Effect of a chelating agent on the synthesis of zeolitic materials from waste sandstone cake using alkali fusion

Autorzy
Treść / Zawartość
Identyfikatory
Warianty tytułu
Języki publikacji
EN
Abstrakty
EN
During quarrying, waste stone cake is discharged as industrial waste, and in Japan the amount of cake amounts annually to 50 millions tons. To promote waste recycling, we attempted to convert waste sandstone cake into zeolitic material using alkali fusion. However, calcium causes the synthesis of an undesirable zeolite by interfering in the synthesis of a high functional zeolite. As a means to inhibit this Ca-interference, we studied the effect of adding a chelating agent, EDTA (Ethylenediaminetetraacetic acid disodium dihydrate), on the synthesis of zeolitic material from sandstone cake using alkali fusion. Hydroxysodalite, zeolite-X and zeolite-P can be synthesized from sandstone cake using alkali fusion. With the addition of EDTA, calcium ions in solution were trapped by chelation, and the amount of zeolite-X and zeolite-P increased. A product with a high CEC, which has a high content of zeolite-X, can be obtained. The chelating agent can inhibit Cainterference for zeolite synthesis by Ca-masking, and the product with high content of zeolite-X can be obtained from waste sandstone cake using alkali fusion.
Rocznik
Tom
Strony
76--87
Opis fizyczny
Bibliogr. 23 poz., rys., tab.
Twórcy
autor
autor
  • Department of Materials-process Engineering and Applied Chemistry for Environments, Akita University, 1-1, Tegata-Gakuen cho, Akita 010-8502, Japan, wajima@gipc.akita-u.ac.jp
Bibliografia
  • [1] R. M. Barrer, Zeolites and Clay Minerals as Sorbents and Molecular Sieves, Academic Press, London 1978, p. 1-22.
  • [2] R. M. Barrer, R. Beaumont, C. Colella, J. Chem. Soc. Dalton Trans., 1974, 934-941.
  • [3] R. Ruiz, C. Banco, C. Pesquera, F. Gonzalez, I. Benito, J. L. Lopez, Appl. Clay Sci., 1997, 12, 73-83.
  • [4] A. Baccouche, E. Srasra, M.E. Maaoui, Appl. Clay Sci., 1998, 13, 255-273.
  • [5] A.F. Gualtieri, Phys. Chem. Miner., 2001, 28, 719-728.
  • [6] D. Boukadir, N. Bettahar, Z. Derriche, Annual de Chimie Science des Materiaux, 2002, 27, 1-13.
  • [7] X. Querol, N. Moreno, J.C. Umaña, A. Alastuey, E. Hernández, Int. J. Coal Geol., 2000, 50, 413-423.
  • [8] G.C.C. Yang, T.-Y. Yang, J. Hazard. Mater., 1998, 62, 75-89.
  • [9] T. Wajima, Y. Ikegami, Ars Separatoria Acta, 2006, 4, 86-95.
  • [10] T. Wajima, H. Ishimoto, K. Kuzawa, K. Ito, O. Tamada, M.E. Gunter, J.F. Rakovan, Am. Miner., 2007, 92, 1105-1111.
  • [11] X. Querol, J.C. Umaña, F. Plana, A. Alastuey, A. López-Solar, A. Medinaceli, A. Valero, M.J. Domingo, E. Gracia-Rojo, Fuel, 2001, 80, 867-865.
  • [12] N. Sigemoto, H. Hayashi, K. Miyamura, J. Mater. Sci., 1993, 28, 4781-4786.
  • [13] G.G. Hollman, G. Steenbruggen, M. Janssen-Jurkovicova, Fuel, 1999, 78, 1225-1230.
  • [14] T. Wajima, K. Kuzawa, H. Ishimoto, O. Tamada, T. Nishiyama, Am. Miner., 2004, 89, 1694-1700.
  • [15] T. Wajima, M. Haga, K. Kuzawa, H. Ishimoto, O. Tamada, K. Ito, T. Nishiyama, R.T. Downs, J.F. Rakovan, J. Hazard. Mater., 2006, B132, 244-252.
  • [16] T. Wajima, T. Shimizu, Y. Ikegami, J. Environ. Sci. Health –A, 2007, 42, 345-350.
  • [17] K. Nishida, T. Nishigata, Y. Tatsuta, T. Okumura, Proc. the 37th conf. Jpn. Geotech. Soc., Japan Geotech. Soc., Tokyo, 2002, 1141-1142.
  • [18] H. Tanaka, Inorganic Mater., 1997, 4, 475.
  • [19] T. Wajima, K. Yoshizuka, Y. Ikegami, J. Jpn Soc. Eng. Geol., 2006, 47(5), 292-296.
  • [20] T. Wajima, Y. Ikegami, K. Yoshizuka, T. Hirai, J. Ion Exch., 2007, 18(4), 142-145.
  • [21] P. Catalfamo, G. Patane, P. Primerano, S.D. Pasquale, F. Corigliano, Mater. Eng., 1994, 5, 159-173.
  • [22] N.R.C. Fernandes Machado, D.M. Malachini Miotto, Fuel, 2005, 84, 2289-2294.
  • [23] Y. Kato, K. Kakimoto, H. Ogawa, M. Tomai, E. Sakamoto, Kougyo-yousui, 1986, 331, 27-33.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-article-BATA-0007-0052
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.