The paper presents the results of a study on the modification of Al-12%Si alloy with a homogeneous modifier produced by fast cooling at a rate of 100 and 200 K/s. The homogeneous modifier had the chemical composition of the modified alloy, and it contained 0, 7, 12 and 20% Si. The modifier was mixed with liquid Al-Si alloy in the crucible for one minute. The effect of cooling rate and the modifier content of alloy mass on alloy structure was determined in the study. An analysis of the modification of eutectic Al-Si alloy with a homogeneous modifier obtained by fast cooling of the treated alloy showed that the modifier affected the structure of Al-12%Si alloy.
PL
W pracy przedstawiono wyniki badań nad modyfikacją stopu Al-12%Si modyfikatorem homogenicznym, wytworzonym przez szybkie studzenie modyfikatora z prędkością 100 i 200 K/s. Modyfikator homogeniczny ma skład chemiczny stopu modyfikowanego i zawiera 0, 7, 12 i 20% Si. Modyfikator dodawano do tygla wraz z ciekłym stopem Al-Si i przetrzymywano przez jedną minutę. W pracy przedstawiono wpływ prędkości studzenia i zawartości modyfikatora w odniesieniu do masy obrabianego stopu na jego strukturę. Analiza procesu modyfikacji eutektycznego stopu Al-Si modyfikatorem homogenicznym otrzymanym z obrabianego stopu przez szybkie studzenie wykazała oddziaływanie modyfikujące na strukturę stopu Al-12%Si.
Rocznik
Tom
Strony
301--311
Opis fizyczny
Bibliogr. 17 poz., rys.
Twórcy
autor
autor
autor
  • Chair of Materials and Machinery Technology, University of Warmia and Mazury in Olsztyn
Bibliografia
  • ATASOY O.A., YILMAZ F., ELLIOTT R. 1984. Growth structures in aluminium-silicon alloys. I. The coupled zone. Journal of Crystal Growth, 66.
  • BORKOWSKI S. 1999. Quality controll of cast constructional materiale for example cast iron. WNT, Warszawa.
  • KRUPIŃSKI M., DOBRZYŃSKI L.A., SOKOLOWSKI J.H. 2008. Microstructure analysis of the automotive Al-Si-Cu casting. Archives of Foundry Enginieering, 8.
  • LIPIŃSKI T. 2008. Improvement of mechanical properties of AlSi7Mg alloy with fast cooling homogenous modifier. Archives of Foundry Enginieering, 8.
  • LIPIŃSKI T. 2000. Influence multicomponents mixtures for increase properties of cast alloys Al-Si. Balttechmasz-2000. Kaliningrad.
  • LIU J., ELLIOTT R. 1996. Lamellar fault formation during eutectic growth. Journal of Crystal Growth, 162.
  • LJUTOVA O.V., VOLCHOK I.P. 2008. Increase of foundry properties of secondary silumins. Archives of Foundry Enginieering, 8.
  • NOVA I., EXNER J., HOSEK Z., NOVAKOVA I. 2004. Crystallization of Al-Si alloys in the course of high pressure die-casting. Archives of Foundry, 4(14).
  • OLEJNIK E., FRAŚ E. 2007. A visualization of the eutectic solidification process. Archives of Foundry Enginieering, 7.
  • PEZDA J. 2007. Continous modification of AK11 silumin with multicomponent salt on base of NaCl. Archives of Foundry Enginieering, 7.
  • PTACEK L. 1999. Slitiny hliniku na odlitku. Slavarenstvi, 1.
  • ROMANKIEWICZ F., ROMANKIEWICZ R. 2006. Wpływ modyfikacji na strukturę i morfologię przełomów siluminu AK132. Archives of Foundry, 6(22).
  • SZAJNAR J.,WRÓBEL T. 2008. Inoculation of pure aluminium aided by electromagnetic field. Archives of Foundry Enginieering, 8.
  • VALENCIK S., TRESA D. 2008. Proposal of recycling system for waste aluminium. Archives of Foundry Enginieering, 8.
  • WOŁCZYŃSKI W., CIACH R. 1980. Growth of undirectional eutectic binary alloys. Solidifications Technology in the foundry and cast house. The Metals Society.
  • WOŁCZYŃSKI W. 1990. Application of the Chemical Potential Gradient in the Description of Eutectic Steady Growth. Metalurgy and Foundry, 2.
  • ZYSKA A., KONOPKA Z., ŁĄGIEWKA M. 2007. The solidification of squeeze cast AlCu4Ti alloy. Archives of Foundry Enginieering, 7.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-article-BAR0-0039-0100
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.