Multilayer Al2O3/Mo composites

Identyfikatory
Warianty tytułu
Języki publikacji
EN
Abstrakty
EN
The present study was concerned with multilayer composites of the .../Al2O3/Al2O3 + x vol. % Mo/Al2O3 type produced by tape casting. Molybdenum content in individual layers of the composites varied from 4 to 28 vol. %. The densities, porosities, Young moduli, bending strengths, and fracture toughnessess of the composites were measured. The residual stress in the layers was analysed by FEM. Investigations of the composite microstructures revealed: α-Al2O3, Mo, and Mo2C. After sintering, the composites had a high relative density (the porosity Pc did not exceed 10%). As the volumetric content of molybdenum increased, the densities of the composites increased, whereas their Young moduli E decreased. The highest values of the bending strength σb (819 MPa), stress intensity factor KIC (7.75MPa·m1/2), and cracking energy γ (102 J/m2 ) were obtained in the composite with the 14 vol. % molybdenum content. The strength σb and fracture toughness of this composite were more than two times higher than those of Al2O3, and the cracking energy – six times. These values can be partly explained in terms of the compressive residual stress in the composite layers.
Słowa kluczowe
Wydawca
Rocznik
Strony
803--812
Opis fizyczny
Bibliogr. 27 poz., rys., tab.
Twórcy
autor
autor
  • Faculty of Materials Science and Engineering, Warsaw University of Technology, ul. Wołoska 141, 02-507 Warsaw, Faculty of Materials Science and Engineering, Warsaw University of Technology, ul. Wołoska 141, 02-507 Warszawa,, huba@inmat.pw.edu.pl
Bibliografia
  • [1] CAHN R.W., HAASEN P., KRAMER E.J., Materials Science and Technology. Structure and Properties of Ceramics, Vol. 11, CH, Weinheim, 1994.
  • [2] MARSHALL D.B., RATTO J.J., LANG F.F., J. Am. Cer. Soc., 74 (1991), 2979.
  • [3] KOVAR D., THOULESS M.D., HALLORAN J.W., J. Am. Cer. Soc., 81 (1998), 1004.
  • [4] HUANG Y., CAI S., GUO H., WANG C., XIE Z., The Biomimetric Structure Design and Preparation of Si3N4 Matrix Composites with High Toughness, 9th Cimtec-World Ceramics Congress 2000, pp. 881–888.
  • [5] ZENG Y., JIANG D., Fabrication and properties of laminated Al2O3/TiC composites, Cer. Int., 27 (2002), 597.
  • [6] MING L.Y., WEI P., SHUGIN L., JIAN CH., RUIGANG W., JIANQUING LI, Cer. Int., 28 (2002), 223.
  • [7] DREWNY E.N., MOON R.J.,BOWMAN K.J.,TRUMBLE K.P.,BREMM J., Scripta Materialia, 41 (1999), 749.
  • [8] CAI P.Z., GREEN D.J., MESSING G.L., J. Am. Cer. Soc., 80 (1997), 1929.
  • [9] CAI P.Z., GREEN D.J., MESSING G.L., J. Am. Cer. Soc., 80 (1997), 1940.
  • [10] GREEN D.J., CAI P.Z., MESSING G.L., J. European Cer. Soc., 19 (1999), 2511.
  • [11] FOLSOM C.A., ZOK F.W., LANGE F.F., J. Am. Cer. Soc., 77 (1994), 689.
  • [12] OECHSNER M., HILLMAN C., LANGE F.F., J. Am. Cer. Soc., 79 (1996), 1834.
  • [13] WANG H., XIAOZHI H., J. Am. Cer. Soc., 79 (1994), 553.
  • [14] SERGO V., LIPKIN D.M., DE PORTU G., CLARKE D.R., J. Am. Cer. Soc., 80 (1997), 1633.
  • [15] LAKSHMINARAYANAN R., SHETTY D.K., CUTLER R.A., J. Am. Cer. Soc., 79 (1996), 79.
  • [16] MARSHALL D.B., MORGAN P.E.D., HOUSLEY R.M., J. Am. Cer. Soc., 80 (1997), 1677.
  • [17] CUTLER W.A., ZOK F.W., LANGE F.F., J. Am. Cer. Soc., 80, (1997), 3029.
  • [18] MOON R.J., BOWMAN K.J., TRUMBLE K.P., RODEL J., Acta Mater., 49 (2001), 995.
  • [19] LUCCHINI E., SBAIZERO O., J. European Cer. Soc., 15 (1995), 975.
  • [20] CAI P.Z., GREEN D.J., MESSING G.L., J. European Cer. Soc., 5 (1998), 2025.
  • [21] ZHANG G-J., YUE X-M., WATANABE T., J. European Cer. Soc., 19 (1999), 2111.
  • [22] JIMENEZ-MELENDO M., GUTIERERREZ-MORA F., DOMINGUEZ-RODRIGUEZ A., Acta Mater., 48 (2000), 4715.
  • [23] HWU K.L., DERBY B., Acta Mater., 47 (1999), 545.
  • [24] CHENG Z., MECHOLSKY J.J., J. Am. Cer. Soc., 76 (1993), 1258.
  • [25] http://michelle.ucsd.edu/lib/props/panos/moa.html.
  • [26] MUNRO R.G., J. Am. Cer. Soc., 80 (1997), 1919.
  • [27] MISTLER R.E., TWINAME E.R., Tape Casting: Theory and Practice, American Ceramic Society, Westerville, OH, 2000.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-article-BPW1-0022-0049
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.