Sealing plates : structure, morphology and cross-linking

Wybrane pełne teksty z tego czasopisma
Identyfikatory
Warianty tytułu
PL
Płyty uszczelniające : struktura, morfologia i sieciowanie
Języki publikacji
EN
Abstrakty
EN
The technology of sealing plates has been outlined, paying attention to the analogy and differences between this technology and rubber technology. The structure and micro-morphology of sealing plates were investigated by the methods of SEM, AFM and nanoindentation. An oscillatory rheometer was successfully used to examine the cross-linking course of the elastomer contained in the plate and accompanying phenomena. Significant differences were found between the courses of sulfur and peroxide vulcanizations. It has been observed that the rubber contained in the plate, after cross-linking, does not form a continuous phase but occurs in the form of isolated clusters, mostly including very thin membranes. There are also numerous visible agglomerates of fillers, especially in the middle part of the plate. It has been found that during plate formation and rubber vulcanization, a considerable temperature gradient occurs. The findings create conditions for the modification of sealing plate technology.
PL
Omówiono w zarysie technologię płyt uszczelniających. Zwrócono uwagę na analogie i różnice między technologią płyt uszczelniających a technologią gumy. Zbadano strukturę i mikromorfologię płyt uszczelniających metodami SEM, AFM i nanoindentacji. Zastosowano z powodzeniem reometr oscylacyjny do badania przebiegu sieciowania elastomeru zawartego w płycie i zjawisk towarzyszących. Stwierdzono występowanie istotnych różnic między przebiegiem wulkanizacji siarkowej i nadtlenkowej. Zaobserwowano, że kauczuk zawarty w płycie, po usieciowaniu, nie tworzy fazy ciągłej, lecz występuje w postaci izolowanych skupisk, najczęściej są to błonki o bardzo małej grubości. Widoczne są również liczne aglomeraty napełniaczy, szczególnie w warstwie środkowej płyty. Ustalono, że podczas formowania płyty i wulkanizacji kauczuku w materiale występuje znaczny gradient temperatury. Wyniki badań stwarzają przesłanki modyfikacji technologii płyt uszczelniających.
Rocznik
Strony
159--164
Opis fizyczny
Bibliogr. 12 poz., rys., tab.
Twórcy
autor
autor
autor
  • Technical University of Łódź, Institute of Polymer and Dyes Technology, ul. Stefanowskiego 12/16, 90-924 Łódź, Poland, ludomir.slusarski@p.lodz.pl
Bibliografia
  • [1] Tietze W. (Hrsg.) Handbuch Dichtungspraxis, 3 Auflage, Vulkan - Verlag, Essen 2003.
  • [2] Ślusarski L., Baryń W., Janczak T., Libudzisz J., Andrzejczak Z., Zielińska A., Matuszyński J., Polish Patent Nr 147805.
  • [3] Ślusarski L., Baryń W., Zaborski M., Libudzisz J., Technology of asbestos-free sealing materials (Gaskets), Polish Journal of Chemical Technology 1999, 1, 31-35.
  • [4] Braun J. Current elastomer compatibility test standards, Sealing Technology 2011, 3, 8-12.
  • [5] Slay B., Webber W., Stress relaxation of elastomer compounds, Sealing Technology 2011, 2, 9-12.
  • [6] Piringer S., Rustemeyer U., Improvement of parameters, based on fibre sealing plates, at elevated temperatures, Sealing Technology 2004, 3, 1-11.
  • [7] Bieliński D., Ślusarski L., Dobrowolski O., Głąb P., Dryzek E., Studies of filler agglomeration by atomic force microscopy and positron anihilation spectroscopy, Kautschuk Gummi Kunststoffe 2004, 11, 579-586.
  • [8] Blachura J. Wpływ struktury i właściwości sprężystych materiału uszczelnień spoczynkowych na ich szczelność, Praca doktorska, Politechnika Wrocławska, Wrocław 2005.
  • [9] De S.K. White J.R. (edit.), Rubber Technologists Handbook, Rapra Technology Limited, Shawbury 2001, U.K.
  • [10] Pazur R.J., Walker F.J., Practical state of cure measurements by magnetic resonance, Kautschuk Gummi Kunststoffe 2011, 10, 16-23.
  • [11] Ślusarski L. The effect of structure on properties of elastomers, Kautschuk Gummi Kunststoffe 1992, 9, 705-707.
  • [12] Kiroski O., Sims J., Packham D.E., Gregory A.L, The use of thiol - amine chemical probes in network Characterisation of NBR vulcanizates, Kautschuk Gummi Kunststoffe 1997, 10, 716-720.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-article-BPC6-0020-0003
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.