J. Li, Z. Peng, C. Li, W. Chen, Z. Zheng, Trans. Nonferrous Met. Soc. China 18, 755-762 (2008).
  • [8] CN 103480789 - Pressure-torsion forming method of high- -strength aluminium-alloy disc-shaped workpiece 2013.
  • [9] CN 102189706- High-pressure shearing deformation method and device for tubular materials 2011.
  • [10] S. M. H-Gangaraj, Y. Alvandi-Tabrizi, G. H. Farrahi, G. H. Majzoobi, H. Ghadbeigi, Trib. Inter. 44, 1583 1588 (2011).
  • [11] M. Benedetti, V. Fontanari, P. Scardi, C. L. A. Ricardo, M. Bandini, International Journal of Fatigue. 31, 1225-1236 (2009).
  • [12] C. A. Rodopoulos, S. A. Curtis, E. R. de los Rios, J. Solis Romero. International Journal of Fatigue. 26, 849-856 (2004).
  • [13] S. Curtis, E. R. de los Rios, C. A. Rodopoulos, A. Levers, International Journal of Fatigue. 25, 59-66 (2003).
  • [14] W. Jianming, L. Feihong, Y. Feng, Z. Gang, The International Journal of Advanced Manufacturing Technology 56, 571-578 (2011).
  • [15] S. A. Meguid, G. Shagal, J. C. Stranart, International Jurnal of Impact Engineering 27, 119-134 (2002).
  • [16] R. Vafaei, M. R. Toroghinejad, R. Pippan. Materials Science and Engineering A. 536, 73-81 (2012).
  • [17] T. Sakai, A. Belyakov, R. Kaibyshev, H. Miura, J. J. Jonas, Prog. Mater. Sci. 60, 130-207 (2014).
Uwagi
EN
This work was supported by the Polish State Committee for Scientific Research under project no. 2012/07/N/ST8/03099.
PL
Opracowanie ze środków MNiSW w ramach umowy 812/P-DUN/2016 na działalność upowszechniającą naukę
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-b15b7e48-3770-43e6-85b9-cb15c1173bc4
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.