The influence of hydrostatic extrusion on size, shape and spatial distribution of intermetallic particles in 7475 aluminium alloy

Identyfikatory
Warianty tytułu
PL
Wpływ wyciskania hydrostatycznego na wielkość, kształt i rozmieszczenie cząstek faz międzymetalicznych w stopie aluminium 7475
Konferencja
Advanced Materials and Technologies, AMT 2007 : XVIII Physical Metallurgy and Materials Science Conference (XVIII; 18-21.06.2007; Warszawa-Jachranka, Polska)
Języki publikacji
EN
Abstrakty
EN
The changes of intermetallic particles in 7475 aluminium during processing by hydrostatic extrusion were investigated by measuring their size, shape and spatial distribution. Samples were processed in three different condition: (i) annealed, (ii) solution heat treated and (iii) solution heat treated and aged. It was found that the particles are refined by hydrostatic extrusion but not down to the nanoscale. The final particle size is about 0.9 urn and does not depend on material initial state. The particle shape and spatial distribution are modiefid by hydrostatic extrusion.
PL
W pracy przedstawiono wpływ wyciskania hydrostatycznego na wielkość, kształt i rozmieszczenie cząstek pierwotnych faz międzymetalicznych w stopie 7475. Badany stop został poddany procesowi wyciskania hydrostatycznego w trzech różnych stanach: wyżarzonym, przesyconym oraz przesyconym i starzonym. Wykazano, że analizowane cząstki faz międzymetalicznych ulegają rozdrobnieniu, lecz nie do rozmiarów manometrycznych. Nieznacznie zmniejsza się ich średnica równoważna, przede wszystkim na skutek fragmentacji cząstek dużych i dla końcowego etapu wyciskania wynosi on 0,9 (im i nie zależy od stanu materiału. Wyciskanie hydrostatyczne prowadzi także do zmian kształtu i rozmieszczenia cząstek.
Rocznik
Strony
486--490
Opis fizyczny
Bibliogr. 12 poz., rys., tab.
Twórcy
autor
  • Warsaw University of Technology, faculty of materials Science and Engineering, 02-507 Warsaw, Woloska 141, Poland, kiniac@o2.pl
Bibliografia
  • [1] Valiev R.Z. The New SPD processing trends to fabricate bulk nanostructured materials. Solid State Phenomena,Vol.114 (2006) 7-18.
  • [2] Lewandowska M, Garbacz H, Pachla W, Mazur A, Kurzydlowski KJ. Hydrostatic extrusion and nanostructure formation in aluminium alloy. Solid State Phenom 2005; 101-102:65-9.
  • [3] Lewandowska M, Kurzydlowski KJ. Thermal stability of nanostructured aluminium alloy. Materials Characterization 2005; 55:395-401.
  • [4] Kurzydlowski KJ, Garbacz H, Richert M. Effect of Severe Plastic Deformation on the mechanical properties of Al and Cu. Re.Adv.Mater.Sci. Vol.8 (2004) 129-133.
  • [5] Lewandowska M. Microstructure and properties of aluminium alloys processed by hydrostatic extrusion. Publishing House of The Warsaw University of Technology, 2006, 43-52.
  • [6] Zhao Y.H., Liao X.Z., Jin Z., Valiev R.Z., Zhu Y.T. Microstructures and mechanical properties of ultrafine grained 7075 Al alloy processed by ECAP and their evoluations during annealing. Acta Materialia Vol 52 (2004) 4589-4599.
  • [7] Immarigeon, J.-P., Holt, R.T.; Koul, A.K.; Zhao, L.; Wallace, W.; Beddoes, J.C.; Lightweight materials for aircraft applications. Materials Characterization Vol. 35 (1995) 41-67.
  • [8] Abis S., Massazza M., Mengucci P., Riontino G.; Early ageing mechanisms in high-copper AlCuMg alloy. Scripta Materialia Vol. 45 (2001) 685-691.
  • [9] Kurzydlowski KJ., Ralph B. Quantitative description of microstructure of materials. Boca Raton: CRS Press: 1995.
  • [10] Li X.-M., Starink M.J. The Effect of compositional variations on the characteristics of coarse intermetallic particles in overaged 7xxx Al alloy. Material Science Technology, Vol. 17 (2001) 1324-28.
  • [11] Li X., Starink M.J. Analysis of precipitation and dissolution in overaged 7XXX aluminium alloy using DSC. Material Science Forum, 2000, vol. 331-337, pp. 1071-1076.
  • [12] Starink M.J., Gao N., Furukawa M., Horsta Z., Xu Ch., Langdon T.G. Microstructural development in a spry-cast Al-7034 alloy processed by Equal-Chanel Angular Pressing. Advenced Materials Science,Vol. 7 (2004) 1-12.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-article-BPL8-0005-0100
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.