Stabilizacja szlamów pogalwanicznycii z użyciem cementu i pyłów krzemionkowych
Języki publikacji
Abstrakty
Solidification in mineral binders is one of the useful methods of neutralizing hazardous materials. In this work some waste created after neutralization of used etching baths, obtained in the process of wire galvanizing and copper plating were solidified by cement mortar with and without silica fume. The researches showed that the addition of waste to cement mortar in the amount of up to 5% is safe in respect of ecology. At such an amount of waste addition to cement, metals are permanently immobilized in a matrix. While the addition of 10% of silica fume to cement improved the strength properties of products, it had no influence on the enhancement of immobilization of metals in cement mortars.
Odpady pogalwaniczne zaliczane są do odpadów niebezpiecznych, dlatego muszą być unieszkodliwiane. Jedną z najprostszych metod unieszkodliwiania jest zestalanie w spoiwaeh mineralnych. W niniejszej pracy przeprowadzono próby zestalania w zaprawie cementowej oraz w zaprawie cementowej z dodatkiem pyłów krzemionkowych odpadu powstałego po neutralizacji zużytych kąpieli do trawienia, rozcieńczonych wodami popłucznymi, pochodzącymi z procesu cynkowania oraz miedziowania drutu. Badania wykazały, że dodatek odpadów w ilości do 5% jest bezpieczny pod względem ekologicznym. Przy takiej ilości dodatku odpadów do cementu następuje nieznaczne obniżenie parametrów fizykomechanicznych, a metale są trwale immobilizowane w matrycy. Dodatek pyłów krzemionkowych w ilości 10% do cementu poprawiał cechy wytrzymałościowe wyrobów, ale wprowadzenie odpadów obniżało te parametry.
Czasopismo
Rocznik
Tom
Strony
117--125
Opis fizyczny
bibliogr. 18 poz., tab., wykr.
Twórcy
autor
autor
- Poznań University of Technology. Faculty of Chemical Technology, Institute of Chemistry and Technical Electrochemistry ul. Piotrowo 3, 60-965 Poznań. Poland, malgorzata.osinska@put.poznan.pl
Bibliografia
- [1] Conner J.R., S.I,. Hoeffner: The History of Stabilization/Solidification Technology, Critical Reviews in Environmental Science and Technology, 28(4), 325-3% (1998).
- [2] Cullinane M.J., I.. W. Jones, P.C. Malone: Handbook for Stabilization/Solidified! ion of Hazardous Wastes, U.S. EPA 45268, Cincinnati, Ohio (EPA/504/2-86/001) June 1986.
- [3] Colak A.: Characteristics of pastes from a Portland cement containing different amounts of natural pozzolan. Cement and Concrete Research, 33, 585-593 (2003).
- [4] EN 196-1:1994: Methods of testing cement. Determination of strength.
- [51 EN 196-3:1994: Methods of testing cement, Determination of setting lime and soudness.
- [6] EPA Regulation on Land Disposal Restrictions, 1991, Appendix 11: Toxicity Characteristic Leaching Procedure, 161:1877, Published by The Bureau of National Affairs, Inc., Washington IXC. 20037.
- [7] Lee C, D.H. Tseng, D.D. Yu: Effectiveness of codisposedfly ash and heavy metal sludge by cement solidification. Journal of Resource Management and Technology, 19, 74-81 (1991).
- [8] Norma: Technische Verordnung über Ablalle, 1990, (TVA) AS. 1991 vom 10 Dezember, Der Schweize-rische Bundesrat.
- [9] Osińska M., T. Stefanowicz: Admixturing of waste nickel hydroxide to ceramic building materials, Polish Journal of Applied Chemistry, 44(3-4), 109-116 (2001).
- [10] Osińska M., A. Ślosarczyk: Trials of post-neutralization sludge solidification. Annals of the Polish Society, 2, 288-291 (2005).
- [11] Osińska M.. A. Ślosarczyk: Solidification of waste material coming from the process of fluoroborale. Annals of the Polish Society, 2, 292-296 (2005).
- [12] Pekmezci B.Y., S. Akciiz: Optimum usage of a natural pozzolan for the maximum comprcssive strength of concrete. Cement and Concrete Research, 34, 2175-2179 (2004).
- [13] Polish Standard PN-88/B-4500: Buildings mortars. Investigation of physical and mechanical properties.
- [14] Shannag M..I.: High strength concrete containing natural pozzolan and silica fume. Cement and concrete composites, 22, 399 406 (2000).
- [15] Stefanowicz T., M. Osińska: Investigation of ceramics admixtured with copper hydroxide. Archives of Environmental Protection, 24. 4, 175-183 (1998).
- [16] Stefanowicz T.,M. Dudka, M. Osińska: Investigation of ceramics admixtured with lead chromate. Chemik, 6, 155-179(1998).
- [17]Stefanowicz T., M. Osińska, S. Napieralska-Zagozda: Investigation of ceramics admixfitred with waste sludge from Send electroplating. Archives of Environmental Protection, 26, 3, 137-149 (2000).
- [18] Stefanowicz T, M. Osińska, D. Paukszta: Nickel immobilization in ceramic matrix admixed with waste nickel hydroxide. Waste Management. 23, 871 -877 (2003).