PL EN


Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników
Tytuł artykułu

Study of the solid phase catalytic oxidation of polypropylene

Identyfikatory
Warianty tytułu
Języki publikacji
EN
Abstrakty
EN
The solid phase catalytic oxidative degradation of isotactic polypropylene was studied. The influences of the type and amount of catalyst, temperature, and type of oxidising agent on the oxidative degradation were investigated. Iron(III), manganese(II), cobalt(II), vanadium(III), copper(II) and nickel(II) acetylacetonates were used as catalysts. The obtained products were characterised by the determination of acid number, saponification number and melting range as an index of the degradation progress.
Rocznik
Strony
1--9
Opis fizyczny
Bibliogr. 41 poz., rys., tab.
Twórcy
autor
autor
autor
  • Department of Chemical Organic Technology and Petrochemistry, Silesian University of Technology, Krzywoustego 4, 44-100 Gliwice, Poland, jan.zawadiak@polsl.pl
Bibliografia
  • [1] Cerasana Research's Brochure: Market Study: Propylene. 2008.
  • [2] Ullmann's Encyclopedia of Industrial Chemistry Sixth Edition, Electronic Release: Wiley-VCH, 2002.
  • [3] Sadlowska M„ Nowak D.. Przem. Chein., 1994. 73. 384.
  • [4] Buchachenko A.I I. Polym. Sci. Symp.. 1976, 57. 299.
  • [5] Halim Hamid S.. Handbook of PolimerDegradation. Chapter II-7, CRS Press. 2000.
  • [61 Shibryaeva L.S.. Popov A.A.. Zaikov G.E.. Russ. J. App. Chem.. 2002. 75(4). 619.
  • [7] Verdu S., Verdu J.. Macromolecules. 1997. 30. 2262.
  • [8[ Achimsky L.. Baudouin L., VerduJ., Polym. Degrad. Stab.. 1996. 52, 161.
  • [9] RychlyJ., Matisova-Rychla L., Csmorova K.. Achimsky L.. Baudouin L., Tcharktchi A., Verdu J„ Polym. Degrad. Stab., 1997. 58. 269.
  • [10] Gugumus F., Polym. Degrad. Stab.. 1998. 62, 245.
  • [11] Gugumus F„ Polym. Degrad. Stab., 1996, 52, 161.
  • [12] Achimsky L., Audouin L., VerduJ„ RychlyJ., Matisova-Rychla L.. Polym. Degrad. Stab.. 1997. 58, 283.
  • [13] Richaud E., Farcas F.. Bartolomeo P.. Fayolle B„ Audouin L„ Verdu J„ Polym. Degrad. Stab., 2006. 91. 398.
  • [14] Achimsky L„ Audouin L., Verdu J„ Polym. Degrad. Stab., 1997. 57, 231.
  • [15] Gugumus F., Polvm. Degrad. Stab.. 1998, 62, 235.
  • [16] Koichiro K., J. App. Polym. Sei.. 1975. 19(6), 1593.
  • [17] Abdouss M.. Sanjani N. S., Baraille P.. J. Sei. Univ. Tehran Int. Ed.. 1998. 3(1), 47.
  • [18] Krisyuk B.E.. Popov A.A;, Denisov E.T., Polymer Science Series B, 1985, 27(4), 266.
  • [19] Zenkiewicz M., Lutomirski S.. Polimeiy, 2006, 51(6), 442.
  • [20] Sickle D.E., Macromolecules. 1977. 10. 474.
  • [21] Sickle D.E., J Polym. Sei. AI, 1972. 10, 355.
  • [22] Iring M., Kelen T„ Tudos F.. Polym. Bull., 1986. 15, 531.
  • [23] Abdouss M., Sharifi-Sanjani N„ Iran. Polym. J„ 1997, 6(4) 1026.
  • [24] Guillet J.E., US Patent 2 828 296, 1958: to Eastman Kodak Co.
  • [25] Mikeska L.A.. Young D.W., US Patent 2 554 259. 1951; to Standard Oil Development Co
  • [26] Thompson W.E.. Albright D.M.. Stuart A.P., US Patent 2 950 267, 1960: to Sun Oil Co.
  • [27] McCall M.A., Shearer N.H. Jr.. US Patent 3 232 917, 1966; to Eastman Kodak Co.
  • [28] Partenheimer W„ US Patent 2004/0019156 Al. 2004.
  • [29] Sheldon R.A., Kochi J.K.. Metal Catalyzed Oxidations of Organic Compounds; Academic Press; New York, 1981.
  • [30] Russell G.A., Peroxide Reaction Mechanism: Peroxide Pathways In Autoxidation; Edwards. J. O., Ed..; Inc. New York. 1962.
  • [31] Bawn C.E.H.. Chaudri S.A., Polymer, 1968. 9, 81.Jadmicek B.R.. Stivala S.S.. Reich L„ Macromolecules. 1972, 5(1), 20.
  • [32] Sipen A.J., Rutherford D.R., J. Environ. Polym. Degrad., 1993. 1, 193.
  • [33] Eyenga I.I., Focke W.W., Prinsloo L.C, Tolmay A.T., Macromolecular Symp.. 2002. 178, 139.
  • [34] Chatteijee A.M., Salanitro J.P., US Patent 5135966 A, 1992: to Shell Oil Company.
  • [35] Lueders W.. Fischer E., DE Patent 2418834 Al. 1975; to Hoechst AG.
  • [36] Hemmerich H.P.. Rosenkranz H.J.. Rudolph H., DE Patent 2 354 534 Al. 1975: to Bayer AG.
  • [37] Isigami M., Arimoto K.. DE Patent 2 242 275 Al. 1973: to Harima Chemicals. INC.
  • [38] DIN EN ISO 2114:2000. Plastics (polyester resins) and paints and varnishes (binders) - Determination of partial acid value and total acid value.
  • [39] DIN EN ISO 3681:1996, Binders for paints and varnishes - Determination of saponification value - Titrimetric method.
  • [41] DIN EN ISO 3146:2000. Plastics - Determination of melting behavior (melting temperature or melting range) of semi-ciystalline polymers by capillary tube and polarizing-microscope methods.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-article-BPC2-0009-0001
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.