The results of the abrasion resistance measurements of aluminized steel strips are presented in the hereby paper. Steel strips of DX52D+AS120 grade, before and after a heat treatment at temperatures of 200-1000 C for 1 – 5760 minutes, were tested. Tests of the abrasion resistance were carried on in a specially built device: rotating disk – sample performing a plane-rotary motion, with an application of a lubricating medium. Examinations of the abrasion resistance were also performed by means of the block-on-ring tester. Estimations of a coating mass loss, roughness and thickness changes were carried on. The obtained results are illustrated by diagrams and macro- and micro-observations. Phase analysis investigations were also performed on samples selected after the abrasibility testing. The range of the heat treatment parameters – after which the Al-Si coating increased its abrasion resistance – was estimated.
PL
W artykule przedstawiono wyniki badan odpornosci na ścieranie aluminiowanych tasm stalowych. Badaniom poddano taśmy stalowe z gatunku DX52D+AS120 przed i po obróbce cieplnej w temperaturze 200-1000 C w czasie 1min-5760min. Wykonano badania odporności na ścieranie w specjalnie przygotowanym urzadzeniu typu obracająca się tarcza – próbka, wykonujaca ruch posuwisto-zwrotny, przy zastosowaniu środka smarujacego Zrealizowano także badania odporności na zużycie cierne za pomocą testera typu rolka-klocek. Dokonano oceny ubytku masy, zmian chropowatoąci i grubości powłoki. Wyniki badan zobrazowano za pomocą wykresów oraz makro i mikro obserwacji. Przeprowadzono także badania analizy fazowej na próbkach wytypowanych po badaniach ścieralności. Określono taki zakres parametrów obróbki cieplnej, po której następuje wzrost odporności na ścieranie powłoki Al-Si.
Twórcy
autor
  • Faculty of Non-Ferrous Metals, AGH University of Science and Technology, 30-059 Cracow, 30 Mickiewicza Av., Poland
Bibliografia
  • [1] EN 10346:2009.
  • [2] ASTM A463/A463M - 06.
  • [3] ASM Handbook: Surface Engineering, ASM International, Handbook Committee 5, 346 (1994).
  • [4] S. Kobayashi, T. Yakou, Materials Science and Engineering A 338, 1-2, 44-53 (2002).
  • [5] Y. Inoue, M. Kikuchi, Nippon Steel Technical Report 88, 62-69 (2003).
  • [6] M. Suehiro, K. Kusumi, T. Miyakoshi, J. Maki, M. Ohgami, Nippon Steel Technical Report 88, 16-21 (2003).
  • [7] W. Chaur-Jeng, Ch. Shih-Ming, Surface and Coatings Technology 200, 22-23, 6601-6605 (2006).
  • [8] K. Żaba, S. Nowak, S. Kąc, M. Wróbel, Research on temperature time and atmospheric impact on Al-Si coat of low-carbon steel strips, International Conference: Problems of modern techniques in aspect of engineering and education, Pedagogical University Cracow, Institute of Technology - Cracow, Monography, 73-78 (2006).
  • [9] Gul Hameed Awan, Faizul Hasan, The morphology of coating/substrate interface in hot-dip-aluminized steels, Materials Science and Engineering, Nr A, 1-9 (2007).
  • [10] K. Żaba, Pomiar temperatury w linii technologicznej zgrzewania stalowych rur z powłoką Al-Si, Rudy i Metale Nieżelazne R 52, 8, 473-481 (2007).
  • [11] R. Vayedaa, J. Wang J, Adhesion of coatings to sheet metal under plastic deformation, International Journal of Adhesion & Adhesives, 27, 480-492 (2007).
  • [12] W. Deqing, Applied Surface Science 254, 10, 3026-3032 (2008).
  • [13] K. Żaba, S. Kąc, Badania efektów działania wysokiej temperatury, czasu i atmosfery na użytkowe własności powłoki Al-Si na stalowych rurach przeznaczonych na elementy układów wydechowych, Rudy i Metale Nieżelazne R 53, 11, 694-704 (2008).
  • [14] K. Żaba, Archives of Civil and Mechanical Engineering 9, 2, 145-152 (2009).
  • [15] K. Żaba, Archives of Metallurgy and Materials 55, 1, 151-162 (2010).
  • [16] A. Misra, I. Finnie, Wear 68, 184-190 (1981).
  • [17] J. H. Tylczak, A. Oregon, ASM Handbook 18, 184-190 (1995).
  • [18] E. Osuch-Słomka, M. Szczerek, Oznaczanie odporności na ścieranie powłok metodą ball-cratering, Tribologia 6, 113-126 (2008).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-article-BSW3-0100-0002
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.